# US 2005/0028892 A1 · Alloy flake for rare earth magnet, production method thereof, alloy powder for rare earth intered magnet, rare earth sintered magnet, alloy powder for bonded magnet and bonded magnet

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2005/0028892 A1
- Document ID: US20050028892A1
- Status: Published application
- Kind: A1
- Application number: 10/498,932
- Filed: 2002-12-18
- Published: 2005-02-10
- Earliest claimed: 2001-12-18
- Assignees: Showa Denko K.K.
- Inventors: Shiro Sasaki
- Web page: https://patentgrep.com/patent/US20050028892A1

## CPC

- B22F 9/023: {Hydrogen absorption}
- B22F 1/06: Metallic powder characterised by the shape of the particles (nanosized particles B22F1/054)
- B22F 1/068: Flake-like particles
- B22F 9/10: using centrifugal force
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/005: {containing rare earths, i.e. Sc, Y, Lanthanides}
- C22C 38/10: containing cobalt
- H01F 1/057: and IIIa elements, e.g. Nd2Fe14B
- H01F 1/0571: {in the form of particles, e.g. rapid quenched powders or ribbon flakes}
- H01F 1/0573: {obtained by reduction or by hydrogen decrepitation or embrittlement}
- H01F 1/0577: {sintered}
- H01F 1/0578: {bonded together}
- H01F 41/0293: {diffusion of rare earth elements, e.g. Tb, Dy or Ho, into permanent magnets}
- B22F 2009/044: {by jet milling}
- B22F 2009/045: {by other means than ball or jet milling}
- B22F 2998/00: Supplementary information concerning processes or compositions relating to powder metallurgy
- B22F 2998/10: Processes characterised by the sequence of their steps
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES

## Abstract

Disclosed is a rare earth magnet in the R-T-B (rare earth element-transition metal-boron) system that is made from an improved composition and properties of main phase alloy in the R-T-B system containing Pr and a boundary alloy. Disclosed also is a manufacturing method of the rare earth magnet alloy flake by a strip casting method with improved rotating rollers such that the alloy flake has a specified fine surface roughness and has a small and regulated amount of fine R-rich phase regions. Consequently, the alloy flake for the rare earth magnet does not containing α-Fe and has a homogeneous morphology so that the rare earth magnet formed by sintering or bonding the alloy flakes exhibits excellent magnetic properties.

## Claims

### Claim 1

A main phase alloy for a rare earth magnet to be processed through a two-alloy-blending method, the main phase alloy containing R(R represents at least one rare earth element including Y) in an amount of 26 to 30% by mass and B in an amount of 0.9 to 1.1% by mass, with the balance being T (T represents transition metals including Fe as an essential element), characterized in that R has a Pr content of at least 5% by mass and the main phase alloy has a percent volume of region containing α-Fe on the basis of the entire microstructure of 5% or less.

### Claim 2 (depends on 1)

A main phase alloy for a rare earth magnet according to claim 1, wherein R has a Pr content of at least 15% by mass.

### Claim 3 (depends on 2)

A main phase alloy for a rare earth magnet according to claim 2, wherein R has a Pr content of at least 30% by mass.

### Claim 4 (depends on 1, 3)

A main phase alloy for a rare earth magnet according to claim 1 or claim 3, wherein at least one surface thereof has a surface roughness, as represented by 10-point average roughness (Rz), falling within a range of 5 μm to 50 μm.

### Claim 5 (depends on 4)

A main phase alloy for a rare earth magnet according to claim 4, wherein at least one surface thereof has a surface roughness, as represented by 10-point average roughness (Rz), falling within a range of 7 μm to 25 μm.

### Claim 6 (depends on 1, 2, 3, 4, 5)

A method for producing a main phase alloy for a rare earth magnet according to any one of claims 1 to 5, wherein the method comprises strip casting.

### Claim 7 (depends on 6)

A method for producing a main phase alloy for a rare earth magnet according to claim 6, wherein the surface roughness, as represented by 10-point average roughness (Rz), of the cast surface of a rotating roller for casting is adjusted to fall within a range of 5 μm to 100 μm.

### Claim 8 (depends on 6)

A method for producing a main phase alloy for a rare earth magnet according to claim 6, wherein the surface roughness, as represented by 10-point average roughness (Rz), of the cast surface of a rotating roller for casting is adjusted to fall within a range of 10 μm to 50 μm.

