# US 2005/0008794 A1 · Ink-jet recording media having a microporous coating comprising cationic fumed silica and cationic polyurethane and methods for producing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2005/0008794 A1
- Document ID: US20050008794A1
- Status: Published application
- Kind: A1
- Application number: 10/616,580
- Filed: 2003-07-10
- Published: 2005-01-13
- Earliest claimed: 2003-07-10
- Assignees: Arkwright Incorporated
- Inventors: Tom Graczyk; Shailesh Mody
- Web page: https://patentgrep.com/patent/US20050008794A1

## CPC

- B41M 5/5281: {Polyurethanes or polyureas}
- B41M 5/502: {characterised by structural details, e.g. multilayer materials (supports, backcoats or intermediate layers for thermal dye transfer donor and receiver sheets B41M5/41, B41M5/42)}
- B41M 5/52: Macromolecular coatings
- B41M 5/5218: {characterised by inorganic additives, e.g. pigments, clays}
- B41M: PRINTING, DUPLICATING, MARKING, OR COPYING PROCESSES; COLOUR PRINTING, (correction of typographical errors B41J; processes for applying transfer pictures or the like B44C1/16; fluid media for correction of typographical errors by coating C09D10/00; printing textiles D06P)

## Abstract

Inkjet recording media for producing high quality images using color printers are provided. The media comprise a substrate material, such as a paper, coated with an ink-receptive composition comprising an aqueous dispersion of cationic fumed silica particles and cationic polyurethane resin. The dispersion comprises at least 60% by weight of cationic fumed silica particles, and at least 14% by weight of cationic polyurethane resin based on solids. The coated ink-receptive layer is free of surface defects and has good ink-absorption properties. The invention also includes ink-jet recording media comprising a substrate coated with an ink-receptive underlayer and an ink-receptive top layer. The resulting media may have a semi-glossy surface finish. The surface gloss may be enhanced further by calendering the coated layer.

## Claims

### Claim 1

An aqueous coating composition for making an ink-jet recording medium, comprising a dispersion of: a) at least 60% by weight of cationic fumed silica particles, and b) at least 14% by weight of cationic polyurethane resin based on total weight of solids in the composition.

### Claim 2 (depends on 1)

The coating composition of claim 1, comprising: a) about 60% to about 86% by weight of cationic fumed silica particles, and b) about 14% to about 40% by weight of cationic polyurethane resin.

### Claim 3 (depends on 1)

The coating composition of claim 1, further comprising a water-soluble polymer selected from the group consisting of cationic acrylic polymers and copolymers, acrylic/acrylamide copolymers, polyvinyl alcohol/N-vinylformamide copolymers, and acrylamide polymers.

### Claim 4 (depends on 1)

The coating composition of claim 1, further comprising a water-dispersible polymer selected from the group consisting of cationic acrylic polymers and copolymers, cationic styrene/acrylic copolymers, and cationic polystyrene latexes

### Claim 5 (depends on 1)

The coating composition of claim 1, further comprising an additive selected from the group consisting of pigments, surface active agents, anti-static agents, optical brighteners, UV light stabilizers, UV absorbers, defoaming agents, humectants, waxes, and plasticizers.

### Claim 6 (depends on 1)

The coating composition of claim 1, wherein the silica particles are primary particles having an average particle size in the range of about 3 nm to about 40 nm.

### Claim 7 (depends on 1)

The coating composition of claim 1, wherein the silica particles comprise about 99.5% by weight silica and about 0.005% to about 0.5% by weight alumina.

### Claim 8 (depends on 1)

The coating composition of claim 1, wherein the composition has a pH in the range of about 3.0 to about 7.0.

### Claim 9 (depends on 1)

The coating composition of claim 1, wherein the composition has a zeta potential of at least 20 mV.

### Claim 10

An ink-jet recording medium, comprising a substrate coated with an ink-receptive layer comprising: a) at least 60% by weight of cationic fumed silica particles, and b) at least 14% by weight of cationic polyurethane resin based on total dry weight of the ink-receptive layer.

### Claim 11 (depends on 10)

The ink-jet recording medium of claim 10, wherein the substrate is a paper.

