- Web page: https://patentgrep.com/patent/US20040202877A1

## CPC

- C04B 41/009: {characterised by the material treated}
- C04B 41/5031: {Alumina}
- C04B 41/52: Multiple coating or impregnating {multiple coating or impregnating with the same composition or with compositions only differing in the concentration of the constituents, is classified as single coating or impregnation}
- C04B 41/87: Ceramics
- C04B 41/89: for obtaining at least two superposed coatings having different compositions
- C23C 16/403: {of aluminium, magnesium or beryllium}
- C04B 2111/0025: {Compositions or ingredients of the compositions characterised by the crystal structure}
- Y10T 428/24355: Continuous and nonuniform or irregular surface on layer or component [e.g., roofing, etc.]
- Y10T 428/24975: No layer or component greater than 5 mils thick
- Y10T 428/265: 1 mil or less
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A coated cutting tool is composed of one or more layers of refractory compounds of which at least one layer is single-phase α-alumina with a pronounced columnar grain-structure and strong texture in the [300]-direction. The alumina layer is preferably deposited by CVD (Chemical Vapor Deposition) and the preferred microstructure and texture are achieved by adding a second metal halide, and a texture modifying agent, to the reaction gas. When coated cemented carbide cutting tools according to the invention are used in the machining of steel or cast iron, several important improvements compared to prior art have been observed, particularly in the machining of nodular cast iron.

## Claims

### Claim 1

A cutting tool comprising:
a body comprising sintered cemented carbide, cermet or ceramic; and
a hard and wear resistant coating on at least functional parts of the body, said coating comprising a structure of one or more refractory layers of which at least one layer comprises an alumina layer having a thickness of 0.5-25 μm, and consisting essentially of single phase α-alumina textured in the [300]-direction with a texture coefficient larger than 1.5, the texture coefficient being defined as:
3 T ⁢ ⁢ C ⁡ ( h ⁢ ⁢ k ⁢ ⁢ l ) = I ⁡ ( h ⁢ ⁢ k ⁢ ⁢ l ) I 0 ⁡ ( h ⁢ ⁢ k ⁢ ⁢ l ) ⁢ { 1 n ⁢ ∑ I ⁡ ( h ⁢ ⁢ k ⁢ ⁢ l ) I 0 ⁡ ( h ⁢ ⁢ k ⁢ ⁢ l ) } - 1
where
I(hkl)=measured intensity of the (hkl) reflection,
Io(hkl)=standard intensity of the ASTM standard, powder pattern diffraction data, card number 43-1484,
n=number of reflections used in the calculation (hkl) reflections used are: (012), (104), (110), (113), (024), (116) and (300).

### Claim 2 (depends on 1)

The cutting tool according to claim 1, wherein the alumina layer has a thickness of 1-10 μm.

### Claim 3 (depends on 1)

The cutting tool according to claim 1, wherein the texture coefficient is larger than 3.

### Claim 4 (depends on 1)

The cutting tool according to claim 1, wherein the texture coefficient is larger than 5.

### Claim 5 (depends on 1)

The cutting tool according to claim 1, wherein the α-alumina layer contains 0.01-10 percent by weight of residues of a texture modifying agent.

### Claim 6 (depends on 5)

The cutting tool according to claim 5, wherein the α-alumina layer contains 0.01-5 percent by weight of residues of a texture modifying agent.

### Claim 7 (depends on 5)

The cutting tool according to claim 5, wherein the α-alumina layer contains less than 1 percent by weight of residues of a texture modifying agent.

### Claim 8 (depends on 1)

The cutting tool according to claim 1, further comprising at least one layer having a thickness of 0.1-10 μm, comprising a nitride, carbide, carbonitride, oxycarbide and/or oxycarbonitride of the metal titanium (TiCxNyOz) and that said layer is in contact with the α-alumina layer.

### Claim 9 (depends on 8)

The cutting tool according to claim 8, wherein the at least one layer has a thickness of 0.5-5 μm.

### Claim 10 (depends on 8)

The cutting tool according to claim 8, wherein the outer layer is α-alumina.

### Claim 11 (depends on 1)

The cutting tool according to claim 1, wherein the outer layer is TiN.

### Claim 12 (depends on 1)

The cutting tool according to claim 1, the surface of the coated cutting tool is smoothened by means of a brushing operation.

### Claim 13

A method of producing a coated cutting tool comprising at least one layer of textured α-alumina, the method comprising:
introducing a tool surface to be coated into a reactive atmosphere comprising H2 and/or Ar;
providing the reactive atmosphere with a concentration of oxidizing species below 5 ppm;
initiating nucleation of the α-alumina layer on the surface by first introducing HCl and CO2 gasses into the atmosphere, than introducing AlCl3 gas into the atmosphere;
maintaining a temperature of 950-1050° C. during nucleation of the α-alumina layer; and
introducing a catalyst and a texture modifying agent into the atmosphere during growth of the α-alumina layer.

### Claim 14 (depends on 13)

The method according to claim 13, wherein the oxidizing species comprises water vapor, the catalyst comprises H2S, and the texture modifying agent comprises ZrCl4.

### Claim 15 (depends on 13)

The method according to claim 13, wherein 0.05-10 percent by volume of the texture modifying agent is introduced.

### Claim 16 (depends on 13)

The method according to claim 13, wherein 0.2-5 percent by volume of the texture modifying agent is introduced.

### Claim 17 (depends on 13)

The method according to claim 13, wherein 0.5-2 percent by volume of the texture modifying agent is introduced.

### Claim 18 (depends on 14)

A method according to claim 14, wherein the addition of the texture modifying agent to the reaction gas mixture is 0.05-10 percent by volume of the total reaction gas mixture.

### Claim 19 (depends on 18)

The method according to claim 18, wherein the addition of the texture modifying agent is 0.2-5 percent by volume of the total reaction gas mixture.

### Claim 20 (depends on 18)

The method according to claim 18, wherein the addition of the texture modifying agent is 0.5-2 percent by volume of the total reaction gas mixture.