# US 2004/0202227 A1 · Temperature sensor and method of making the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0202227 A1
- Document ID: US20040202227A1
- Status: Published application
- Kind: A1
- Application number: 10/803,556
- Filed: 2004-03-17
- Published: 2004-10-14
- Earliest claimed: 2001-12-04
- Assignees: Delphi Technologies, Inc.
- Inventors: Charles Scott Nelson; Paul Casey Kikuchi; James Paul Vargo; Douglas James Behrendt; Walter T. Symons; William J. LaBarge; Kaius K. Polikarpus; Rick D. Kerr; Jinping Zhang; Paul R. Daniel JR.
- Web page: https://patentgrep.com/patent/US20040202227A1

## CPC

- H01C 17/075: by thin-film techniques
- G01K 7/18: the element being a linear resistance, e.g. platinum resistance thermometer (G01K7/26 takes precedence)
- G01K 15/00: Testing or calibrating of thermometers
- H01C 17/242: by laser
- Y10T 29/49004: including measuring or testing of device or component part
- Y10T 29/49085: Thermally variable
- H01C: RESISTORS
- G01K: MEASURING TEMPERATURE; MEASURING QUANTITY OF HEAT; THERMALLY-SENSITIVE ELEMENTS NOT OTHERWISE PROVIDED FOR (radiation pyrometry G01J5/00)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A method for manufacturing a planar sensor, comprises disposing a film of a material on a substrate, wherein the material is selected from the group consisting of platinum, rhodium, palladium and mixtures and alloys comprising at least one of the foregoing materials; annealing the material; measuring a resistance value of the material; laser trimming the annealed material; heat treating the laser trimmed material; and laser trimming the heat treated material to form the sensor.

## Claims

### Claim 1

A method for manufacturing a planar sensor, comprising:
disposing a film of a material on a substrate, wherein the material is selected from the group consisting of platinum, rhodium, palladium, iridium, gold, and mixtures and alloys comprising at least one of the foregoing materials;
annealing the material;
measuring a resistance value of the material;
laser trimming the annealed material;
heat treating the laser trimmed material; and
laser trimming the heat treated material to form the sensor.

### