# US 2005/0110602 A1 · Low resistance shield

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2005/0110602 A1
- Document ID: US20050110602A1
- Status: Published application
- Kind: A1
- Application number: 10/986,929
- Filed: 2004-11-15
- Published: 2005-05-26
- Earliest claimed: 2003-11-22
- Assignees: Bruker BioSpin GmbH
- Inventors: Michael Westphal
- Web page: https://patentgrep.com/patent/US20050110602A1

## CPC

- H05K 9/0077: {comprising superconductors}
- Y10S 505/872: Magnetic field shield
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

A flat multi-layer arrangement (1; 1a-1f) of superconducting wires (4,5) with normally conducting substrate (17) and at least one fiber (16) which is electrically conductingly connected to the substrate (17) and is superconducting under predetermined operating conditions is characterized in that the superconducting wires (4, 5) in a respective layer (2, 3; 22, 23) are substantially disposed such that they do not cross. A resistive electric contact is provided between the superconducting wires (4, 5) of different layers (2,3; 22, 23) and the superconducting wires (4, 5) of at least two neighboring layers (2, 3; 22, 23) do cross, wherein no closed superconducting loops are present in the arrangement (1; 1a-1f). This arrangement permits shielding of the working volume of a magnet coil arrangement against low-frequency stray fields in an efficient and reliable manner.

## Claims

### Claim 1

A thin multi-layer structure having wire which is superconducting under operating conditions and having normally conducting material which is not superconducting under operating conditions, the structure comprising:
a first layer of first wires which are superconducting during operation of the structure, said first wires disposed to extend without crossing each other;
a second layer of second wires which are superconducting during operation of the structure, said second wires disposed to extend without crossing each other but to cross said first wires in said first layer; and
normally conducting material which is not superconducting during operation of the structure, said normally conducting material cooperating with said first and said second wires to effect resistive electrical contact between said first and said second layers, wherein the structure contains no closed superconducting loops.

### Claim 2 (depends on 1)

The structure of claim 1, wherein said first wires of said first layer are designed as warp threads and said second wires of said second layer are designed as weft threads interwoven with said warp threads of said first layer.

### Claim 3 (depends on 1)

The structure of claim 1, wherein said first layer extends at a substantially constant separation from said second layer.

### Claim 4 (depends on 3)

The structure of claim 3, wherein said first and said second layers have curved surfaces.

### Claim 5 (depends on 1)

The structure of claim 1, wherein said first wires of said first layer are disposed parallel to each other and said second wires of said second layer are disposed parallel to each other but extending in a different direction than said first wires of said first layer, wherein said first and said second layers are soldered together with a solder which is normally conducting.

### Claim 6 (depends on 1)

The structure of claim 1, wherein said first wires and/or said second wires are soldered onto a flat support body, which is normally conducting during operation and using solder which is normally conducting during operation.

### Claim 7 (depends on 1)

The structure of claim 1, wherein said first wires and said second wires cross each other at angles of at least 300.

### Claim 8 (depends on 7)

The structure of claim 7, wherein said first and said second wires cross at an angle of substantially 900.

### Claim 9 (depends on 3)

The structure of claim 3, wherein said first and said second wires are each directly soldered onto a flat support body using a solder which is normally conducting during operation.

### Claim 10 (depends on 1)

The structure of claim 1, wherein said first and said second wires have a flat cross-section with large width parallel to a flat extension and small height perpendicular to said flat extension.

### Claim 11 (depends on 1)

The structure of claim 1, wherein said first and/or said second wires consist essentially of a low-temperature superconductor which is superconducting only at temperatures below a critical temperature of less than 30° K.

### Claim 12 (depends on 1)

The structure of claim 1, wherein said first and/or said second wires consist essentially of a high-temperature superconductor which is superconducting at temperatures below a critical temperature of more than 30° K.

### Claim 13 (depends on 1)

The structure of claim 1, wherein said first layer contains first partial sections disposed next to each other in a first smooth surface and said second layer contains second partial sections disposed next to each other in a second smooth surface, wherein said first and said second partial sections are not directly connected to each other or are only connected resistively to another and borders between said first partial sections are shifted in a parallel manner with respect to said second partial sections.

### Claim 14 (depends on 1)

The structure of claim 1, wherein said thin multi-layer structure defines a closed cylinder surface.

### Claim 15 (depends on 14)

The structure of claim 14, wherein said closed cylinder surface is a circular cylinder surface.

### Claim 16 (depends on 14)

The structure of claim 14, wherein a time constant of an induced current which flows in a peripheral direction of said cylinder surface is adjusted to a predetermined value through selection and arrangement of said first wires, said second wires, and said normally conducting material.

### Claim 17 (depends on 16)

The structure of claim 16, where said time constant is between 1 second and 5 minutes.

### Claim 18 (depends on 1)

The structure of claim 1, wherein said first and said second wires are transferred from a superconducting into a normally conducting state at a precisely predetermined value of a current load under operating conditions through selection of superconducting properties thereof.

### Claim 19 (depends on 1)

A magnet system comprising the thin multi-layer structure of claim 1.

### Claim 20 (depends on 19)

The magnet system of claim 19, wherein the magnet system is structured and dimensioned for an NMR, MRI or ICR apparatus.

### Claim 21 (depends on 19)

The magnet system of claim 19, wherein the system comprises a superconducting magnet coil and the thin multi-layer structure is disposed on a cylindrical body.

### Claim 22 (depends on 21)

The magnet structure of claim 21, wherein said magnet coil is disposed in a helium tank of a cryostat and is actively shielded, the thin multi-layer structure being disposed on a wall of the helium tank or on outermost windings of said superconducting magnet coil.

### Claim 23 (depends on 21)

The magnet system of claim 21, wherein the system comprises a refrigerator cooling for said superconducting magnet coil and the thin multi-layer structure shields electromagnetic disturbances caused by said refrigerator cooling.

### Claim 24 (depends on 23)

The magnet system of claim 23, wherein the thin multi-layer structure substantially surrounds a cold head of said refrigerator cooling.

### Claim 25 (depends on 21)

The magnet system of claim 21, wherein the thin multi-layer structure surrounds shielding coils of said superconducting magnet coil or is integrated therein.

### Claim 26 (depends on 21)

The magnet system of claim 21, wherein the thin multi-layer structure is disposed radially inside a shielding coil of said superconducting magnet coil.

### Claim 27 (depends on 26)

The magnet system of claim 26, wherein a radially outer thin multi-layer structure has a first time constant for an induced current which flows in a peripheral direction which is larger than a second time constant of a radially inner thin multi-layer structure.

### Claim 28 (depends on 19)

The magnet system of claim 19, wherein the system comprises an H- or C-shaped pole shoe magnet and the thin multi-layer structure is substantially planar.