# US 2005/0087746 A1 · Group III-nitride on Si using epitaxial BP buffer layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2005/0087746 A1
- Document ID: US20050087746A1
- Status: Published application
- Kind: A1
- Application number: 10/691,055
- Filed: 2003-10-22
- Published: 2005-04-28
- Earliest claimed: 2003-10-22
- Assignees: University of Florida Research Foundation, Inc.
- Inventors: Olga Kryliouk; Tim Anderson; Omar Bchir; Kee Kim
- Web page: https://patentgrep.com/patent/US20050087746A1

## CPC

- H10H 20/815: having stress relaxation structures, e.g. buffer layers
- H10H 20/01335: {the light-emitting regions comprising nitride materials}
- H10P 14/24: using chemical vapour deposition [CVD]
- H10P 14/2905: {Silicon, silicon germanium or germanium}
- H10P 14/3218: {Phosphides}
- H10P 14/3416: {Nitrides}
- H10P 14/3602: {In-situ cleaning}
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A semiconductor device and method for forming the same includes a silicon (111) single crystal substrate, and an epitaxial boron phosphide (BP) layer disposed on the substrate. A group III-nitride semiconductor epitaxial layer is disposed on the BP epitaxial layer.

## Claims

### Claim 1

A semiconductor device, comprising:
a silicon (111) single crystal substrate;
a single crystal epitaxial boron phosphide (BP) comprising layer disposed directly on said substrate, and
a group III-nitride semiconductor epitaxial layer disposed directly on said BP layer.

### Claim 2

(canceled)

### Claim 3 (depends on 1)

The device of claim 1, wherein said group III-nitride layer comprises GaN.

### Claim 4 (depends on 3)

The device of claim 3, wherein said GaN layer is single crystal.

### Claim 5 (depends on 1)

The device of claim 1, wherein said buffer layer has a thickness in the range of 0.1-10 μm.

### Claim 6

A light-emitting diode (LED), comprising:
a silicon (111) single crystal substrate;
a single crystal epitaxial boron phosphide (BP) comprising layer disposed directly on said substrate;
a group III-nitride semiconductor epitaxial layer on said BP layer, and
an active layer comprising InxGa1-xN disposed directly on said group III-nitride layer.

### Claim 7 (depends on 6)

The LED of claim 6, wherein said BP layer is a single crystal.

### Claim 8 (depends on 6)

The LED of claim 6, wherein said group III-nitride layer comprises GaN.

### Claim 9 (depends on 6)

The LED of claim 6, wherein one terminal of said LED is contacted through said silicon substrate.

### Claim 10 (depends on 6)

The LED of claim 6, father comprising a first and second cladding layer sandwiching said active layer.

### Claim 11 (depends on 6)

The LED of claim 6, wherein said active layer comprises InxGa1-xN, wherein 0≦X≦1.

### Claim 12

A method for forming group III-nitride articles, comprising the steps of
providing a single crystal (111) silicon substrate,
depositing a single crystal epitaxial boron phosphide (BP) comprising layer disposed directly on said substrate, and
depositing an epitaxial group III-nitride semiconductor epitaxial layer disposed directly on said BP layer.

### Claim 13 (depends on 12)

The method of claim 12, wherein said BP layer is a single crystal.

### Claim 14 (depends on 12)

The method of claim 12, wherein said group III-nitride layer comprises single crystal GaN.

### Claim 15 (depends on 12)

The method of claim 12, farther comprising the step of in-situ removal of native oxide on a surface of said Si substrate in a reactor used for depositing said BP prior to depositing said BP.

### Claim 16 (depends on 15)

The method of claim 15, wherein said in-situ removal comprises hydrogen reduction.