# US 2004/0202952 A1 · Toner processes

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0202952 A1
- Document ID: US20040202952A1
- Status: Published application
- Kind: A1
- Application number: 10/413,633
- Filed: 2003-04-14
- Published: 2004-10-14
- Earliest claimed: 2003-04-14
- Assignees: Xerox Corporation
- Inventors: Amy A. Albright; Peter V. Nguyen; Donald Riley; Allan K. Chen; Emily L. Moore; Tie Hwee Ng; Chieh-Min Cheng
- Web page: https://patentgrep.com/patent/US20040202952A1

## CPC

- G03G 9/0904: {Carbon black}
- C08J 3/215: at least one additive being also premixed with a liquid phase
- G03G 9/0804: {whereby the components are brought together in a liquid dispersing medium}
- G03G 9/0819: {characterised by the dimensions of the particles}
- G03G 9/0821: {characterised by physical parameters (magnetic parameters G03G9/083)}
- G03G 9/0825: {characterised by their structure; characterised by non-homogenuous distribution of components (microcapsular toners G03G9/093)}
- G03G 9/0827: {characterised by their shape, e.g. degree of sphericity}
- G03G 9/08704: {Polyalkenes}
- G03G 9/08706: {Polymers of alkenyl-aromatic compounds}
- G03G 9/08708: {Copolymers of styrene}
- G03G 9/08711: {with esters of acrylic or methacrylic acid}
- G03G 9/08724: {Polyvinylesters}
- G03G 9/08726: {Polymers of unsaturated acids or derivatives thereof}
- G03G 9/08728: {Polymers of esters}
- G03G 9/08733: {Polymers of unsaturated polycarboxylic acids}
- G03G 9/08782: {Waxes}
- G03G 9/08795: {characterised by their chemical properties, e.g. acidity, molecular weight, sensitivity to reactants}
- G03G 9/08797: {characterised by their physical properties, e.g. viscosity, solubility, melting temperature, softening temperature, glass transition temperature}
- G03G 9/0906: {Organic dyes}
- G03G: ELECTROGRAPHY; ELECTROPHOTOGRAPHY; MAGNETOGRAPHY
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)

## Abstract

A toner process comprising mixing a colorant dispersion with a latex, a wax dispersion, and a coagulant, and wherein the polymer latex selected possesses a weight average molecular weight of from about 20,000 to about 55,000, a number average molecular weight of from about 5,000 to about 18,000, an onset glass transition temperature Tg of from about 40° C. to about 80° C., and a particle size distribution PSD of from about 50 to about 500 nanometers.s

## Claims

### Claim 1

A toner process comprising mixing a colorant dispersion with a latex, a wax dispersion, and a coagulant, and wherein the polymer latex selected possesses a weight average molecular weight of from about 20,000 to about 55,000, a number average molecular weight of from about 5,000 to about 18,000, an onset glass transition temperature Tg of from about 40° C. to about 80° C., and a particle size distribution PSD of from about 50 to about 500 nanometers.

### Claim 2 (depends on 1)

A process in accordance with claim 1 wherein said weight average molecular weight is from about 25,000 to about 45,000.

### Claim 3 (depends on 1)

A process in accordance with claim 1 wherein said weight average molecular weight is from about 28,000 to about 40,000.

### Claim 4 (depends on 1)

A process in accordance with claim 1 wherein said weight average molecular weight is from about 28,000 to about 37,000.

### Claim 5 (depends on 4)

A process in accordance with claim 4 wherein said number average molecular weight is from about 5,000 to about 20,000.

### Claim 6 (depends on 1)

A process in accordance with claim 1 wherein said number average molecular weight is from about 6,000 to about 15,000.

### Claim 7 (depends on 3)

A process in accordance with claim 3 wherein said number average molecular weight is from about 8,000 to about 13,000.

### Claim 8 (depends on 4)

A process in accordance with claim 4 wherein said number average molecular weight is from about 9,000 to about 12,000.

### Claim 9 (depends on 1)

A process in accordance with claim 1 wherein said onset glass transition temperature Tg is from about 45° C. to about 70° C.

### Claim 10 (depends on 1)

A process in accordance with claim 1 wherein said onset glass transition temperature Tg is from about 48 to about 60° C.

### Claim 11 (depends on 1)

A process in accordance with claim 1 wherein said particle size distribution PSD is from about 70 to about 400 nanometers.

### Claim 12 (depends on 1)

A process in accordance with claim 1 wherein said particle size distribution PSD is from about 100 to about 350 nanometers.

### Claim 13 (depends on 1)

A process in accordance with claim 1 wherein said particle size distribution PSD is from about 150 to about 300 nanometers.

### Claim 14 (depends on 4)

A process in accordance with claim 4 wherein said particle size distribution PSD is from about 180 to about 300 nanometers.

### Claim 15 (depends on 7)

A process in accordance with claim 7 wherein said particle size distribution PSD is from about 190 to about 260 nanometers.

### Claim 16 (depends on 1)

A process in accordance with claim 1 wherein said polymer latex selected possesses a weight average molecular weight of about 33,000, a number average molecular weight of about 11,000, an onset glass transition temperature Tg of about 51° C., and a particle size distribution PSD of about 230 nanometers.

