# US 2005/0087778 A1 · Semiconductor device and method of manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2005/0087778 A1
- Document ID: US20050087778A1
- Status: Published application
- Kind: A1
- Application number: 10/986,652
- Filed: 2004-11-12
- Published: 2005-04-28
- Earliest claimed: 2001-03-16
- Assignees: Fujitsu Limited
- Inventors: Yasuo Gamo; Koji Takahashi
- Web page: https://patentgrep.com/patent/US20050087778A1

## CPC

- H10D 64/0134: {with a treatment, e.g. annealing, after the formation of the insulator and before the formation of the conductor}
- H10B 43/30: characterised by the memory core region
- H10B 69/00: Erasable-and-programmable ROM [EPROM] devices not provided for in groups H10B41/00 - H10B63/00, e.g. ultraviolet erasable-and-programmable ROM [UVEPROM] devices
- H10D 64/685: {being perpendicular to the channel plane}
- H10D 64/693: {the insulator comprising nitrogen, e.g. nitrides, oxynitrides or nitrogen-doped materials}
- H10D 64/01342: {by deposition, e.g. evaporation, ALD or laser deposition (H10D64/01344 takes precedence)}
- H10P 14/662: {Laminate layers, e.g. stacks of alternating high-k metal oxides (adhesion layers or buffer layers H10P14/6508, H10P14/6548)}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P 14/69433: {the material being a silicon nitride not containing oxygen, e.g. SixNy or SixByNz}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10B: ELECTRONIC MEMORY DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

To ensure sufficient electrical insulation between bit and word lines and realize excellent charge holding characteristic by suppressing undesirable bird's beak formation, a buried bit line type flash memory includes bit lines formed by ion-implanting impurities into a semiconductor substrate, said bit lines serving also as sources and drains, and word lines crossing said bit lines and serving also as gate electrodes. After the impurity ion implantation for forming the bit lines and annealing for activating the impurities, an ONO film having a three-layer structure of silicon oxide film/silicon nitride film/silicon oxide film is formed.

## Claims

### Claim 1

A semiconductor device manufacturing method comprising:
a first step of introducing impurities into a surface layer in an active region of a semiconductor substrate and annealing said semiconductor substrate to form source and drain regions;
after said first step, a second step of forming a multilayer film so as to cover said active region, said multilayer film being made up from at least three layers, in which a first insulating film having a charge trap function is sandwiched by second and third insulating films from upper and lower sides of said first insulating film; and
a third step of depositing an electrode material on said multilayer film and patterning said electrode material and said multilayer film to form a gate electrode, said gate electrode being located over said semiconductor substrate with said multilayer film being interposed between them.

### Claim 2 (depends on 1)

The method according to claim 1, wherein, in said third step, said gate electrode is formed at the position between said source and drain regions over said semiconductor substrate with said multilayer film being interposed between said gate electrode and said source and drain regions.

### Claim 3 (depends on 1)

The method according to claim 1, wherein, in said first step, after said impurities are introduced, a substance having an accelerated oxidation suppressing function is subsequently introduced into said active region, and then said semiconductor substrate is annealed to form said source and drain regions.

### Claim 4 (depends on 3)

The method according to claim 3, wherein said substance having an accelerated oxidation suppressing function is one selected from the group of nitrogen, carbon, and compounds containing nitrogen or carbon.

### Claim 5 (depends on 4)

The method according to claim 4, wherein, as said substance having an accelerated oxidation suppressing function, nitrogen or carbon ions are implanted into said active region.

### Claim 6 (depends on 4)

The method according to claim 4, wherein said substance having an accelerated oxidation suppressing function is one selected from the group of NO2, NO, NH3, and CxHy (x and y are appropriate numbers), and annealing is performed in an atmosphere of said substance to dope said active region with said substance.

### Claim 7 (depends on 5)

The method according to claim 5, wherein said substance having an accelerated oxidation suppressing function is ion implanted obliquely to a surface of said active region.

### Claim 8 (depends on 1)

The method according to claim 1, wherein said first insulating film having a charge trap function is a silicon nitride film.

### Claim at position 9

9-13. (canceled)

### Claim 14

A method of manufacturing a semiconductor device comprising: a semiconductor substrate;
source and drain regions formed in a surface layer of said semiconductor substrate;
a multilayer film formed on said semiconductor substrate between said source and drain regions, said multilayer film being made up from at least three layers, in which a first insulating film having a charge trap function is sandwiched by second and third insulating films from upper and lower sides of said first insulating film; and
a gate electrode formed on said multilayer film,
said method comprising the steps of:
introducing impurities into a surface layer in an active region of said semiconductor substrate;
annealing said semiconductor substrate to form said source and drain regions; and forming said multilayer film.

### Claim 15 (depends on 14)

The method according to claim 14, wherein said gate electrode is formed at the position between said source and drain regions over said semiconductor substrate with said multilayer film being interposed between said gate electrode and said source and drain regions.

### Claim 16 (depends on 14)

The method according to claim 14, wherein, after said impurities are introduced, a substance having an accelerated oxidation suppressing function is subsequently introduced into said active region, and then said semiconductor substrate is annealed to form said source and drain regions.

### Claim 17 (depends on 16)

The method according to claim 16, wherein said substance having an accelerated oxidation suppressing function is one selected from the group of nitrogen, carbon, and compounds containing nitrogen or carbon.

### Claim 18 (depends on 17)

The method according to claim 17, wherein, as said substance having an accelerated oxidation suppressing function, nitrogen or carbon ions are implanted into said active region.

### Claim 19 (depends on 17)

The method according to claim 17, wherein said substance having an accelerated oxidation suppressing function is one selected from the group of NO2, NO, NH3, and CxHy (x and y are appropriate numbers), and annealing is performed in an atmosphere of said substance to dope said active region with said substance.

### Claim 20 (depends on 18)

The method according to claim 18, wherein said substance having an accelerated oxidation suppressing function is ion implanted obliquely to a surface of said active region.

### Claim 21 (depends on 14)

The method according to claim 14, wherein said first insulating film having a charge trap function is a silicon nitride film.