# US 2004/0202779 A1 · Method of making a field emission cold cathode

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0202779 A1
- Document ID: US20040202779A1
- Status: Published application
- Kind: A1
- Application number: 10/764,806
- Filed: 2004-01-26
- Published: 2004-10-14
- Earliest claimed: 2001-05-23
- Assignees: The United States of America as represented by the Secretary of the Air Force
- Inventors: Donald A. Shiffler JR.
- Web page: https://patentgrep.com/patent/US20040202779A1

## CPC

- H01J 1/304: Field-emissive cathodes
- H01J 2201/30446: characterised by the emitter material
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)

## Abstract

A method for making a field emission cold cathode for use in vacuum tubes. A carbon velvet material is coated with a low work function cesiated salt and bonded to a cathode surface. Alternatively, the carbon velvet material is bonded to the cathode surface before being coated with the cesiated salt. The coating may be applied by spraying the carbon velvet material with a cesiated salt solution, or by dipping the material into a crucible of molten cesiated salt. This abstract is provided to comply with the rules requiring an abstract, and is intended to allow a searcher or other reader to quickly ascertain the subject matter of the technical disclosure. It is submitted with the understanding that it will not be used to interpret or limit the scope or meaning the claims.

## Claims

### Claim 1

A method for coating a carbon velvet material attached to a cathode to make a field emission cold cathode, comprising:
forming a solution of a low work function cesiated salt and de-ionized water;
spraying the carbon velvet material with the cesiated salt solution to form a coated carbon velvet material;
baking the coated carbon velvet material at a temperature of at least 100° C. for approximately an hour in a vacuum oven evacuated to less than 1 torr.; and
venting the vacuum oven to an atmospheric pressure using dry nitrogen.

### Claim 2 (depends on 1)

A coating method as recited in claim 1, wherein the spraying step includes pressurizing a spraying means with dry nitrogen.

### Claim 3 (depends on 1)

A coating method as recited in claim 1, wherein the cesiated salt is selected from a group consisting of cesium tellurate and cesium bromide.

### Claim 4 (depends on 1)

A coating method as recited in claim 1, wherein the steps of forming, spraying, baking, and venting are repeated until a film of cesiated salt having a thickness of 1 angstrom to 10 microns is formed on each of a plurality of shafts of the carbon velvet material.

### Claim 5

A method of making a field emission cold cathode, comprising:
forming a solution of a cesiated salt;
coating a carbon velvet material with the cesiated salt solution; and
bonding the carbon velvet material to a cathode.

### Claim 6 (depends on 5)

A method as recited in claim 5 wherein the carbon velvet material is comprised of shaft having tips, and the coating step coats only the tips with the cesiated salt solution.

### Claim 7 (depends on 5)

A method as recited in claim 5 wherein the carbon velvet material is comprised of shafts, and the coating step coats a plurality of the shafts with a film of cesiated salt having a thickness of 1 angstrom to 10 microns.

### Claim 8

A method of making a field emission cold cathode, comprising:
depositing a vaporized cesiated salt solution onto fibers of a carbon velvet material;
forming cesiated salt crystals on the fibers; and
bonding the carbon velvet material to a cathode.

### Claim 9 (depends on 8)

A method as recited in claim 8 wherein the solution includes de-ionized water and the forming step is comprised of evaporating the de-ionized water.

### Claim 10 (depends on 9)

A method as recited in claim 9 wherein the fibers have tips, and the cesiated salt crystals are formed only on the tips.

### Claim 11

A method of making a field emission cold cathode, comprising:
forming a film of cesiated salt having a thickness of 1 angstrom to 10 microns on each of a plurality of shafts of a carbon velvet material; and
bonding the carbon velvet material to a cathode.

### Claim 12 (depends on 11)

A method as recited in claim 11 wherein the shafts have tips, and the film is formed only on the tips.

### Claim 13

A method of making a field emission cold cathode comprising:
attaching a carbon velvet material having fibers to a cathode;
dipping the fibers in a molten cesiated salt solution; and
cooling the solution while the fibers are immersed in the solution.

### Claim 14 (depends on 13)

A method as recited in claim 13 wherein the fibers have tips, and only the tips are dipped in the molten cesiated salt solution.

### Claim 15

A method of making a field emission cold cathode comprising:
attaching a carbon velvet material having fibers to a cathode;
dipping the fibers in a molten cesiated salt solution;
removing the fibers from the solution; and
cooling the fibers after the fibers have been removed from the solution.

### Claim 16 (depends on 15)

A method as recited in claim 15 wherein the fibers have tips, and only the tips are dipped in the molten cesiated salt solution.

### Claim 17 (depends on 15)

A method as recited in claim 15 wherein the steps of dipping, removing and cooling are repeated until a film of cesiated salt having a thickness of 1 angstrom to 10 microns is formed on a plurality of the fibers.

### Claim 18 (depends on 17)

A method as recited in claim 17 wherein the fibers have tips, and only the tips are dipped in the molten cesiated salt solution.