# US 2005/0217565 A1 · Method for epitaxial growth of a gallium nitride film separated from its substrate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2005/0217565 A1
- Document ID: US20050217565A1
- Status: Published application
- Kind: A1
- Application number: 10/516,358
- Filed: 2003-05-28
- Published: 2005-10-06
- Earliest claimed: 2003-05-28
- Assignees: Lumilog
- Inventors: Hacene Lahreche; Gilles Nataf; Bernard Beaumont
- Web page: https://patentgrep.com/patent/US20050217565A1

## CPC

- H10P 90/1916: {with separation or delamination along an ion implanted layer, e.g. Smart-cut}
- H10P 14/271: {characterised by the preparation of substrate for selective deposition}
- H10P 14/2921: {being crystalline insulating materials}
- H10P 14/3216: {Nitrides}
- H10P 14/3416: {Nitrides}
- H10P 14/3444: {P-type}
- H10P 54/52: {by cleaving}
- H10P 90/1912: {using selective deposition, e.g. epitaxial lateral overgrowth [ELO] or selective deposition of single crystal silicon}
- H10W 10/181: {Semiconductor-on-insulator [SOI] isolation regions, e.g. buried oxide regions of SOI wafers}
- H10H 20/018: {Bonding of wafers}
- Y10S 117/915: Separating from substrate
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

The invention concerns the preparation of gallium nitride films by epitaxy with reduced defect density levels. It concerns a method for producing a gallium nitride (GaN) film by epitaxial deposition of GaN. The invention is characterized in that it comprises at least a step of epitaxial lateral overgrowth and in that it comprises a step which consists in separating part of the GaN layer from its substrate by embrittlement through direct ion implantation in the GaN substrate. The invention also concerns the films obtainable by said method as well as the optoelectronic and electronic components provided with said gallium nitride films.

## Claims

### Claim 1

A method of producing a film of gallium nitride (GaN) using a substrate, by deposition of GaN by epitaxy, characterised in that the deposition of GaN comprises at least one step of epitaxial lateral overgrowth (ELO) and in that it comprises a step of separating part of the layer of GaN from its substrate by weakening by ion implantation in the layer of GaN directly.

### Claim 2 (depends on 1)

A method of producing a film of gallium nitride (GaN) according to claim 1, characterised in that it comprises the following successive steps:
(i) the deposition of a layer of GaN on a substrate by vapour or liquid phase epitaxy,
(ii) a weakening ion implantation step so as to create a weak area in the layer of GaN deposited during the previous step,
(iii) a step of reworking by epitaxial lateral overgrowth (ELO) in order to form a new layer of GaN and (iv) a spontaneous separation step at the weak area.

### Claim 3 (depends on 2)

A method according to claim 2, characterised in that the deposition of GaN during step (i) is effected by epitaxy by vapour or liquid phase epitaxial lateral overgrowth ELO.

### Claim 4 (depends on 3)

A method according to claim 3, characterised in that step (i) is implemented by vapour phase epitaxy technology using halides and hydrides (HVPE), by organometallic pyrolysis vapour phase epitaxy (EPVOM) technology or by sublimation (CSVT).

### Claim 5 (depends on 3, 4)

A method according to claim 3 or 4, characterised in that step (i) comprises the following steps:
deposition of a layer of GaN,
deposition of a dielectric layer which is etched in order to obtain openings,
deposition of GaN in the areas of GaN located in the openings, and then
deposition of GaN giving rise to a lateral overgrowth until the patterns of GaN coalesce.

### Claim 6 (depends on 3, 4)

A method according to claim 3 or 4, characterised in that step (i) is a step of spontaneous ELO which comprises the following steps:
deposition of silicon nitride to a thickness of around 10 to 20 nm,
deposition of a continuous buffer layer of GaN,
annealing at a high temperature of between 1050° and 1120° C. so that the buffer layer converts from a continuous layer to a discontinuous layer formed from patterns of GaN in the form of islands, and then
deposition by epitaxy of GaN.

### Claim 7 (depends on 6)

A method according to claim 6, characterised in that the implantation is effected either in the islands, or at an intermediate stage where the islands are not entirely coalesced, or after total coalescent of these islands.

### Claim 8 (depends on 1, 2, 3, 4, 5, 6, 7)

A method according to one of claims 1 to 7, characterised in that the implantation ions can be chosen from amongst H−, ions of rare gas such as helium, neon or krypton, as well as boron.

### Claim 9 (depends on 1, 2, 3, 4, 5, 6, 7, 8)

A method according to any one of claims 1 to 8, characterised in that the implantation energies can vary from 80 to 160 kev.

### Claim 10 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9)

A method according to any one of claims 1 to 9, characterised in that the ions implanted in the layer of GaN are H+ ions.

### Claim 11 (depends on 10)

A method according to claim 10, characterised in that the implantation ions are H+ ions and the H+ ion implantation dose varies from 1016 to 1017 cm−2.

### Claim 12 (depends on 2, 3, 4, 5, 6, 7, 8, 9, 10, 11)

A method according to any one of claims 2 to 11, characterised in that the spontaneous separation at the weak area of the layer formed during step (i) defined in claim 2 is implemented by a return to ambient temperature after the resumption of epitaxy.

### Claim 13 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12)

A method according to any one of claims 1 to 12, characterised in that the depth of implantation varies from 50 nm up to the GaN/initial substrate interface.

### Claim 14 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13)

A method according to any one of claims 1 to 13, characterised in that the substrate is chosen from amongst sapphire, ZnO, 6H-SiC, LiAlO2, LiAlO2, LiGaO2, MgAlO2, Si, GaAs, AlN or GaN.

### Claim 15 (depends on 14)

A method according to claim 14, characterised in that the substrate is a sapphire substrate.

### Claim 16 (depends on 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13, 14, 15)

A method according to any one of claims 2 to 15, characterised in that the epitaxial lateral overgrowth according to step (iii) as defined in claim 2 is performed by EPVOM, HVPE or CSVT epitaxy or liquid phase epitaxy (LPE).

### Claim 17 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13, 14, 15, 16)

A method according to any one of claims 1 to 16, characterised in that the gallium nitride is doped during at least one of the epitaxial lateral overgrowth steps by means of a doping substance which may be chosen from amongst magnesium, zinc, beryllium, calcium, carbon, boron or silicon.

### Claim 18 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13, 14, 15, 16, 17)

A film of gallium nitride, characterized in that it is able to be obtained by a method according to any one of claims 1 to 17.

### Claim 19 (depends on 18)

A film of gallium nitride according to claim 18, characterised in that it has a thickness of more than 50 μm.

### Claim 20 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13, 14, 15, 16, 17)

A substrate after separation of the layer of gallium nitride by ion implantation according to the method as described in any one of claims 1 to 17, comprising part of the GaN directly deposited on the substrate during step (i) as defined in claim 2, by way of new substrate which can be used for subsequent reworking by GaN epitaxy.

### Claim 21 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13, 14, 15, 16, 17)

Use of the substrate after separation of the layer of gallium nitride by ion implantation according to the method as defined in any one of claims 1 to 17, comprising part of the GaN directly deposited on the substrate during step (i) as defined in claim 2, by way of new substrate for reworking by GaN epitaxy.

### Claim 22 (depends on 18, 19)

An optoelectronic component, characterised in that it is provided with a film of GaN according to claim 18 or 19.

### Claim 23 (depends on 18, 19)

A laser diode, a UV light-emitting diode, photodetector or transistor, characterised in that it is provided with a film of GaN according to claim 18 or 19.