# US 2005/0028898 A1 · Method for the production of a siderurgical product made of carbon steel with a high copper content, and siderurgical product obtained according to said method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2005/0028898 A1
- Document ID: US20050028898A1
- Status: Published application
- Kind: A1
- Application number: 10/501,456
- Filed: 2003-01-13
- Published: 2005-02-10
- Earliest claimed: 2002-01-14
- Assignees: Usinor
- Inventors: Nicolas Guelton; Michel Faral; Jean-Pierre Birat; Catherine Juckum
- Web page: https://patentgrep.com/patent/US20050028898A1

## CPC

- C22C 38/04: containing manganese
- C21D 8/0415: {Rapid solidification; Thin strip casting}
- C21D 8/0426: {Hot rolling}
- C21D 8/0473: {Final recrystallisation annealing}
- C22C 1/02: by melting {(C22C1/1036 takes precedence)}
- C22C 38/16: containing copper
- C21D 2211/001: Austenite
- C21D 2211/004: Dispersions; Precipitations
- C21D 2211/005: Ferrite
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)

## Abstract

The invention relates to a method for producing a siderurgical product made of carbon steel having a high copper content, according to which:—a liquid steel having the composition: 0.0005%≦1%; O.5≦Cu≦10%; 0≦Mn≦2%; 0≦Si≦5% 0≦Ti≦0.5%; 0≦Nb≦0.5%; 0≦Ni≦5%; 0≦Al≦2%, the remainder being iron and impurities, is produced;—said liquid steel is poured directly in the form of a thin strip having a thickness of no more than 10 mm;—the strip is subjected to forced cooling and/or is surrounded by a non-oxidizing atmosphere while having a temperature of more than 1000? C.;—said thin strip is hot rolled at a reduction rate of at least 10%, the temperature at the end of the rolling process being such that all of the copper is still in a solid solution in the ferrite and/or austenite matrix;—and the strip is coiled. The invention also relates to a siderurgical product obtained according to said method.

## Claims

### Claim 1

Process for manufacturing a steel product made of copper-rich carbon steel, wherein:
a liquid steel is produced, which has the following composition, expressed as percentages by weight:
0,0005%≦C≦1%
0.5≦Cu≦10%
0≦Mn≦2%
0≦Si≦5%
0≦Ti≦0.5%
0≦Nb≦0.5%
0≦Ni≦5%
0≦Al≦2%
the remainder being iron and impurities resulting from production;
this liquid steel is cast directly into the form of a thin strip having a thickness less than or equal to 10 mm;
the strip is cooled rapidly to a temperature less than or equal to 1000° C.;
the thin strip is subjected to hot-rolling at a reduction rate of at least 10%, the end-of-rolling temperature being such that, at this temperature, all the copper is still in a solid solution in the ferrite and/or austenite matrix;
the strip is subjected to forced cooling so as to keep the copper in a supersaturated solid solution in the ferrite and/or austenite matrix;
and the strip is coiled.

### Claim 2 (depends on 1)

Process according to claim 1, characterised in that the Mn/Si ratio is greater than or equal to 3.

### Claim 3 (depends on 1)

Process according to claim 1, characterised in that the thin strip is cast on a casting installation between two internally cooled rolls rotating in opposite directions.

### Claim 4 (depends on 1)

Process according to claim 1, characterised in that hot-rolling of the strip is carried out in line with the casting of the strip.

### Claim 5 (depends on 1)

Process according to claim 1, characterised in that the rate V of forced cooling after hot-rolling is such that
V≧e1.98(% Cu)-0.08
wherein V is expressed in ° C./s and % Cu in % by weight.

### Claim 6 (depends on 1)

Process according to claim 1, characterised in that the carbon content of the steel is between 0.1 and 1% and in that the strip is coiled at a temperature higher than the temperature Ms at the beginning of martensitic transformation.

### Claim 7 (depends on 1)

Process according to claim 1, characterised in that the strip is coiled at less than 300° C. and in that the strip is then subjected to a copper precipitation heat treatment at between 400 and 700° C.

### Claim 8 (depends on 7)

Process according to claim 7, characterised in that the carbon content of the steel is between 0.1 and 1% and in that the strip is subjected to precipitation heat treatment without being uncoiled beforehand.

### Claim 9 (depends on 1)

Process according to claim 1, characterised in that coiling of the strip is carried out at a temperature which is both higher than the temperature Ms at which the martensitic transformation begins and lower than 300° C., and is followed by cold-rolling, recrystallisation annealing in a temperature range where the copper is in a supersaturated solid solution, forced cooling to keep the copper in a solid solution and precipitation tempering.

### Claim 10 (depends on 9)

Process according to claim 9, characterised in that said precipitation tempering is carried out at between 600 and 700° C. in a continuous annealing installation.

### Claim 11 (depends on 9)

Process according to claim 9, characterised in that said precipitation tempering is carried out at between 400 and 700° C. in a batch annealing installation.

### Claim 12 (depends on 1)

Process according to claim 1, characterised in that coiling of the strip is carried out at a temperature which is both higher than the temperature Ms at which the martensitic transformation begins and lower than 300° C. and is followed by cold-rolling and batch annealing at between 400 and 700° C. which acts as both recrystallisation annealing and precipitation tempering.

### Claim 13 (depends on 9)

Process according to claim 9, characterised in that the carbon content of the steel is between 0.1 and 1%.

### Claim 14 (depends on 9)

Process according to claim 9, characterised in that the carbon content of the steel is between 0.01 and 0.2%.

### Claim 15 (depends on 9)

Process according to claim 9, characterised in that the carbon content of the steel is between 0.0005% and 0.05% and in that its copper content is between 0.5 and 1.8%.

### Claim 16 (depends on 15)

Process according to claim 15, characterised in that, prior to precipitation hardening, the strip is cut to form a sheet which is shaped by drawing, and in that precipitation tempering is carried out on the drawn sheet.

### Claim 17 (depends on 1)

Process according to claim 1, characterised in that the strip is subjected to a final treatment in a skin-pass rolling mill.

### Claim 18 (depends on 1)

Steel product, characterised in that it is obtained by a process according to claim 1.