# US 2004/0247794 A1 · Coating method and coater

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0247794 A1
- Document ID: US20040247794A1
- Status: Published application
- Kind: A1
- Application number: 10/858,369
- Filed: 2004-06-02
- Published: 2004-12-09
- Earliest claimed: 2003-06-03
- Assignees: Fuji Photo Film Co., Ltd.
- Inventors: Yasuhiko Tokimasa; Akio Tsuji
- Web page: https://patentgrep.com/patent/US20040247794A1

## CPC

- G03C 1/74: Applying photosensitive compositions to the base; Drying processes therefor (G03C1/496 takes precedence)
- B05C 5/0254: {Coating heads with slot-shaped outlet (B05C5/0283 takes precedence)}
- G11B 5/848: Coating a support with a magnetic layer by extrusion
- B05C 9/06: for applying two different liquids or other fluent materials, or the same liquid or other fluent material twice, to the same side of the work
- G03C 2001/7459: {Extrusion coating}
- G03C: PHOTOSENSITIVE MATERIALS FOR PHOTOGRAPHIC PURPOSES (for photomechanical purposes G03F); PHOTOGRAPHIC PROCESSES, e.g. CINE, X-RAY, COLOUR, STEREO-PHOTOGRAPHIC PROCESSES; AUXILIARY PROCESSES IN PHOTOGRAPHY (photographic processes characterised by the use or manipulation of apparatus classifiable per se in subclass G03B, see G03B; photomechanical production of textured or patterned surfaces G03F; electrophotography, magnetography G03G)
- B05C: APPARATUS FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (spraying apparatus, atomising apparatus, nozzles B05B; plant for applying liquids or other fluent materials to objects by electrostatic spraying B05B5/08)
- G11B: INFORMATION STORAGE BASED ON RELATIVE MOVEMENT BETWEEN RECORD CARRIER AND TRANSDUCER (recording measured values in a way that does not require playback through a transducer G01D9/00; recording or playback apparatus using mechanically marked tape, e.g. punched paper tape, or using unit records, e.g. punched or magnetically marked cards G06K; transferring data from one type of record carrier to another G06K1/18; circuits for coupling output of reproducer to radio receiver H04B1/20; gramophone pick-ups or like acoustic electromechanical transducers or circuits therefor H04R)

## Abstract

A coater to coat web includes an extrusion die, which has a die slot, for ejecting coating solution. A valve is disposed downstream from first and second conduits, for selectively feeding coating solution and bubble removing liquid to the extrusion die. A shifting mechanism moves the extrusion die between an offset position and a coating position. A controller causes the shifting mechanism to set the extrusion die in the offset position, feeds the bubble removing liquid to the extrusion die by setting the valve at the first conduit, feeds the coating solution by setting the valve at the second conduit, and causes the shifting mechanism to move the extrusion die to the coating position, to eject the coating solution from the extrusion die in the coating position. A bead of the coating solution is formed, for applying the coated layer to the web.

## Claims

### Claim 1

A coating method of coating web with liquid in a form of a bead, in which a die is used and includes a manifold and a die slot of which one end is connected with said manifold, and another end constitutes an orifice, said liquid is fed to said manifold and ejected from said orifice, to form said bead between said orifice and said web in a coating position where said orifice is positioned close to said web being transported, and a decompression chamber is used for reducing pressure of a portion of said web disposed upstream from said bead as viewed in a transporting direction, said coating method comprising:
a first liquid feeding step of feeding said liquid to said manifold while said die is in an offset position offset from said web, and while said die is kept to direct said orifice upwards and to direct said die slot to extend crosswise to a horizontal plane, wherein said liquid is fed to said orifice readily for ejection;
a second liquid feeding step of, after said first liquid feeding step, further feeding said liquid commonly used in said first liquid feeding step to said manifold, and ejecting said liquid from said orifice;
a third liquid-feeding/die-moving step of, after said second liquid feeding step, feeding said liquid to said manifold, ejecting said liquid from said orifice, and simultaneously moving said die from said offset position to said coating position;
wherein said web starts being coated after said third step.

### Claim 2 (depends on 1)

A coating method as defined in claim 1, wherein in said second liquid feeding step, said liquid is fed for 5 minutes or more.

### Claim 3 (depends on 1)

A coating method as defined in claim 1, wherein said die slot includes a small-size portion, having a minimum slot thickness equal to or more than 50 microns and equal to or less than 200 microns, and having a length equal to or more than 25 mm in a flowing direction of said liquid;
said die in said offset position is kept at such an angle that a condition of:
15°<θ1<90°
is satisfied, and is moved from said offset position to said coating position while kept at said angle, where θ1 is a slot angle of said small-size portion having said minimum slot thickness with reference to said horizontal plane.

