# US 2004/0209995 A1 · Process for the preparation of latices using block copolymers as surfactants

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0209995 A1
- Document ID: US20040209995A1
- Status: Published application
- Kind: A1
- Application number: 10/844,275
- Filed: 2004-05-12
- Published: 2004-10-21
- Earliest claimed: 2001-05-04
- Inventors: Herve Adam; Wan-Li Liu
- Web page: https://patentgrep.com/patent/US20040209995A1

## CPC

- C08F 2/24: with the aid of emulsifying agents
- C08F 2/38: Polymerisation using regulators, e.g. chain terminating agents {, e.g. telomerisation}
- C08F 8/00: Chemical modification by after-treatment (graft polymers, block polymers, crosslinking with unsaturated monomers or with polymers C08F251/00 - C08F299/00; of conjugated diene rubbers C08C)
- C08F 287/00: Macromolecular compounds obtained by polymerising monomers on to block polymers
- C08F 2800/20: as weight or mass percentages
- C08F 2810/40: taking place solely at one end or both ends of the polymer backbone, i.e. not in the side or lateral chains
- Y10S 526/922: Polymerization process of ethylenic monomers using manipulative technique
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

A subject-matter of the present invention is a process for the preparation of a latex by radical aqueous emulsion polymerization in the presence of at least one ethylenically unsaturated monomer, of at least one radical polymerization initiator and of at least one surface-active block copolymer comprising at least one hydrophilic block and at least one hydrophobic block which is prepared by a “living” or “controlled” preparation process, the said copolymer exhibiting a number-average molecular mass of between 2 000 and 20 000, preferably between 4 000 and 16 000, a glass transition temperature of the hydrophobic block of less than 30° C., preferably of less than 25° C., and greater than −100° C., and a surface tension of less than 60 millinewtons per metre (mN/m), preferably of less than 50 mN/m, measured at a concentration in demineralized water of less than or equal to 10−4 mol/l at 20° C. and under one atmosphere, and the transfer agent having been rendered inert with respect to the said radical polymerization. The latices obtained can be used in particular in paints, adhesives and building materials.

## Claims

### Claim at position 1

1-20. (Canceled)

### Claim 21

A process for the preparation of a latex comprising the steps of:
a) radical aqueous emulsion polymerization of a reaction mixture, to obtain a latex, said reaction mixture comprising at least one ethylenically unsaturated monomer, at least one radical polymerization initiator and at least an effective amount of a surface-active block copolymer comprising at least one hydrophilic block and at least one hydrophobic block which is prepared by a “living” preparation process using a transfer agent being a dithiocarbonate selected from the group consisting of the compounds of following formulae (IA), (IB) and (IC):
3
wherein:
R2 and R2′ represent
(i) an alkyl, acyl, aryl, alkene or alkyne group,
(ii) an optionally aromatic, saturated or unsaturated carbonaceous ring, or
(iii) a saturated or unsaturated heterocycle,
groups and rings (i), (ii) and (iii) being optionally substituted,
R1 and R1′ represent
(i) an optionally substituted alkyl, acyl, aryl, alkene or alkyne group,
(ii) a carbonaceous ring which is saturated or unsaturated and which is optionally substituted or aromatic, or
(iii) an optionally substituted, saturated or unsaturated heterocycle or a polymer chain, and
p is between 2 and 10; and
said copolymer exhibiting:
a number-average molecular mass of between 2 000 and 20 000 g/mol,
a glass transition temperature of the hydrophobic block of less than 30° C., and greater than −100° C., and
a surface tension of less than 60 millinewtons per metre (mN/m), measured at a concentration in demineralized water of less than or equal to 10−4 mol/l at 20° C. and under one atmosphere,
the transfer agent having been rendered inert with respect to the said radical polymerization, and
b) recovery of the latex thus obtained.

### Claim 22 (depends on 1)

The process according to claim 1, wherein the copolymer exhibits:
a number-average molecular mass of between 4 000 and 16 000 g/mol,
a glass transition temperature of the hydrophobic block of less than 25° C., and
a surface tension of less than 50 millinewtons per metre.

### Claim 23 (depends on 21)

The process according to claim 21, wherein the block copolymer is prepared by a process comprising the following steps:
aa) as a first implementation, bringing into contact to obtain a polymer:
at least one ethylenically unsaturated monomer,
at least one source of free radicals, and
at least one transfer agent of formulae (IA), (IB) or (IC):
bb) repeating, at least once, the above operation of bringing into contact using:
different monomers from the preceding implementation, and
instead of the precursor compound of formula (I), the polymer resulting from the preceding implementation, and
cc) rendering the transfer agent inert at the end of the polymerization.

### Claim 24 (depends on 23)

The process according to claim 23, wherein step cc) comprises masking of active chemical functional groups of the transfer agent by means of a masking agent or destruction of the transfer agent by a hydrolysis or oxidation reaction by metal catalysis or by use of primary radicals.

### Claim 25 (depends on 23)

The process according to claim 23, wherein the hydrophilic block derives from hydrophilic monomers selected from the group consisting of:
unsaturated ethylenic mono- and dicarboxylic acids,
monoalkyl esters of the dicarboxylic acids of the type mentioned with alkanols preferably having 1 to 4 carbon atoms and their N-substituted derivatives,
amides of unsaturated carboxylic acids, and
ethylenic monomers comprising a sulphonic acid group and its alkali metal or ammonium salts.