### Claim 9 (depends on 1, 2, 3)

A method for producing a main phase alloy for a rare earth magnet according to any one of claims 1 to 3, characterized by comprising a centrifugal casting method including depositing and solidifying a molten metal on an inner surface of a cylindrical mold which is rotating.

### Claim 10

A mixed powder for a rare earth sintered magnet produced by mixing a main phase alloy for a rare earth magnet according to any one of 1 to 3 with a boundary phase alloy which has an R content higher than that of the main phase alloy and has a Pr content of R lower than that of the main phase alloy.

### Claim 11 (depends on 10)

A mixed powder for a rare earth sintered magnet according to claim 10, wherein the boundary phase alloy contains substantially no Pr.

### Claim 12 (depends on 10, 11)

A rare earth sintered magnet produced through a powder metallurgical method making use of a mixed powder for a rare earth magnet according to claim 10 or claim 11.

### Claim 13

A rare earth magnet alloy flake comprising an R-T-B alloy (R represents at least one rare earth element including Y; T represents transition metals including Fe as an essential element; and B represents boron), characterized in that the flake has a thickness falling within a range of 0.1 mm to 0.5 mm, and that at least one surface of the flake has a surface roughness, as represented by 10-point average roughness (Rz), falling within a range of 5 μm to 50 μm.

### Claim 14 (depends on 13)

A rare earth magnet alloy flake (13) according to claim 13, wherein at least one surface of the alloy flake has a surface roughness, as represented by 10-point average roughness (Rz), falling within a range of 7 μm to 25 μm.

### Claim 15 (depends on 13, 14)

A rare earth magnet alloy flake according to claim 13 or claim 14, wherein the flake has a percent volume of fine R-rich phase region in alloy that constitutes the alloy flake of 20% or less.

### Claim 16

A method for producing a rare earth magnet alloy flake formed of an R-T-B alloy including a strip casting method, characterized by comprising adjusting the surface roughness, as represented by 10-point average roughness (Rz), of the cast surface of a rotating roller for casting to fall within a range of 5 μm to 100 μm.

### Claim 17

A method for producing a rare earth magnet alloy flake according to any one of 13 to 15 formed of an R-T-B alloy including a strip casting method, characterized by comprising adjusting the surface roughness, as represented by 10-point average roughness (Rz), of the cast surface of a rotating roller to fall within a range of 5 μm to 100 μm.

### Claim 18 (depends on 16, 17)

A method for producing a rare earth magnet alloy flake according to claim 16 or claim 17, wherein the surface roughness, as represented by 10-point average roughness (Rz), of the cast surface of the rotating roller for casting is adjusted to fall within a range of 10 μm to 50 μm.

### Claim 19 (depends on 13, 14, 15)

A rare earth sintered magnet alloy powder produced by subjecting, to a hydrogen decrepitation step, a rare earth magnet alloy flake according to any one of claims 13 to 15, followed by pulverization by means of jet milling.

### Claim 20 (depends on 19)

A rare earth sintered magnet produced from a rare earth magnet alloy powder according to claim 19 through a powder metallurgy method.

### Claim 21 (depends on 13, 14, 15)

A bonded magnet alloy powder produced by use of a rare earth magnet alloy flake according to any one of claims 13 to 15 through an HDDR method.

### Claim 22 (depends on 21)

A bonded magnet produced by use of a bonded magnet alloy powder according to claim 21.

### Claim 23

A rare-earth-containing alloy flake, characterized in that the alloy flake has a thickness falling within a range of 0.1 mm to 0.5 mm, at least one surface of the alloy flake has a plurality of elongated raised/dented segments (i.e., small ridge/valley areas) formed so as to cross one another, and the surface having the elongated raised/dented segments has a surface roughness, as represented by 10-point average roughness (Rz), falling within a range of 3 μm to 30 μm.

### Claim 24 (depends on 23)

A rare-earth-containing alloy flake according to claim 23, wherein the alloy flake comprises an R-T-B alloy (R represents at least one rare earth element including Y; T represents transition metals including Fe as an essential element; and B represents boron) which serves as a raw material for producing a rare earth magnet

### Claim 25 (depends on 24)

A rare-earth-containing alloy flake according to claim 24, wherein the flake has a percent volume of fine R-rich phase region in alloy that constitutes the alloy flake of 20% or less.

### Claim 26

A method for producing a rare-earth-containing alloy flake including a strip casting (SC) method, characterized by comprising employing a rotating roller for casting, the roller having, on the cast surface, a plurality of elongated raised/dented segments formed so as to cross one another and having a surface roughness of the cast surface, as represented by 10-point average roughness (Rz), falling within a range of 3 μm to 30 μm.

