# US 2005/0089437 A1 · Free-cutting steel and fuel injection system component using the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2005/0089437 A1
- Document ID: US20050089437A1
- Status: Published application
- Kind: A1
- Application number: 10/963,492
- Filed: 2004-10-11
- Published: 2005-04-28
- Earliest claimed: 2003-10-28
- Assignees: Daido Tokushuko Kabushiki Kaisha; Denso Corporation
- Inventors: Takashi Kano; Yasuhiro Hazama; Junya Asaoka; Masaki Shimizu; Katsumi Mori; Hisashi Endo
- Web page: https://patentgrep.com/patent/US20050089437A1

## CPC

- C22C 38/22: with molybdenum or tungsten
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- F02M 55/025: {Common rails}
- F02M 61/168: {Assembling; Disassembling; Manufacturing; Adjusting}
- F02M 2200/8069: involving removal of material from the fuel apparatus, e.g. by punching, hydro-erosion or mechanical operation
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- F02M: SUPPLYING COMBUSTION ENGINES IN GENERAL WITH COMBUSTIBLE MIXTURES OR CONSTITUENTS THEREOF

## Abstract

The present invention is to provide a free-cutting steel capable of suppressing production of coarse inclusions, and having a high fatigue strength and a desirable machinability. The free-cutting steel aimed at solving the foregoing problems consists essentially of, in % by mass, C: 0.1-0.5%, Si: 0.05-2.5%, Mn: 0.1-3.5%, S: 0.0005-0.004%, Al: 0.01-0.06%, Ti: 0.003-0.01%, O: up to 0.0015%, N: 0.003-0.01%, Bi: 0.015-0.025%, and the balance of Fe and inevitable impurities, wherein the formula (1) below is satisfied: −4.8≦log(([N]−0.0015)×[Ti]0.98)≦−4.3 formula (1).

## Claims

### Claim 1

A free-cutting steel consisting essentially of, in % by mass, C: 0.1-0.5%, Si: 0.05-2.5%, Mn: 0.1-3.5%, S: 0.0005-0.004%, Al: 0.01-0.06%, Ti: 0.003-0.01%, 0: up to 0.0015%, N: 0.003-0.01%, Bi: 0.015-0.025%, and the balance of Fe and inevitable impurities, wherein the formula (1) below is satisfied:
−4.8≦log(([N]−0.0015)×[Ti]0.98)≦−4.3 formula (1).

### Claim 2 (depends on 1)

The free-cutting steel as claimed in claim 1, wherein, out of these inclusions reside in the steel texture:
a composite inclusion, in which a sulfide-base inclusion and a Bi metal inclusion are hybridized, has a maximum diameter {square root}{square root over ( )} AREAmax (MnS+Bi), estimated by the extreme value statistics, of 25 μm or less;
the sulfide-base inclusion as a single entity has a maximum diameter {square root}{square root over ( )} AREAmax (MnS), estimated by the extreme value statistics, of 20 μm or less; and
the Bi metal inclusion as a single entity has a maximum diameter {square root}{square root over ( )} AREAmax (Bi), estimated by the extreme value statistics, of 20 μm or less.

### Claim 3 (depends on 1)

The free-cutting steel as claimed in claim 1, wherein the steel further contains one or both of Cr: up to 3.5%, and Mo: up to 2%.

### Claim 4 (depends on 1)

A method of manufacturing the free-cutting steel as claimed in claim 1, wherein a Ti addition step for adding Ti, and a Bi addition step for adding Bi are carried out in this order, while keeping N concentration in a molten steel at 100 ppm or below.

### Claim 5 (depends on 2)

A method of manufacturing the free-cutting steel as claimed in claim 2, wherein a Ti addition step for adding Ti, and a Bi addition step for adding Bi are carried out in this order, while keeping N concentration in a molten steel at 100 ppm or below.

### Claim 6 (depends on 3)

A method of manufacturing the free-cutting steel as claimed in claim 3, wherein a Ti addition step for adding Ti, and a Bi addition step for adding Bi are carried out in this order, while keeping N concentration in a molten steel at 100 ppm or below.

### Claim 7 (depends on 4)

The method of manufacturing the free-cutting steel as claimed in claim 4, wherein said Bi addition step is carried out so as to add Bi at a rate of addition of 0.05 kg per minute and per ton of molten steel to 0.20 kg per minute and per ton of molten steel, both ends inclusive.

### Claim 8 (depends on 5)

The method of manufacturing the free-cutting steel as claimed in claim 5, wherein said Bi addition step is carried out so as to add Bi at a rate of addition of 0.05 kg per minute and per ton of molten steel to 0.20 kg per minute and per ton of molten steel, both ends inclusive.

### Claim 9 (depends on 6)

The method of manufacturing the free-cutting steel as claimed in claim 6, wherein said Bi addition step is carried out so as to add Bi at a rate of addition of 0.05 kg per minute and per ton of molten steel to 0.20 kg per minute and per ton of molten steel, both ends inclusive.

### Claim 10 (depends on 1)

A fuel injection system component composed of the free-cutting steel as claimed in claim 1.

### Claim 11 (depends on 2)

A fuel injection system component composed of the free-cutting steel as claimed in claim 2.

### Claim 12 (depends on 3)

A fuel injection system component composed of the free-cutting steel as claimed in claim 3.

### Claim 13 (depends on 1)

A fuel injection system component composed of the free-cutting steel as claimed in claim 1, having a joint hole.

### Claim 14 (depends on 2)

A fuel injection system component composed of the free-cutting steel as claimed in claim 2, having a joint hole.

### Claim 15 (depends on 3)

A fuel injection system component composed of the free-cutting steel as claimed in claim 3, having a joint hole.