### Claim 26 (depends on 25)

The process according to claim 25, wherein the hydrophilic block derives from hydrophilic monomers selected from the group consisting of acrylic acid, methacrylic acid, itaconic acid, maleic acid, fumaric acid, 2-hydroxyethyl acrylate or methacrylate, acrylamide, methacrylamide, vinylsulphonic acid, vinylbenzenesulphonic acid, alpha-acrylamidomethylpropanesulphonic acid, 2-sulphoethyl methacrylate, 2-acrylamido-2-methylpropanesulphonic acid and styrenesulphonate.

### Claim 27 (depends on 23)

The process according to claim 23, wherein the hydrophobic block derives hydrophobic monomers selected from the group consisting of:
esters of acrylic acid and of methacrylic acid with hydrogenated or fluorinated C1-C12 alcohols,
vinyl nitriles having from 3 to 12 carbon atoms,
carboxylic acid vinyl esters,
vinyl halides,
vinylamine amides, and
unsaturated ethylenic monomers comprising a secondary, tertiary or quaternary amino group, or a heterocyclic group comprising nitrogen.

### Claim 28 (depends on 27)

The process according to claim 27, wherein the hydrophobic block derives hydrophobic monomers selected from the group consisting of methyl acrylate, ethyl acrylate, propyl acrylate, n-butyl acrylate, isobutyl acrylate, 2-ethylhexyl acrylate, t-butyl acrylate, methyl methacrylate, ethyl methacrylate, n-butyl methacrylate, isobutyl methacrylate, acrylonitrile, methacrylonitrile, vinyl acetate, vinyl versatate, vinyl propionate, vinylformamide, vinylacetamide, vinylpyridines, vinylimidazole, dimethylaminoethyl acrylate or methacrylate, di-tert-butylaminoethyl acrylate or methacrylate, and dimethylaminomethylacrylamide or -methacrylamide.

### Claim 29 (depends on 28)

The process according to claim 28, wherein the polymerization of the copolymer is carried out in tetrahydrofuran or in a linear, cyclic or branched C1-C8 aliphatic alcohol.

### Claim 30 (depends on 29)

The process according to claim 29, wherein the alcohol is methanol, ethanol, cyclohexanol or ethylene glycol, and wherein the hydrophilic monomer is acrylic acid (AA), acrylamide (AM), 2-acrylamido-2-methylpropanesulphonic acid (AMPS) or styrenesulphonate (SS).

### Claim 31 (depends on 21)

The process according to claim 21, wherein said process comprises the following steps:
aaa) a stable aqueous preemulsion comprising starting ethylenically unsaturated monomers and the surface-active block copolymer is prepared,
bbb) a reaction mixture comprising a conventional surfactant, an initiator and water is introduced into a radical polymerization reactor comprising two openings and from 1 to 10% by weight of preemulsion prepared in step aaa) is added to the said mixture,
ccc) the reaction mixture obtained at the end of stage bbb) is heated to a temperature of between 40 and 90° C., for the purpose of generating a seed formed of latex particles in dispersion in the water,
ddd) the preemulsion obtained in stage aaa) is added with an additional amount of initiator via the two separate openings of the reactor to produce the latex, and
eee) optionally, the latex obtained in stage ddd) is heated at a temperature of between 40 and 90° C.

### Claim 32 (depends on 31)

The process according to claim 31, wherein:
in step bbb) of preemulsion prepared is of between 3 and 7%,
in step ccc), the temperature is of between 60 and 80° C., and
in optional step eee), the temperature is of between 60 and 80° C.

### Claim 33 (depends on 21)

The process according to claim 21, wherein the ethylenically unsaturated monomer or monomers are selected from the group consisting of styrene, styrene derivatives, butadiene, chloroprene, (meth)acrylic esters and vinyl nitrites.

### Claim 34 (depends on 21)

The process according to claim 21, wherein 0.5 to 5% by weight of the surface-active block copolymer with respect to the total weight of water is employed during the polymerization of the latex, or of 1 to 8% by weight of the surface-active block copolymer copolymer with respect to the total weight of the monomers employed during the polymerization of the latex.

### Claim 35 (depends on 34)

The process according to claim 34, wherein 1 to 4% by weight of the surface-active block copolymer with respect to the total weight of water is employed during the polymerization of the latex, and 2 to 5% by weight of the surface-active block copolymer with respect to the total weight of the monomers employed during the polymerization of the latex.

### Claim 36 (depends on 31)

The process according to claim 31, wherein 0.5 to 5% by weight of the surface-active block copolymer with respect to the total weight of water is employed during the polymerization of the latex, or 1 to 8% by weight of the surface-active block copolymer copolymer with respect to the total weight of the monomers employed during the polymerization of the latex.

### Claim 37 (depends on 36)

The process according to claim 36, wherein 1 to 4% by weight of the surface-active block copolymer with respect to the total weight of water is employed during the polymerization of the latex, and 2 to 5% by weight of the surface-active block copolymer with respect to the total weight of the monomers employed during the polymerization of the latex.