- Assignees: Taisei Chemical Industries, Ltd.
- Inventors: Takashi Sunamori; Fumiyuki Kadowaki; Koichi Noguchi; Hideto Uchida; Kazuki Torinoumi
- Web page: https://patentgrep.com/patent/US20040204514A1

## CPC

- C09B 67/0096: {Purification; Precipitation; Filtration}
- C09B 67/0063: {of organic pigments with only macromolecular substances}
- C09B: ORGANIC DYES OR CLOSELY-RELATED COMPOUNDS FOR PRODUCING DYES {, e.g. PIGMENTS}; MORDANTS; LAKES (fermentation or enzyme using processes to synthesise a desired chemical compound C12P)

## Abstract

There is provided a method for producing colorants which can exhibit excellent color development even in a small amount and are low in thixotropy. The constituent feature of the present invention comprises: enhancing the molecular extinction coefficient of the coloring matter substance by ion exchanging method, to afford a room for increasing B (resin) of P/B; then a composition is designed and employed to enhance the effect increasing the polar group concentration which is a role of resin and the quality of the effect; it thus becomes possible to achieve the limit value of the molecular extinction coefficient as much as possible and to eliminate the factors adversely affecting the present process.

## Claims

### Claim 1

A method for producing a colorant comprising:
contacting a dispersion of a powdery coloring matter substance in deionized water with an anion exchange resin and/or a cation exchange resin to subject the dispersion to ion exchanging until an electrical conductivity of the dispersion reaches 25
μS/cm or lower, thereby obtaining a purified coloring matter substance;
contacting with an anion exchange resin and/or a cation exchange resin an aqueous solution or organic solvent solution of a binder resin prepared so that a carboxyl group concentration or a sum of a carboxyl group concentration and a hydroxyl group concentration is 0.001 mol/ml or higher, to obtain a purified binder resin solution;
kneading the purified coloring matter substance and the purified binder resin solution to obtain a colorant precursor; and
contacting the colorant precursor with an anion exchange resin and/or a cation exchange resin.

### Claim 2 (depends on 1)

The method according to claim 1, further comprising:
subjecting the liquid colorant precursor to an ultra-high speed centrifugal separation at 5000-15000 rpm after the contacting with the anion exchange resin and/or the cation exchange resin.

### Claim 3 (depends on 1)

A method according to claim 1, wherein the binder resin is a copolymer of at least one polymerizable monomer containing a carboxyl group and at least one polymerizable monomer containing neither carboxyl group nor hydroxyl group, a copolymer of at least one polymerizable monomer containing a carboxyl group, at least one polymerizable monomer containing a hydroxyl group and at least one polymerizable monomer containing neither carboxyl group nor hydroxyl group, or a mixture thereof.

### Claim 4 (depends on 1)

A colorant obtainable by a method according to claim 1.

### Claim 5 (depends on 1)

The purified coloring matter substance obtained in the method according to claim 1.

### Claim 6 (depends on 1)

The purified binder resin solution obtained in the method according to claim 1.

### Claim 7 (depends on 1)

The colorant precursor obtained in the method according to in claim 1.