### Claim 27 (depends on 26)

A method for producing a rare-earth-containing alloy flake according to claim 26, wherein the alloy flake has a thickness falling within a range of 0.1 mm to 0.5 mm; at least one surface of the alloy flake has a plurality of elongated raised/dented segments formed so as to cross one another; and the surface having the elongated raised/dented segments has a surface roughness, as represented by 10-point average roughness (Rz), falling within a range of 3 μm to 30 μm.

### Claim 28 (depends on 26, 27)

A method for producing a rare-earth-containing alloy flake according to claim 26 or claim 27, wherein the rare-earth-containing alloy flake comprises an R-T-B alloy (R represents at least one rare earth element including Y; T represents transition metals including Fe as an essential element; and B represents boron) which serves as a raw material for producing a rare earth magnet.

### Claim 29 (depends on 28)

A method for producing a rare-earth-containing alloy flake according to claim 28, wherein the flake has a percent volume of fine R-rich phase region in alloy that constitutes the alloy flake of 20% or less.

### Claim 30

An alloy powder for a rare earth sintered magnet produced by subjecting, to a hydrogen decrepitation step, a rare-earth-containing alloy flake as recited in (24) or (25), followed by pulverization by means of a jet mill.

### Claim 31 (depends on 30)

A rare earth sintered magnet produced from an alloy powder for a rare earth sintered magnet according to claim 30 through a powder metallurgy method.

### Claim 32

An alloy powder for a bonded magnet produced by use of a rare-earth-containing alloy flake as recited in (24) or (25) through an HDDR method.

### Claim 33 (depends on 32)

A bonded magnet produced by use of an alloy powder for a bonded magnet according to claim 32.

### Claim 34

A method for producing a rare-earth-containing alloy flake including a strip casting method, characterized by comprising employing a rotating roller for casting, the roller having, on the cast surface, a plurality of elongated raised/dented segments and having a surface roughness provided by a plurality of elongated raised/dented segments, as represented by 10-point average roughness (Rz), falling within a range of 3 μm to 60 μm, 30% or more of raised/dented segments among entire elongated raised/dented segments extending in a direction forming an angle of 30° or more to a roller rotation direction.

### Claim 35 (depends on 34)

A method for producing a rare-earth-containing alloy flake according to claim 34, characterized by comprising employing a rotating roller for casting, 30% or more of raised/dented segments among entire elongated raised/dented segments extending in a direction forming an angle of 45° or more to a roller rotation direction.

### Claim 36 (depends on 34)

A method for producing a rare-earth-containing alloy flake according to claim 34, characterized by comprising employing a rotating roller for casting, 50% or more of raised/dented segments among entire elongated raised/dented segments extending in a direction forming an angle of 30° or more to a roller rotation direction.

### Claim 37 (depends on 34, 35, 36)

A method for producing a rare-earth-containing alloy flake according to any one of claims 34 to 36, characterized by comprising employing a rotating roller for casting, 50% or more of raised/dented segments among entire elongated raised/dented segments extending in a direction forming an angle of 45° or more to a roller rotation direction.

### Claim 38 (depends on 34, 35, 36, 37)

A method for producing a rare-earth-containing alloy flake according to any one of claims 34 to 37, wherein the rare-earth-containing alloy flake comprising an R-T-B alloy (R represents at least one rare earth element including Y; T represents transition metals including Fe as an essential element; and B represents boron) which serves as a raw material for producing a rare earth magnet in the production of the rare-earth-containing alloy flake by the strip casting method.

### Claim 39 (depends on 38)

An alloy flake for rare earth magnet produced by the method according to claim 38, which has a percent volume of fine R-rich phase region in alloy that constitutes the alloy flake of 20% or less.

### Claim 40 (depends on 38)

A powder for a rare earth sintered magnet produced by subjecting, to a hydrogen decrepitation step, an alloy flake for rare earth magnet produced by the method according to claim 38, followed by pulverization by means of a jet mill.

### Claim 41 (depends on 40)

A rare earth sintered magnet produced from an alloy powder for a rare earth sintered magnet according to claim 40 through a powder metallurgy method.

### Claim 42 (depends on 38)

An alloy powder for a bonded magnet produced by use of an alloy flake for rare earth magnet produced by the method according to claim 38 through an HDDR method.

### Claim 43 (depends on 42)

A bonded magnet produced by use of an alloy powder for a bonded magnet according to claim 42.