- Assignees: Ceramtec AG Innovative Ceramic Engineering
- Inventors: Guenter Riedel; Hartmut Kruener; Matthias Steiner; Peter Stingl
- Web page: https://patentgrep.com/patent/US20040204306A1

## CPC

- C04B 35/6455: {Hot isostatic pressing}
- C04B 35/584: based on silicon nitride
- C04B 35/5935: {obtained by gas pressure sintering}
- C04B 35/597: based on silicon oxynitride, {e.g. SIALONS}
- C04B 35/62655: {Drying, e.g. freeze-drying, spray-drying, microwave or supercritical drying}
- C04B 35/6303: {Inorganic additives}
- C04B 35/632: Organic additives
- C04B 35/63416: {Polyvinylalcohols [PVA]; Polyvinylacetates}
- C04B 35/63488: {Polyethers, e.g. alkylphenol polyglycolether, polyethylene glycol [PEG], polyethylene oxide [PEO]}
- C04B 2235/3217: Aluminum oxide or oxide forming salts thereof, e.g. bauxite, alpha-alumina
- C04B 2235/3225: Yttrium oxide or oxide-forming salts thereof
- C04B 2235/3244: Zirconium oxides, zirconates, hafnium oxides, hafnates, or oxide-forming salts thereof
- C04B 2235/3463: Alumino-silicates other than clay, e.g. mullite
- C04B 2235/3873: Silicon nitrides, e.g. silicon carbonitride, silicon oxynitride
- C04B 2235/3882: Beta silicon nitrides
- C04B 2235/5409: expressed by specific surface values
- C04B 2235/604: Pressing at temperatures other than sintering temperatures
- C04B 2235/767: Hexagonal symmetry, e.g. beta-Si3N4, beta-Sialon, alpha-SiC or hexa-ferrites
- C04B 2235/77: Density
- C04B 2235/78: Grain sizes and shapes, product microstructures, e.g. acicular grains, equiaxed grains, platelet-structures
- C04B 2235/784: Monomodal
- C04B 2235/785: Submicron sized grains, i.e. from 0,1 to 1 micron
- C04B 2235/786: Micrometer sized grains, i.e. from 1 to 100 micron
- C04B 2235/788: Aspect ratio of the grains
- C04B 2235/80: Phases present in the sintered or melt-cast ceramic products other than the main phase
- C04B 2235/85: Intergranular or grain boundary phases
- C04B 2235/94: Products characterised by their shape
- C04B 2235/96: Properties of ceramic products, e.g. mechanical properties such as strength, toughness, wear resistance
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE

## Abstract

The invention relates to cast parts which contain at least 87 wt. % silicon nitride and up to 13 wt. % of an additive combination comprised of Al2O3 and Y2O3. The initial composition of the mass formulation starts with Y2O3/Al2O3 ratios of less than 1.1, preferably with Y2O3 Al2O3 ratios of 0.2 to 1.09. 1% to 20% of the Y2O3 portion can thus be substituted by an additional element group of IVb of the periodic table or by the oxide thereof. The cast parts can comprise up to 1.0 wt. % HfO2 and/or ZrO2. Said cast parts preferably have a thickness >98% of the theoretic thickness. At room temperature, the bending strength of the inventive cast parts amounts to ≧1100 MPa and amounts to ≧850 MPa at 1000° C. The inventive cast parts correspond to the formula Si6-zAlzOzN8-z. The degree of substitution z thus amounts to 0.20 to 0.60, preferably from 0.22 to 0.54, especially from 0.3 to 0.35.

## Claims

### Claim 1

Shaped body of sintered silicon nitride ceramic with high mechanical strength at room temperature and at elevated temperatures, characterised in that it corresponds to the formula Si6-zAlzOzN8-z wherein the degree of substitution z is 0.20 to 0.60, that it contains at least 87 wt. % of silicon nitride and up to 13 wt. % of an additive combination of Al2O3 and Y2O3 and the weight ratio of the additives Y2O3/Al2O3 is less than 1.1.

### Claim 2 (depends on 1)

Shaped body according to claim 1, characterised in that 1% to 20% of the Y2O3 fraction is replaced by another element of Group lVb of the periodic system or by an oxide thereof.

### Claim 3 (depends on 1)

Shaped body according to claim 1, characterised in that it contains up to 1.0 wt. % HfO2 and/or ZrO2.

### Claim 4 (depends on 1)

Shaped body according to claim 1, characterised in that the weight ratio of the additives Y2O3/Al2O3 is 0.2 to 1.09.

### Claim 5 (depends on 1)

Shaped body according to claim 1, characterised in that it has a density of >98% of the theoretical density.

### Claim 6 (depends on 1)

Shaped body according to claim 1, characterised in that the bending strength of the shaped bodies according to the invention is ≧1100 MPa at room temperature and ≧850 MPa at 1000° C.

### Claim 7 (depends on 1)

Shaped body according to claim 1, characterised in that the degree of substitution z is 0.22 to 0.54, preferably 0.3 to 0.35.

### Claim 8 (depends on 1)

Shaped body according to claim 1, characterised in that the fracture toughness K1c is >6.5 MPa·m1/2 at room temperature and >5 MPa·m1/2 at 1000° C.

### Claim 9 (depends on 1)

Process for producing a shaped body according to claim 1, characterised in that silicon nitride raw material having an initial oxygen content of 1.3% and up to 13 wt. % of an additive combination of Al2O3 and Y2O3 is mixed as sintering additive in a liquid dispersing agent, ground, plasticised and then spray dried, the resultant agglomerate is compressed into pressed pieces, and the pressed pieces are baked and then sintered at temperatures between 1600° C. and 1900° C., preferably at temperatures between 1850° C. and 1875° C.

### Claim 10 (depends on 9)

Process according to claim 9, characterised in that 1% to 20% of the Y2O3 fraction is replaced by another element of Group IVb of the periodic system or by an oxide thereof.

### Claim 11 (depends on 9)

Process according to claim 9, characterised in that the mixture additionally contains up to 1.0 wt. % HfO2 and/or ZrO2.

### Claim 12 (depends on 9)

Process according to claim 9, characterised in that the weight ratio of the additives Y2O3/Al2O3 is 0.2 to 1.09.

### Claim 13 (depends on 9)

Process according to claim 9, characterised in that the compression of the shaped pieces is carried out above 1500 bar and/or the sintering is carried out in a gas-fired press sintering furnace at a maximum nitrogen pressure of 80 bar.

### Claim 14 (depends on 1)

Use of shaped bodies according to claim 1, in machinery and plant construction as well as in combustion engine manufacture.