# US 2005/0088261 A1 · Method of making a micromechanical device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2005/0088261 A1
- Document ID: US20050088261A1
- Status: Published application
- Kind: A1
- Application number: 10/692,548
- Filed: 2003-10-24
- Published: 2005-04-28
- Earliest claimed: 2003-10-24
- Inventors: Lianjun Liu; Steven Smith
- Web page: https://patentgrep.com/patent/US20050088261A1

## CPC

- B81C 1/00142: {Bridges (deformable micromirrors G02B26/0841)}
- B81B 2201/016: having a bridge fixed on two ends and connected to one or more dimples
- B81C: PROCESSES OR APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OR TREATMENT OF MICROSTRUCTURAL DEVICES OR SYSTEMS (making microcapsules or microballoons B01J13/02; processes or apparatus specially adapted for the manufacture or treatment of piezoelectric, electrostrictive or magnetostrictive elements per se H10N30/01)
- B81B: MICROSTRUCTURAL DEVICES OR SYSTEMS, e.g. MICROMECHANICAL DEVICES (piezoelectric, electrostrictive or magnetostrictive elements per se H10N30/00, H10N35/00)

## Abstract

A method of making a micromechanical device including forming a dielectric layer over a sacrificial layer, wherein the dielectric layer includes silicon, oxygen and nitrogen. In on embodiment, the dielectric layer is silicon oxynitride formed using plasma enhanced chemical vapor deposition (PECVD). Silicon oxynitride can easily be formed as a low stress material, unlike silicon dioxide, and does not have a large charge trap density like silicon nitride.

## Claims

### Claim 1

A method of making a device comprising the steps of:
providing a substrate;
forming a first conductive layer over the substrate;
forming a sacrificial layer over the first conductive layer;
forming a dielectric layer over the sacrificial layer, wherein the dielectric layer comprises silicon, oxygen, and nitrogen.
forming a second conductive layer over the sacrificial; and
removing the sacrificial layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein the forming the sacrificial layer comprises forming a polyimide layer.

### Claim 3 (depends on 1)

The method of claim 1, wherein the forming the dielectric layer further comprises forming a silicon oxynitride.

### Claim 4 (depends on 3)

The method of claim 3, wherein forming the silicon oxynitride comprises performing plasma enhanced chemical vapor deposition (PECVD).

### Claim 5 (depends on 4)

The method of claim 4, wherein performing PECVD further comprises:
flowing N2O;
flowing N2;
flowing NH3; and
flowing SiH4.

### Claim 6 (depends on 5)

The method of claim 5, wherein performing PECVD occurs at a temperature between approximately 200 and 300 degrees Celsius.

### Claim 7 (depends on 6)

The method of claim 6, wherein the temperature is approximately 240 degrees Celsius.

### Claim 8 (depends on 1)

The method of claim 1, wherein the dielectric layer further comprises hydrogen.

### Claim 9

A method of making a microelectronic device comprising the steps of:
providing a substrate;
forming an input signal line over the substrate;
forming an output signal line over the substrate and spaced apart from the input signal line;
forming a sacrificial layer over the input signal line and the output signal line;
forming a dielectric layer over the sacrificial layer, wherein the dielectric layer comprises silicon, oxygen and nitrogen;
removing the sacrificial layer; and
forming a conductive layer over the dielectric layer

### Claim 10 (depends on 9)

The method of claim 9, wherein forming the dielectric layer further comprises forming silicon oxynitride.

### Claim 11 (depends on 10)

The method of claim 10, wherein forming the silicon oxynitride comprises performing plasma enhanced chemical vapor deposition (PECVD).

### Claim 12 (depends on 11)

The method of claim 11, wherein performing PECVD occurs at a temperature between approximately 200 and 300 degrees Celsius.

### Claim 13 (depends on 12)

The method of claim 12, wherein the temperature is approximately 240 degrees Celsius.

### Claim 14

A microelectronic device comprising:
a substrate;
a first conductive layer over the substrate;
a dielectric layer over the first conductive layer, wherein the dielectric layer comprises silicon, oxygen, and nitrogen;
a gap between the first conductive layer and the dielectric layer; and
a second conductive layer over the dielectric layer.

### Claim 15 (depends on 14)

The microelectronic device of claim 14, wherein the dielectric layer further comprises silicon oxynitride.

### Claim 16 (depends on 14)

The microelectronic device of claim 14, wherein the dielectric layer is part of a cantilever structure.

### Claim 17

A method of making a device comprising the steps of:
providing a substrate;
forming a first conductive layer over the substrate;
forming a sacrificial layer over the first conductive layer;
forming a dielectric layer over the sacrificial layer, wherein the dielectric layer comprises a silicon oxynitride;
forming a second conductive layer over the sacrificial layer; and
removing the sacrificial layer.

### Claim 18 (depends on 17)

The method of claim 17, wherein forming the silicon oxynitride comprises performing plasma enhanced chemical vapor deposition (PECVD).

### Claim 19 (depends on 18)

The method of claim 18, wherein performing PECVD occurs at a temperature between approximately 200 and 300 degrees Celsius.

### Claim 20 (depends on 19)

The method of claim 19, wherein the temperature is approximately 240 degrees Celsius.