# US 2005/0029614 A1 · High switching speed two mask schottky diode with high field breakdown

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2005/0029614 A1
- Document ID: US20050029614A1
- Status: Published application
- Kind: A1
- Application number: 10/633,500
- Filed: 2003-08-05
- Published: 2005-02-10
- Earliest claimed: 2003-08-05
- Assignees: Chip Integration Tech. Co., Ltd.
- Inventors: Shye-Lin Wu
- Web page: https://patentgrep.com/patent/US20050029614A1

## CPC

- H10D 8/605: {of the trench conductor-insulator-semiconductor barrier type, e.g. trench MOS barrier Schottky rectifiers [TMBS]}
- H10D 8/051: {of Schottky diodes}
- H10D 8/60: Schottky-barrier diodes
- H10D 62/107: {Buried supplementary regions, e.g. buried guard rings (multi-RESURF H10D62/111)}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A power Schottky rectifier device and its fabrication method are disclosed. The method comprises the following steps: First, a semiconductor substrate having a relatively heavily doped n+ doped layer and a lightly doped is provided. A buried p region is then formed in the epi layer by ion implantation. Afterward, a first oxide layer and a nitride layer are then successively formed on the epi layer. The result structure is then patterned to form trenches. Subsequently, a thermal oxidation step is performed to recover etch damage. A wet etch is then performed to remove the thin oxide layer in the trench to expose the silicon in the sidewall. After that, a silicidation process is then performed to form silicide layer on the n-epi-layer in the trenches. After a removal of un-reacted metal layer, a top metal layer is then formed on the silicide layer and on the first oxide layer or nitride layer. The top metal layer on the termination region portion is then patterned to define anode. Finally, after backside layers formed on the rear surface of the substrate are removed, another cathode layer is formed on the rear surface.

## Claims

### Claim at position 1

1-6. (Canceled)

### Claim 7

A power rectifier device, comprising:
a semiconductor substrate having a first conductive layer doped with first-type impurities, an epi layer formed thereon which is extended to a first surface thereof and is lightly doped with said first-type impurities;
a cathode metal layer formed on said first conductive layer opposite said first surface;
a first oxide layer formed on said first surface;
a pair of trenches formed through said first oxide layer and into a top of said epi-layer and spaced from each other by a first mesa region;
a termination mesa region surrounding said pair of cell trenches;
a second conductive type doped region formed into said epi layer of said first mesa region and said termination mesa region, wherein said first mesa region and said termination mesa region are regions located on said first surface having said first oxide layer formed thereon;
a Schottky barrier silicide layer formed on said epi layer located on bottom and side surfaces of said trenches;
a top metal layer acted acting as an anode and formed on said Schottky barrier silicide layer and extended to cover all surfaces of said first mesas region and a portion of said termination mesa region.

### Claim 8 (depends on 7)

The power rectifier device according to claim 7 and further comprising a nitride layer formed in between said first oxide layer and said top metal layer.

### Claim 9 (depends on 8)

The power rectifier device according to claim 8 wherein said first oxide layer has a thickness between about 100-1000 nm and said nitride layer has a thickness between about 50-300 nm.

### Claim 10 (depends on 8)

The power rectifier device according to claim 8 wherein said trenches have a depth of between about 1 to 5 μm measured from the surface of said epi layer.

### Claim 11 (depends on 7)

The power rectifier device according to claim 7 wherein said Schottky barrier silicide layer is formed of metal silicide selected from the group consisting of silicide of Ti, Ni, Cr, Mo, Pt, Zr, and W with silicon.

### Claim 12 (depends on 7)