### Claim 4 (depends on 1)

A coating method as defined in claim 1, wherein in said first liquid feeding step, said liquid is fed to said manifold at such a flow rate that an average of a linear flow rate of said liquid in a small-size portion of said die slot having a minimum slot thickness is equal to or smaller than 3 cm/sec.

### Claim 5 (depends on 1)

A coating method as defined in claim 1, wherein a dissolved air amount of said liquid fed in said first and second liquid feeding steps is 70% or less relative to solubility of saturation.

### Claim 6 (depends on 1)

A coating method as defined in claim 1, wherein said liquid comprises first and second liquids, said first liquid is adapted to removal of a residual bubble or foam in said die, said second liquid is used for coating;
in said first and second liquid feeding steps, said first liquid is fed;
feeding to said manifold is changed over from said first liquid to said second liquid between said second liquid feeding step and said third liquid-feeding/die-moving step.

### Claim 7 (depends on 1)

A coating method as defined in claim 1, wherein said die is moved at a speed equal to or less than 3 cm/sec from said offset position to said coating position.

### Claim 8 (depends on 1)

A coating method as defined in claim 1, wherein a backup roller is used and contacts said web in said coating position to be transported.

### Claim 9 (depends on 1)

A coating method as defined in claim 1, wherein part of said liquid dropped from said orifice is withdrawn by a withdrawing path disposed under said die.

### Claim 10 (depends on 9)

A coating method as defined in claim 9, wherein said decompression chamber includes one portion for constituting said withdrawing path.

### Claim 11 (depends on 1)

A coating method as defined in claim 1, wherein said die in said coating position is kept at such an angle satisfying a condition of:
90°≦θ3≦150°
where θ3 is an angle defined between said web after coating and an extension of said orifice of said slot.

### Claim 12 (depends on 1)

A coating method as defined in claim 1, wherein said die in said coating position is distant from said web at a small clearance, and a minimum of said small clearance is equal to or more than 30 microns and equal to or less than 100 microns.

### Claim 13 (depends on 12)

A coating method as defined in claim 12, wherein said die includes plural die blocks arranged in said transporting direction, and said minimum of said small clearance is defined by a lip of one of said die blocks positioned downstream in said transporting direction.

### Claim 14 (depends on 1)

A coating method as defined in claim 1, wherein a coating of said liquid on said web has a wet film thickness equal to or less than 10 microns.

### Claim 15

A coater for coating web with liquid in a form of a bead, having a die including a manifold and a die slot of which one end is connected with said manifold, and another end constitutes an orifice, wherein said liquid is fed to said manifold and ejected from said orifice, to form said bead between said orifice and said web in a coating position where said orifice is positioned close to said web being transported, and having a decompression chamber for reducing pressure of a portion of said web disposed upstream from said bead as viewed in a transporting direction, said coater comprising:
a die holder for holding said die, to direct said orifice upwards and to direct said die slot to extend crosswise to a horizontal plane;
a moving mechanism for moving said die holder between an offset position where said die is offset from said web, and said coating position where said die is close to said web for forming said bead;
a controller for operating in a first liquid feeding step of feeding said liquid to said manifold while said shifting mechanism is in said offset position, wherein said liquid is fed to said orifice readily for ejection, and then for operating in a second liquid feeding step of ejecting said liquid from said orifice for 5 minutes or more while said shifting mechanism is in said offset position, and then for ejecting said liquid from said orifice, and simultaneously moving said shifting mechanism from said offset position to said coating position, to coat said web with said liquid.

### Claim 16 (depends on 15)

A coater as defined in claim 15, wherein said die slot includes a small-size portion, having a minimum slot thickness equal to or more than 50 microns and equal to or less than 200 microns, and having a length equal to or more than 25 mm in a flowing direction of said liquid;
said die holder keeps said die in said offset position at such an angle satisfying a condition of:
15°≦θ1≦90°
and moves said die from said offset position to said coating position while kept at said angle, where θ1 is a slot angle of said small-size portion having said minimum slot thickness with reference to said horizontal plane.

### Claim 17 (depends on 15)

A coater as defined in claim 15, wherein in said first liquid feeding step, said liquid is fed to said manifold at such a flow rate that an average of a linear flow rate of said liquid in a small-size portion of said die slot having a minimum slot thickness is equal to or smaller than 3 cm/sec.

### Claim 18 (depends on 15)

A coater as defined in claim 15, further comprising a membrane degassing device for reducing a dissolved air amount of said liquid fed in said first and second liquid feeding steps to 70% or less relative to solubility of saturation.