# US 2005/0029696 A1 · Method of manufacturing continuous foam from thermoplastic elastomeric material in atmosphere

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2005/0029696 A1
- Document ID: US20050029696A1
- Status: Published application
- Kind: A1
- Application number: 10/824,466
- Filed: 2004-04-15
- Published: 2005-02-10
- Earliest claimed: 2003-08-07
- Assignees: Microcell Composite Company
- Inventors: Chun-Hsiung Wu; Ruey-Sheng Shih
- Web page: https://patentgrep.com/patent/US20050029696A1

## CPC

- C08J 9/103: {Azodicarbonamide}
- B29C 44/06: Making multilayered articles {(B29C44/0407 - B29C44/0492 take precedence)}
- B29C 44/20: for articles of indefinite length
- C08J 9/08: developing carbon dioxide
- C08J 2201/03: Extrusion of the foamable blend
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)

## Abstract

The present invention is to provide a method of manufacturing continuous foam from a thermoplastic elastomeric composite in atmosphere, which comprises the steps of using thermoplastic elastomer as a raw material, adding different composing agent, foaming agent, and crosslinking agent into the raw material, kneading and rolling the raw material for forming a continuous sheet by means of a conventional rubber continuous foaming device, baking the sheet in an oven, foaming the heated sheet in a normal pressure, and cooling the foamed sheet to produce the foam material of the present invention.

## Claims

### Claim 1

A method of manufacturing a continuous foam from a thermoplastic elastomeric composite in atmosphere, comprising the steps of:
using a thermoplastic elastomer as a raw material;
adding different additive, foaming agent, and crosslinking agent into the raw material;
kneading and rolling the raw material for forming a continuous sheet by means of conventional rubber continuous foaming techniques and devices;
cutting the continuous sheet and weighing the sheatsto an oven;
foaming the heated sheet in a normal pressure; and
cooling the foamed sheet to produce the continuous foam.

### Claim 2 (depends on 1)

The method of claim 1, wherein the thermoplastic elastomer as the raw material is selected from a styrenic thermoplastic elastomer including a styrene butadiene styrene (SBS), a styrene-ethylene/butene-styrene (SEBS), a styrene isoprene styrene (SIS), and a styrene ethylene propylene styrene (SEPS) having a percentage about 50% to 100% of the total weight of the raw material.

### Claim 3 (depends on 2)

The method of claim 2, wherein the thermoplastic elastomer further comprises polymeric materials including styrene butadiene rubber (SBR), polystyrene (PS), ethylene vinyl acetate (EVA), low density polyethylene (LDPE), and ethylene-propylene-diene terpolymer rubber (EPDM) having a percentage about 0% to 50% of the total weight of the raw material.

### Claim 4 (depends on 2)

The method of claim 2, wherein components of the thermoplastic elastomeric composite in a predetermined weight percentage are poured into the conventional devices for uniformly mixing by kneading and rolling in a temperature ranged from about 90° C. to 130° C.

### Claim 5 (depends on 4)

The method of claim 4, wherein the continuous sheet is baked in the oven in a temperature ranged from about 150° C. to 180° C. in a normal pressure for a predetermined period of time for foaming the continuous sheet to produce a foam material.

### Claim 6 (depends on 2)

The method of claim 2, wherein the foaming agent is selected from a chemical foaming agent (e.g., azodicarbonamide) or a physical foaming agent including sodium bicarbonate having a percentage about 1% to 15% of the total weight of the raw material.

### Claim 7 (depends on 6)

The method of claim 6, wherein the crossling agent is selected from a dicumyl peroxide, 2,5-(tert-butylperoxide)-2,5-dimethylhexane or sulfur having a percentage about 0.1% to 1% of the total weight of the raw material.

### Claim 8 (depends on 7)

The method of claim 7, wherein the thermoplastic elastomer further comprises accelarator for foaming agent selected from a zinc oxide or urea having a percentage about 0% to 3% of the total weight of the raw material.

### Claim 9 (depends on 7)

The method of claim 7, wherein the thermoplastic elastomer further comprises a processing agent selected from stearate or hard zinc based stearate.

