# US 2005/0028558 A1 · Process for producing glass molded lens

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2005/0028558 A1
- Document ID: US20050028558A1
- Status: Published application
- Kind: A1
- Application number: 10/912,569
- Filed: 2004-08-06
- Published: 2005-02-10
- Earliest claimed: 2003-08-06
- Assignees: Hoya Corporation
- Inventors: Kouichi Sato
- Web page: https://patentgrep.com/patent/US20050028558A1

## CPC

- C03B 11/08: for making solid articles, e.g. lenses
- C03B 40/02: by lubrication; Use of materials as release or lubricating compositions
- C03C 17/22: with other inorganic material (C03C17/34, C03C17/44 take precedence)
- C03B 2215/46: Lenses, e.g. bi-convex
- C03B 2215/49: Complex forms not covered by groups C03B2215/47 or C03B2215/48
- C03B 2215/66: Means for providing special atmospheres, e.g. reduced pressure, inert gas, reducing gas, clean room
- C03C 2217/282: Carbides, silicides
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

Provided is a process for producing a small-diameter glass molded lens that is made of a high-refractivity optical glass and having a small central thickness and a biconvex form, without causing cracking or breaking of the lens, and the process includes the steps of introducing a glass material made of an optical glass having a refractive index nd of 1.70 or more and provided with a mold release functional film on a surface into a mold and press-molding the glass material to obtain the glass molded lens, the glass material having a surface free energy of 55 mJ/m2 or less when it is press-molded.

## Claims

### Claim 1

A process for producing a glass molded lens, which comprises the steps of introducing a glass material made of an optical glass having a refractive index nd of 1.70 or more and provided with a mold release functional film on a surface into a mold and press-molding the glass material to obtain the glass molded lens, the glass material having a surface free energy of 55 mJ/m2 or less when it is press-molded.

### Claim 2 (depends on 1)

The process of claim 1, wherein the glass material is pre-heated in a non-oxidizing atmosphere up to a temperature corresponding to a viscosity of 106.5 to 108.5 poise as a glass viscosity before the glass material is introduced into the mold.

### Claim 3 (depends on 2)

The process of claim 2, wherein the press-molding is carried out in a non-oxidizing atmosphere in the mold that is heated up to a temperature corresponding to a viscosity of 107.5 to 1010.0 poise as a glass viscosity.

### Claim 4 (depends on 1)

The process of claim 1, wherein the optical glass contains at least one member selected from TiO2, Nb2O5 or WO3 and has a TiO2, Nb2O5 and WO3 total content of 20 to 45 mol %.

### Claim 5 (depends on 1)

The process of claims 1, wherein the optical glass is a phosphate glass.

### Claim 6 (depends on 1)

The process of claim 1, wherein the optical glass contains at least one member selected from La2O3 or Gd2O3 and has a La2O3 and Gd2O3 total content of 12 to 24 mol %.

### Claim 7 (depends on 1)

The process of claim 1, wherein the glass molded lens has a biconvex form having a central thickness of 1.2 to 1.8 mm and has a diameter of 5 to 20 mm after produced by press-molding.

### Claim 8 (depends on 1)

The process of claim 1, wherein the glass molded lens has an annular flat portion in a circumference thereof.

### Claim 9 (depends on 1)

The process of claim 1, wherein the glass molded lens has a rim thickness of 0.1 to 0.7 mm.