# US 2005/0087792 A1 · Method for fabricating a silicon nanocrystal, silicon nanocrystal, method for fabricating a floating gate type memory capacitor structure, and floating gate type memory capacitor structure

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2005/0087792 A1
- Document ID: US20050087792A1
- Status: Published application
- Kind: A1
- Application number: 10/925,966
- Filed: 2004-08-26
- Published: 2005-04-28
- Earliest claimed: 2003-10-23
- Assignees: National University Corporation Nagoya University
- Inventors: Hiroki Kondo; Yukio Yasuda; Shigeaki Zaima; Akira Sakai; Mitsuo Sakashita; Shinya Naito; Masaki Satake
- Web page: https://patentgrep.com/patent/US20050087792A1

## CPC

- H10D 64/035: {comprising conductor-insulator-conductor-insulator-semiconductor structures}
- B82Y 10/00: Nanotechnology for information processing, storage or transmission, e.g. quantum computing or single electron logic
- H10D 30/6893: {wherein the floating gate has multiple non-connected parts, e.g. multi-particle floating gate}
- H10P 14/24: using chemical vapour deposition [CVD]
- H10P 14/2905: {Silicon, silicon germanium or germanium}
- H10P 14/3238: {being insulating materials}
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10P 14/3461: {Nanoparticles}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A silicon oxide layer is formed at a surface region of a silicon substrate. Then, an amorphous silicon layer 13 is formed preferably in a thickness of 1 nm or below on the silicon substrate via the silicon oxide layer. Then, the amorphous silicon layer 13 is exposed to a silane gas preferably with heating the silicon substrate within a temperature range of 400-800° C. to form a high density and minute silicon nanocrystal.

## Claims

### Claim 1

A method for fabricating a silicon nanocrystal, comprising the steps of:
forming an amorphous silicon layer on a silicon substrate, and
supplying a raw material gas onto said amorphous silicon layer to form a silicon nanocrystal.

### Claim 2 (depends on 1)

The fabricating method as defined in claim 1, wherein a thickness of said amorphous silicon layer is set to 1 nm or below.

### Claim 3 (depends on 1)

The fabricating method as defined in claim 1, wherein said raw material gas is a silane gas.

### Claim 4 (depends on 1)

The fabricating method as defined in claim 1, wherein said amorphous silicon layer is exposed to said raw material gas with heating said silicon substrate to form said silicon nanocrystal.

### Claim 5 (depends on 4)

The fabricating method as defined in claim 4, wherein said silicon substrate is heated within a temperature range of 200-1000° C.

### Claim 6 (depends on 1)

The fabricating method as defined in claim 1, wherein a number density of said silicon nanocrystal is 1×1012/cm2 or over.

### Claim 7 (depends on 1)

The fabricating method as defined in claim 1, wherein a crystal grain size of said silicon nanocrystal is 10 nm or below.

### Claim 8

A silicon nanocrystal comprising a number density of 1×1012/cm2 or over, wherein said silicon nanocrystal is formed on a silicon substrate.

### Claim 9 (depends on 8)

The silicon nanocrystal as defined in claim 8, further comprising a crystal grain size of 10 nm or below.

### Claim 10

A method for fabricating a floating gate type memory capacitor structure, comprising the steps of:
forming a silicon oxide layer at a surface region of a silicon substrate,
forming an amorphous silicon layer on said silicon substrate via said silicon oxide layer,
supplying a raw material gas onto said amorphous silicon layer to form a silicon nanocrystal,
oxidizing a surface region of said silicon nanocrystal,
forming an additional amorphous silicon layer so as to embed said silicon nanocrystal,
thermally oxidizing said additional amorphous silicon layer to form an additional silicon oxide layer, and
forming an electrode on said additional silicon oxide layer.

### Claim 11 (depends on 10)

The fabricating method as defined in claim 10, wherein a thickness of said amorphous silicon layer is set to 1 nm or below.

### Claim 12 (depends on 10)

The fabricating method as defined in claim 10, wherein said raw material gas is a silane gas.

### Claim 13 (depends on 10)

The fabricating method as defined in claim 10, wherein said amorphous silicon layer is exposed to said raw material gas with heating said silicon substrate to form said silicon nanocrystal.

### Claim 14 (depends on 13)

The fabricating method as defined in claim 13, wherein said silicon substrate is heated within a temperature range of 200-1000° C.

### Claim 15 (depends on 10)

The fabricating method as defined in claim 10, wherein a number density of said silicon nanocrystal is 1×1012/cm2 or over.

### Claim 16 (depends on 10)

The fabricating method as defined in claim 10, wherein before said oxidizing of said surface region of said silicon nanocrystal, a crystal grain size of said silicon nanocrystal is 10 nm or below.

### Claim 17 (depends on 10)

The fabricating method as defined in claim 10, wherein after said thermally oxidizing of said additional silicon oxide layer, a crystal grain size of said silicon nanocrystal is 10 nm or below.

### Claim 18

A floating gate type memory capacitor structure comprising:
a silicon nanocrystal formed on a silicon nanocrystal and having a number density of 1×1012/cm2 or over, and
an electrode formed above said silicon nanocrystal via a silicon oxide layer,
wherein said silicon nanocrystal functions as a memory.

### Claim 19 (depends on 18)

The floating gate type capacitor structure as defined in claim 18, wherein said silicon nanocrystal has a crystal grain size of 10 nm or below.