### Claim 17 (depends on 1)

A process in accordance with claim 1 wherein said toner is generated by the aggregation and coalescence of said latex polymer, said wax, and said colorant.

### Claim 18 (depends on 17)

A process in accordance with claim 17 wherein said aggregation is accomplished by heating at a temperature of below about the glass transition temperature of said polymer.

### Claim 19 (depends on 17)

A process in accordance with claim 17 wherein said temperature is from about 40° C. to about 70° C.

### Claim 20 (depends on 17)

A process in accordance with claim 17 wherein said coalescence is accomplished by heating at a temperature of about above the glass transition temperature of said polymer.

### Claim 21 (depends on 20)

A process in accordance with claim 20 wherein said heating is at a temperature of from about 80° C. to about 95° C.

### Claim 22 (depends on 17)

A process in accordance with claim 17 wherein said aggregation is accomplished by heating at a temperature of from about 35° C. to about 50° C., and said coalescence is accomplished by heating at a temperature of from about 70° C. to about 98° C.

### Claim 23 (depends on 1)

A process in accordance with claim 1 wherein the toner possesses a minimum fix temperature (MFT) of about 100° C. to about 180° C.

### Claim 24 (depends on 1)

A process in accordance with claim 1 wherein the toner hot offset temperature (HOT) is from about 195° C. to about 250° C.

### Claim 25 (depends on 1)

A process in accordance with claim 1 wherein said coagulant is comprised of polymetal chloride.

### Claim 26 (depends on 1)

A process in accordance with claim 1 wherein said polymer is selected from the group comprised of poly(styrene-butadiene), poly(methylstyrene-butadiene), poly(methyl methacrylate-butadiene), poly(ethyl methacrylate-butadiene), poly(propyl methacrylate-butadiene), poly(butyl methacrylate-butadiene), poly(methyl acrylate-butadiene), poly(ethyl acrylate-butadiene), poly(propyl acrylate-butadiene), poly(butyl acrylate-butadiene), poly(styrene-isoprene), poly(methylstyrene-isoprene), poly(methyl methacrylate-isoprene), poly(ethyl methacrylate-isoprene), poly(propyl methacrylate-isoprene), poly(butyl methacrylate-isoprene), poly(methyl acrylate-isoprene), poly(ethyl acrylate-isoprene), poly(propyl acrylate-isoprene), poly(butyl acrylate-isoprene), poly(styrene-propyl acrylate), poly(styrene-butyl acrylate), poly(styrene-butadiene-acrylic acid), poly(styrene-butadiene-methacrylic acid), poly(styrene-butadiene-acrylonitrile-acrylic acid), poly(styrene-butyl acrylate-acrylic acid), poly(styrene-butyl acrylate-methacrylic acid), poly(styrene-butyl acrylate-acrylononitrile), poly(styrene-butyl acrylate-acrylononitrile-acrylic acid), poly(styrene-butadiene-β-carboxyethyl acrylate), poly(styrene-butadiene-acrylonitrile-β-carboxyethyl acrylate), poly(styrene-butyl acrylate-β-carboxyethyl acrylate), and poly(styrene-butyl acrylate-acrylononitrile-β-carboxyethyl acrylate).

### Claim 27 (depends on 1)

A process in accordance with claim 1 wherein said coagulant is polymetal halide of a polyaluminum chloride, a polyaluminum sulfosilicate, or a polyaluminum sulfate.

### Claim 28 (depends on 1)

A process in accordance with claim 1 wherein said wax is selected in an amount of from about 5 to about 20 weight percent.

### Claim 29 (depends on 1)

A process in accordance with claim 1 wherein said colorant is a cyan, a magenta, a yellow, a black, or mixtures thereof.

### Claim 30 (depends on 1)

A process in accordance with claim 1 wherein said coagulant is comprised of a mixture of coagulants of a polymetal halide, and a second cationic coagulant wherein the first coagulant is present in the amount of about 0.02 to about 0.2 percent by weight of toner, and the second coagulant is present in the amount of about 0.05 to about 2 percent by weight of toner.

### Claim 31 (depends on 1)

A process in accordance with claim 1 wherein said colorant is a carbon black.

### Claim 32 (depends on 1)

A process in accordance with claim 1 wherein said colorant is a pigment, or a dye.

### Claim 33 (depends on 17)

A process in accordance with claim 17 wherein the aggregation temperature is from about 45° C. to about 60° C., and wherein the coalescence or fusion temperature is from about 80° C. to about 95° C., and wherein said coagulant is a polyaluminum halide.

### Claim 34

A process comprising heating a colorant dispersion with a latex, a wax dispersion, and a coagulant, and wherein the polymer latex selected possesses a weight average molecular weight of from about 20,000 to about 55,000, a number average molecular weight of from about 5,000 to about 20,000, an onset glass transition temperature Tg of from about 40° C. to about 80° C.

### Claim 35

A process comprising heating a colorant dispersion with a latex, a wax dispersion, and a coagulant, and wherein the polymer latex selected possesses a weight average molecular weight of from about 20,000 to about 55,000, a number average molecular weight of from about 5,000 to about 20,000, an onset glass transition temperature Tg of from about 40° C. to about 80° C.; and wherein said heating comprises a first and second heating, and wherein said second heating is above the temperature of said first heating.