# US 2004/0204559 A1 · Polyurethane resin with high carbonate group content

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0204559 A1
- Document ID: US20040204559A1
- Status: Published application
- Kind: A1
- Application number: 10/701,908
- Filed: 2003-11-05
- Published: 2004-10-14
- Earliest claimed: 2002-11-07
- Assignees: Bayer Aktiengesellschaft
- Inventors: Martin Melchiors; Thomas Munzmay; Torsten Pohl; Uwe Klippert
- Web page: https://patentgrep.com/patent/US20040204559A1

## CPC

- C08G 18/6659: {with compounds of group C08G18/34}
- C08G 18/0823: {containing carboxylate salt groups or groups forming them}
- C08G 18/44: Polycarbonates
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS

## Abstract

The invention relates to solvent-borne polyurethane resins with a high carbonate group content which are dilutable in water, to aqueous coating compositions prepared thereof, to a process for preparing them and to their use.

## Claims

### Claim 1

A water-dilutable polyurethane resin obtained by reacting
A1) at least one polycarbonate polyol with a number average molecular weight of from 400 to 6000 Da,
A2) optionally, a polyester polyol which is different from component (A1) with a number-average molecular weight Mn of from 400 to 6000 Da,
A3) optionally, a low molecular weight compound containing two or more hydroxy and/or amino groups having a molecular weight of from 60 to 400 Da,
A4) optionally, a compound which is monofunctional in terms of reaction with NCO groups or which contains active hydrogen atoms differing in reactivity, these units being located in each case at the chain end of a polymer containing urethane groups,
A5) at least one compound containing at least two isocyanate-reactive groups and at least one group capable of forming anions, and
A6) one or more polyisocyanates,
the resultant polyurethane resin containing from 5.8% to 20.0% by weight of incorporated carbonate groups —O(C═O)O— and being present in a solvent which is inert towards isocyanate groups.

### Claim 2 (depends on 1)

The water-dilutable polyurethane resin according to claim 1, wherein the average molecular weight (Mn is from 1000 to 30,000 Da, the acid number is from 10 to 80 mg KOH/g and the OH content is from 0.5 to 5% by weight.

### Claim 3 (depends on 1)

The water-dilutable polyurethane resin according to claim 1, wherein the solids content is at least 50% by weight, the remainder to 100% by weight being made up of one or more solvents which are inert towards isocyanate groups and customary coatings auxiliaries and additives.

### Claim 4 (depends on 1)

The water-dilutable polyurethane resin according to claim 1, wherein the polyurethane has been synthesized from
A1) from 25 to 80% by weight of at least one polycarbonate polyol having a molecular weight (Mn) of from 400 to 6000 Da and which has a carbonate group content of at least 10% by weight,
A2) from 0 to 60% by weight of at least one polyester polyol which is different from component (A1) and has a number-average molecular weight Mn of from 400 to 6000 Da,
A3) from 0 to 20% by weight of at least one low molecular weight compound which contains two or more hydroxyl and/or amino groups and has a molecular weight of from 60 to 400 Da,
A4) from 0 to 10% by weight of at least one compound which is monofunctional in terms of reaction with NCO groups or contains active hydrogen atoms differing in reactivity, these units being located in each case at the chain end of a polymer containing urethane groups,
A5) from 2 to 10% by weight of at least one compound containing at least two isocyanate-reactive groups and at least one group capable of forming anions, and
A6) from 5 to 50% by weight of one or more polyisocyanates, the sum. of the components being 100% by weight.

### Claim 5 (depends on 1)

The water-dilutable polyurethane resin according to claim 1, wherein component (A1) is linear hydroxyl polycarbonates (A1).

### Claim 6 (depends on 1)

The water-dilutable polyurethane resin according to claim 1, wherein the polyurethane resin is free from sulfonic acid groups.

### Claim 7 (depends on 1)

A process for preparing the water-dilutable polyurethanes according to claim 1, comprising preparing an OH- and/or NH-functional polyurethane from components (A1), (A5) and (A6) and optionally, components (A2) to (A4) in a solvent which is inert towards isocyanate groups.

### Claim 8 (depends on 1)

An aqueous coating system comprising
a) at least one non-aqueous component comprising the water-dispersible polyurethane resin according to claim 1,
b) one or more aqueous binder components comprising at least one hydroxyl-free polyurethane dispersion,
c) optionally, auxiliaries and additives and
d) at least one crosslinker component.

### Claim 9 (depends on 8)

The aqueous coating system according to claim 8, wherein the crosslinker component is hydrophobic or hydrophilicized polyisocyanates containing free isocyanate groups based on aliphatic, cycloaliphatic, araliphatic and/or aromatic isocyanates.

### Claim 10 (depends on 9)

The aqueous coating system according to claim 9, wherein the crosslinker component is hydrophobic or hydrophilicized polyisocyanates containing free isocyanate groups based on aliphatic or cycloaliphatic isocyanates.

### Claim 11 (depends on 8)

The process for preparing aqueous coating systems according to claim 8, further comprising incorporating the water-dilutable polyurethane resin into an aqueous phase comprising at least one hydroxyl-free aqueous polyurethane dispersion and, if desired, auxiliaries and additives and subsequently at least one crosslinker component and also, where appropriate, further auxiliaries and additives are dispersed into this aqueous stock varnish.

### Claim 12 (depends on 1)

A method of coating, varnishing and sealing a substrate comprising applying the water-dilutable resin of claim 1 to the substrate, wherein the substrate is selected from mineral construction material surfaces, wood, wood materials, metallic surfaces, asphaltic coverings, bituminous coverings, and plastics surfaces.

### Claim 13 (depends on 1)

A method of producing a soft-feel effect coating material comprising applying the water-dilutable resin of claim 1 to a substrate.

### Claim 14 (depends on 13)

The method of claim 13, wherein the substrate is plastic or wood.

### Claim 15 (depends on 1)

A substrates coated with a crosslinked coating system comprising the water-dilutable polyurethane resins according to claim 1.