# US 2004/0235386 A1 · Methods to improve insulator performance for cathode-ray tube (CRT) applications

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0235386 A1
- Document ID: US20040235386A1
- Status: Published application
- Kind: A1
- Application number: 10/873,335
- Filed: 2004-06-22
- Published: 2004-11-25
- Earliest claimed: 2000-12-20
- Assignees: Thomson Licensing
- Inventors: Attiganal Narayanaswamy Sreeram; Leszek Hozer
- Web page: https://patentgrep.com/patent/US20040235386A1

## CPC

- H01J 29/81: using shadow masks
- H01J 2229/0777: Coatings
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)

## Abstract

A color cathode-ray tube (CRT) having an evacuated envelope with an electron gun therein for generating at least one electron beam is provided. The envelope further includes a faceplate panel having a luminescent screen with phosphor elements on an interior surface thereof. A focus mask, having a plurality of spaced-apart first conductive strands, is located adjacent to an effective picture area of the screen. The spacing between the first conductive strands defines a plurality of apertures substantially parallel to the phosphor elements on the screen. Each of the first conductive strands has a substantially continuous insulating material layer formed on a screen facing side thereof. A plurality of second conductive wires are oriented substantially perpendicular to the plurality of first conductive strands and are bonded thereto by the insulating material layer. The insulating material layer comprises a low porosity lead-zinc-borosilicate glass.

## Claims

### Claim 1

A method of manufacturing a cathode-ray tube comprising an evacuated envelope having therein an electron gun for generating an electron beam, a faceplate panel having a luminescent screen with phosphor elements on an interior surface thereof, and a focus mask, wherein the focus mask includes a plurality of spaced-apart first conductive strands, and a plurality of spaced-apart second conductive wires oriented substantially perpendicular to the plurality of spaced-apart first conductive strands, comprising the steps of:
applying an insulating material to the plurality of spaced-apart first conductive strands, wherein the insulating material comprises a low porosity lead-zinc-borosilicate glass formed from a lead-zinc-borosilicate glass powder having a median particle size less than about 1 μm; and
bonding the plurality of spaced-apart second conductive wires to the insulating material.

### Claim 2 (depends on 1)

The method of claim 1 wherein the low porosity lead-zinc-borosilicate glass includes one or more transition metal oxides.

### Claim 3 (depends on 2)

The method of claim 2 wherein the one or more transition metal oxides are selected from the group consisting of iron oxide (Fe2O3 and Fe3O4), titanium oxide (TiO2), zinc oxide (ZnO), molybdenum oxide (MoO3), chromium oxide (Cr2O3), tin oxide (SnO2), nickel oxide (NiO), and combinations thereof.

### Claim 4 (depends on 2)

The method of claim 2 wherein the one or more transition metal oxides in the low porosity lead-zinc-borosilicate glass have a weight % in a range of about 2% by weight to about 12% by weight.

### Claim 5 (depends on 1)

The method of claim 1 wherein the low porosity lead-zinc-borosilicate glass is SCC-11, or a mixture of lead, zinc, boron and silicon oxides melted together to form an SCC-11-like glass.

### Claim 6 (depends on 2)

The method of claim 2 wherein the one or more transition metal oxides are added to the low porosity lead-zinc-borosilicate glass either by premelting or by mixing with the lead-zinc-borosilicate powder.