# US 2004/0203227 A1 · Ceric-ion slurry for use in chemical-mechanical polishing

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0203227 A1
- Document ID: US20040203227A1
- Status: Published application
- Kind: A1
- Application number: 10/837,458
- Filed: 2004-04-29
- Published: 2004-10-14
- Earliest claimed: 1999-03-29
- Inventors: Anne E. Miller; A. Daniel Feller; Kenneth C. Cadien
- Web page: https://patentgrep.com/patent/US20040203227A1

## CPC

- C09G 1/02: containing abrasives or grinding agents {(abrasives as such C09K3/14; polishing of semi-conductors H10P52/40)}
- C09K 3/1463: {Aqueous liquid suspensions}
- C23F 3/00: Brightening metals by chemical means
- H10P 52/403: {of conductive or resistive materials}
- C09G: POLISHING COMPOSITIONS (French polish C09F11/00); SKI WAXES
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- C23F: NON-MECHANICAL REMOVAL OF METALLIC MATERIAL FROM SURFACE (working metal by laser beams B23K26/00; desurfacing by applying flames B23K7/00; working of metal by electro-erosion B23H; producing decorative effects by removing surface material, e.g. by engraving, by etching, B44C1/22; electrolytic etching or polishing C25F); INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL; MULTI-STEP PROCESSES FOR SURFACE TREATMENT OF METALLIC MATERIAL INVOLVING AT LEAST ONE PROCESS PROVIDED FOR IN CLASS C23 AND AT LEAST ONE PROCESS COVERED BY SUBCLASS C21D OR C22F OR CLASS C25
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

The invention provides a chemical-mechanical polishing slurry comprising a liquid, cerium ions as an oxidizer, an abrasive, and a pH increasing substance. The cerium ions are in the liquid in a quantity equal to the inclusion of at least 0.02 molar ammonium cerium nitrate in the liquid. The abrasive is also included in the liquid. The liquid, the cerium ions and the abrasive jointly have a first pH value. The pH increasing substance increases the first pH value to a second pH value above 1.5.

## Claims

### Claim at position 1

1-20. (canceled)

### Claim 21

A method of forming a metal line, comprising:
forming a first layer, with an opening therein, over a semiconductor substrate;
depositing a metal layer which fills the opening and covers the first layer;
applying a chemical-mechanical polishing slurry onto the metal layer, the slurry comprising cerium ions as an oxidizer, and an abrasive;
contacting a polishing surface against the metal layer; and
moving the polishing surface over the metal layer.

### Claim 22 (depends on 21)

The method of claim 21 wherein the slurry comprises cerium ions in quantity sufficient to oxidize a portion of the metal layer, and the abrasive in quantity sufficient to assist in removal of the oxidized portion when the polishing surface is moved over the metal layer.

### Claim 23 (depends on 21)

The method of claim 21 wherein the metal layer is of a metal selected from the group consisting of copper and tungsten.

### Claim 24 (depends on 21)

The method of claim 21 further comprising:
depositing a barrier layer over the first layer and before depositing the metal layer, the cerium ions selectively oxidizing the material of the metal layer over the material of the barrier layer.

### Claim 25 (depends on 21)

The method of claim 21 wherein the metal layer is removed at a rate of at least 1000 angstroms per minute.