# US 2005/0025691 A1 · Method for heat treatment of silicon wafers and silicon wafer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2005/0025691 A1
- Document ID: US20050025691A1
- Status: Published application
- Kind: A1
- Application number: 10/929,480
- Filed: 2004-08-31
- Published: 2005-02-03
- Earliest claimed: 1998-12-28
- Assignees: Shin-Etsu Handotai Co., Ltd.
- Inventors: Norihiro Kobayashi; Shoji Akiyama; Yuuichi Matsumoto; Masaro Tamatsuka
- Web page: https://patentgrep.com/patent/US20050025691A1

## CPC

- H10P 36/20: Intrinsic gettering, i.e. thermally inducing defects by using oxygen present in the silicon body
- Y10S 438/913: Diverse treatments performed in unitary chamber
- Y10S 438/935: Gas flow control
- Y10S 438/955: Melt-back
- Y10S 438/974: Substrate surface preparation
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

According to the present invention, there are provided a method for heat treatment of silicon wafers wherein a silicon wafer is subjected to a heat treatment at a temperature of from 1000° C. to the melting point of silicon in an inert gas atmosphere, and temperature decreasing in the heat treatment is performed in an atmosphere containing 1-60% by volume of hydrogen, a method for heat treatment of silicon wafers under a reducing atmosphere containing hydrogen by using a rapid heating and rapid cooling apparatus, wherein temperature decreasing rate from the maximum temperature in the heat treatment to 700° C. is controlled to be 20° C./sec or less, and a silicon wafer which has a crystal defect density of 1.0×104 defects/cm3 or more in a wafer bulk portion, a crystal defect density of 1.0×104 defects/cm3 or less in a wafer surface layer of a depth of 0.5 μm from the surface, a crystal defect density of 0.15 defects/cm2 or less on a wafer surface and surface roughness of 1.0 nm or less in terms of the P-V value. By these, crystal defects in wafer surface layers can be reduced by a simple method with a small amount of hydrogen used without degrading microroughness of wafers.

## Claims

### Claim 1

A silicon wafer which has a crystal defect density of 1.0×104 defects/cm3 or more in a wafer bulk portion, a crystal defect density of 1.0×104 defects/cm3 or less in a wafer surface layer of a depth of 0.5 μm from the surface, a crystal defect density of 0.15 defects/cm2 or less on a wafer surface and surface roughness of 1.0 nm or less in terms of the P-V value.

### Claim 2

A silicon wafer subjected to a heat treatment, the heat treatment comprising:
subjecting a silicon wafer to a heat treatment at a temperature of from 1000° C. to the melting point of silicon in an argon atmosphere;
increasing the mixing ratio of hydrogen in the atmosphere to control the hydrogen concentration to be 1-60% by volume; and
decreasing the heat treatment temperature in the atmosphere.

### Claim 3 (depends on 2)

The silicon wafer according to claim 2, which has a crystal defect density of 1.0×104 defects/cm3 or more in a wafer bulk portion, a crystal defect density of 1.0×104 defects/cm3 or less in a wafer surface layer of a depth of 0.5 μm from the surface, a crystal defect density of 0.15 defects/cm2 or less on a wafer surface and surface roughness of 1.0 nm or less in terms of the P-V value.