# US 2005/0037596 A1 · Internal gettering in SIMOX SOI silicon substrates

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2005/0037596 A1
- Document ID: US20050037596A1
- Status: Published application
- Kind: A1
- Application number: 10/640,917
- Filed: 2003-08-14
- Published: 2005-02-17
- Earliest claimed: 2003-08-14
- Assignees: Ibis Technology Corporation
- Inventors: Yuri Erokhin; Kevin Dempsey
- Web page: https://patentgrep.com/patent/US20050037596A1

## CPC

- H10P 30/209: {in silicon to make buried insulating layers}
- H10P 36/07: {of silicon-on-insulator structures}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

The present invention provides methods for forming SOI wafers having internal gettering layers for sequestering metallic impurities. More particularly, in one embodiment of the invention, a plurality of sites for sequestering metallic impurities are formed in a silicon substrate by implanting a selected dose of oxygen ions therein. In one embodiment, an epitaxial layer of crystalline silicon is formed over the substrate, and a buried continuous oxide layer is generated in the epitaxial layer, for example, by employing a SIMOX process.

## Claims

### Claim 1

A method for processing a silicon substrate, comprising the steps of
implanting a dose of an ion into the substrate so as to generate a plurality of sites for sequestering metallic impurities present in said substrate,
implanting oxygen ions in said substrate to generate a buried oxygen-rich layer, and
annealing said substrate to generate a continuous buried oxide layer in said oxygen-rich layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein said plurality of sites comprise precipitation sites and/or associated structural defects generated by interaction of said implanted ions with said substrate.

### Claim 3 (depends on 1)

The method of claim 1, further comprising selecting said implanted ions for generating sequestering sites to be oxygen ions.

### Claim 4 (depends on 3)

The method of claim 3, wherein said sequestering sites comprise oxide precipitates.

### Claim 5 (depends on 3)

The method of claim 3, wherein the step of implanting oxygen ions comprises exposing the substrate to a beam of oxygen ions having an energy in a range of about 30 to about 300 keV.

### Claim 6 (depends on 3)

The method of claim 3, further comprising selecting the implanted oxygen dose for generating the sequesteration sites to be in a range of about 5×1015 cm−2 to about 1×1018 cm−2.

### Claim 7 (depends on 6)

The method of claim 6, further comprising selecting the implanted oxygen dose for generating the sequestration sites to be in a range of about 5×1016 cm−2 to about 2×1017 cm−2.

### Claim 8 (depends on 6)

The method of claim 6, further comprising selecting the implanted oxygen dose for generating the oxygen-rich layer to be in a range of about 1016 to about 1018 cm−2.

### Claim 9 (depends on 1)

The method of claim 1, wherein the annealing step comprises maintaining the substrate at a temperature in a range of about 1150 C to about 1400 C for period of a few hours.

### Claim 10

A method for processing a silicon substrate, comprising the steps of:
generating a plurality of sites for gettering metallic impurities below a surface of the substrate,
growing an epitaxial layer of crystalline silicon over said substrate surface, and
generating a continuous insulating layer in said crystalline epitaxial silicon layer.

### Claim 11 (depends on 10)

The method of claim 10, wherein the step of generating a plurality of gettering sites comprises implanting a dose of oxygen ions in said substrate.

### Claim 12 (depends on 11)

The method of claim 11, further comprising selecting a dose of implanted oxygen ions to be in a range of about 5×1010 cm−2 to about 1×1018 cm−2

### Claim 13 (depends on 12)

The method of claim 12, further comprising selecting a dose of the implanted oxygen ions to be in a range of about 5×1016 cm−2 to about 2×1017 cm−2.

### Claim 14 (depends on 11)

The method of claim 11, wherein the step of implanting a dose of oxygen ions comprises exposing the substrate to a beam of oxygen ions having an energy in a range of about 30 to about 300 keV.

### Claim 15 (depends on 10)

The method of claim 10, wherein the step of generating a continuous insulating layer comprises
implanting a dose of oxygen ions in said epitaxial layer to generate a damaged buried layer, and
annealing said substrate at an elevated temperature to generate a continuous insulating layer in said buried damaged layer.

### Claim 16 (depends on 15)

The method of claim 15, further comprising selecting said dose of implanted oxygen for generating a buried damaged layer to be in a range of about 1016 to about 1018 cm−2.

### Claim 17 (depends on 15)

The method of claim 15, wherein said annealing step comprises maintaining said substrate at a temperature in a range of about 1100 C to about 1400 C for a time period of a few hours.

### Claim 18

A method for processing a silicon substrate, comprising the steps of
implanting a first dose of oxygen ions through a first surface of the substrate to generate a plurality of sites for gettering metallic impurities in a region below said first surface,
growing an epitaxial crystalline layer of silicon over a second surface of the substrate opposed to said first surface,
generating a buried continuous oxide layer within said epitaxial layer of silicon.

### Claim 19 (depends on 18)

The method of claim 18, wherein the step of generating a buried continuous oxide layer comprises:
implanting a second dose of oxygen ions through a top surface of said epitaxial layer to generate a buried oxygen-rich layer, and
annealing said substrate at an elevated temperature to generate said continuous oxide layer within said buried oxygen rich layer.

### Claim 20 (depends on 19)

The method of claim 19, further comprising selecting said second dose of oxygen ions to be in a range of about 1016 to about 1018 cm−2.

### Claim 21 (depends on 19)

The method of claim 19, wherein said annealing step comprises maintaining said substrate at a temperature in a range of about 1100 C to about 1400 C for a time period of a few hours.

### Claim 22

A method of generating an SOI wafer, comprising
generating a first set of sequestration sites for gettering metallic impurities in a silicon wafer by exposing said wafer to a beam of oxygen ions having a first energy to implant first dose of oxygen ions therein,
generating a second set of sequestration sites in said wafer by exposing the wafer to a beam of oxygen ions having a second energy different than said first energy to implant a second dose of oxygen ions therein,
forming an epitaxial layer of silicon over said wafer, and
generating a buried continuous oxide layer in said epitaxial layer.

### Claim 23 (depends on 22)

The method of claim 22, wherein said first oxygen dose is selected to be in a range of about 2×1015 to about 5×107 cm−2.

### Claim 24 (depends on 23)

The method of claim 23, wherein said second oxygen dose is selected to be in a range of about 2×1015 to about 5×1017 cm−2.

### Claim 25 (depends on 24)

The method of claim 24, wherein a sum of said first oxygen dose and said second oxygen dose is selected to be in a range of about 4×1015 to about 1018 cm−2.

### Claim 26 (depends on 22)

The method of claim 22, wherein the step of generating a buried continuous oxide layer in said epitaxial layer comprises
implanting a selected dose of oxygen ions in said epitaxial layer to generate a buried oxygen-rich layer therein, and
annealing said wafer to cause formation of a buried continuous oxide layer within said oxygen-rich layer.

### Claim 27 (depends on 26)

The method of claim 26, wherein said annealing step comprises maintaining said wafer at an elevated temperature in a range of about 1100 C to about 1400 C for a time period in a range of about 2 hours to about 16 hours.

### Claim 28

An SOI wafer, comprising
a silicon substrate,
a continuous buried oxide layer formed below a surface of said substrate,
at least two buried gettering layers having a plurality of sites for preferential sequestration of metallic impurities.