### Claim 12 (depends on 11)

The ink-jet recording medium of claim 11, wherein the substrate is a porous paper having water absorption as measured per a Cobb TAPPI Test Method T441 in one minute in the range of about 20 to about 100.

### Claim 13 (depends on 11)

The ink-jet recording medium of claim 11, wherein the paper is a matte paper having a gloss in the range of about 2 to about 10.

### Claim 14 (depends on 11)

The ink-jet recording medium of claim 11, wherein the paper has a base weight in the range of about 70 to about 260 g/m2.

### Claim 15 (depends on 10)

The ink-jet recording medium of claim 10, wherein the weight of the weight of the ink-receptive layer is in the range of about 5 to about 40 g/m2.

### Claim 16

An ink-jet recording medium, comprising a substrate coated with a) an ink-receptive underlayer comprising a pigment and a polymer selected from the group consisting of a water-soluble and water dispersible polymer and b) an ink-receptive top layer comprising: a) at least 60% by weight of cationic fumed silica particles, and b) at least 14% by weight of cationic polyurethane resin based on total dry weight of the top layer.

### Claim 17 (depends on 16)

The ink-jet recording medium of claim 16, wherein the ink-receptive underlayer comprises pigment and a water-soluble polymer selected from the group consisting of poly(vinyl alcohol), poly(vinyl pyrrolidone); poly(2-ethyl-2-oxazoline), modified starch cellulose; and cellulose derivatives, and mixtures thereof.

### Claim 18 (depends on 16)

The ink-jet recording medium of claim 16, wherein the ink-receptive underlayer comprises polyvinyl alcohol and silica.

### Claim 19 (depends on 16)

The ink-jet recording medium of claim 16, wherein the ink-receptive underlayer comprises pigment and a water-dispersible polymer selected from the group consisting of acrylates; methacrylates; polyvinyl acetate; vinyl acetate copolymers, polystyrene; styrene copolymers; polyesters; vinyl-acrylic terpolymers, polyacrylonitrile; acrylonitrile copolymers, polyurethanes; and
mixtures thereof.

### Claim 20 (depends on 16)

The ink-jet recording medium of claim 16, wherein the substrate is a paper.

### Claim 21 (depends on 16)

The ink-jet recording medium of claim 16, wherein the weight of the ink-receptive underlayer is in the range of about 5 to about 20 g/m2 and the weight of the ink-receptive top layer is in the range of about 5 to about 40 g/m2.

### Claim 22 (depends on 16)

The ink-jet recording medium of claim 16, wherein the paper is a substantially impermeable paper having a polymeric moisture barrier coating.

### Claim 23 (depends on 16)

The ink-jet recording medium of claim 16, wherein the substrate is a polymeric film comprising a polymer selected from the group consisting of polyesters, polycarbonates, polyethylene, polypropylene, polyvinyl chloride, polystyrene, polyacrylics, polyacetals, ionomers, and mixtures thereof.

### Claim 24 (depends on 16)

The ink-jet recording medium of claim 16, wherein the substrate is a metal foil.

### Claim 25 (depends on 16)

The ink-jet recording medium of claim 16, wherein the substrate is a metal-coated material.

### Claim 26

A method of making an ink-jet recording medium, comprising the steps of a) coating a substrate with an ink-receptive underlayer comprising a pigment and polymer selected from the group consisting of water-soluble and water-dispersible polymers, and drying the underlayer; and
b) coating an ink-receptive top layer over the underlayer, said top layer comprising an aqueous dispersion of: a) at least 60% by weight of cationic fumed silica particles and b) at least 14% by weight of cationic polyurethane resin based on total weight of solids in the dispersion, and drying the top layer.

### Claim 27 (depends on 25)

The method of claim 25, wherein the ink-receptive layers are applied using a Meyer-rod, slot-die, roller, blade, wire bar, dip, solution extrusion, reverse roll, air-knife, curtain slide, doctor-knife, and gravure method.

### Claim 28 (depends on 25)

The method of claim 25, wherein the ink-receptive top layer is not calendered, said top layer having a surface gloss of 10 or greater.

### Claim 29 (depends on 25)

The method of claim 25, wherein the ink-receptive top layer is calendered, said top layer having a surface gloss of 20 or greater.