### Claim 10 (depends on 7)

The method of claim 7, wherein the thermoplastic elastomer further comprises an additive including a coloring agent, a calcium carbonate, and wood chips.

### Claim 11 (depends on 7)

The method of claim 7, wherein the thermoplastic elastomer further comprises an functional additive selected from an anti-static agent, a flame retardation agent, or a reinforced agent having a percentage about 0.1% to 50% of the total weight of the raw material.

### Claim 12

A method of manufacturing a continuous foam from a thermoplastic elastomeric composite in atmosphere, comprising the steps of:
using a thermoplastic elastomer as a raw material;
adding different additive, foaming agent, and crosslinking agent into the raw material;
kneading and rolling above materials for forming a continuous sheet by means of conventional rubber continuous foaming techniques and devices;
cutting the continuous sheet into a plurality of sheet members with a predetermined size;
stacking a selected weight of the sheet members depending on requirements;
cutting the selected weight of the sheet members to a mold to heat for forming a blank;
cutting the blank to an oven to foam in a normal pressure; and
cooling the foamed blank to produce a foam material having a predetermined shape.

### Claim 13 (depends on 12)

The method of claim 12, wherein the thermoplastic elastomer as the raw material is selected from a styrenic thermoplastic elastomer including styrene butadiene styrene (SBS), styrene-ethylene/butene-styrene (SEBS), styrene isoprene styrene (SIS), or styrene ethylene propylene styrene (SEPS) having a percentage about 50% to 100% of the total weight of the raw material.

### Claim 14 (depends on 13)

The method of claim 13, wherein the components of the thermoplastic elastomeric composite in a predetermined weight percentage are poured into the conventional devices for uniformly mixing by kneading and rolling in a temperature ranged from about 90° C. to 130° C.

### Claim 15 (depends on 14)

The method of claim 14, wherein responsive to uniformly mixing the components of the thermoplastic elastomeric composite, the uniformly mixed components of the thermoplastic elastomeric composite are transported to a two-roll mill for rolling a predetermined number of times to form a continuous sheet with required thickness prior to cutting into a plurality of sheet members with the predetermined size by means of an automatic cutter.

### Claim 16 (depends on 15)

The method of claim 15, further comprising the steps of:
stacking a selected weight of sheet members having a required weight; and
cutting the selected weight of sheet members to the mold to heat in a temperature ranged from about 150° C. to 180° C. in a pressure about 90 to 250 kg/cm2,
wherein the blank is formed after heating a predetermined period of time.

### Claim 17 (depends on 12)

The method of claim 12, wherein the foaming agent is selected from a chemical foaming agent (e.g., azodicarbonamide) or a physical foaming agent including sodium bicarbonate having a percentage about 1% to about 15% of the total weight of the raw material.

### Claim 18 (depends on 17)

The method of claim 17, wherein the crosslinking agent is selected from a dicumyl peroxide, 2,5-(tert-butylperoxide)-2,5-dimethylhexane or sulfur having a percentage about 0.1% to 1% of the total weight of the raw material.

### Claim 19 (depends on 18)

The method of claim 18, wherein the thermoplastic elastomer composite further comprises polymeric materials including styrene butadiene rubber (SBR), polystyrene (PS), ethylene vinyl acetate (EVA), low density polyethylene (LDPE), and ethylene-propylene-diene terpolymer rubber (EPDM) having a percentage about 0% to 50% of the total weight of the raw material.

### Claim 20 (depends on 18)

The method of claim 18, wherein the thermoplastic elastomer composite further comprises a accelarator for foaming agent selected from a zinc oxide or urea having a percentage about 0% to 3% of the total weight of the raw material.

### Claim 21 (depends on 18)

The method of claim 18, wherein the thermoplastic elastomer composite further comprises a processing agent selected from stearate or stearate.

### Claim 22 (depends on 18)

The method of claim 18, wherein the thermoplastic elastomer composite further comprises an additive including a coloring agent, a calcium carbonate, and wood chips.

### Claim 23 (depends on 18)

The method of claim 18, wherein the thermoplastic elastomer composite further comprises an functional additive selected from an anti-static agent, a flame retardation agent, or a reinforced agent having a percentage about 0% to 50% of the total weight of the raw material.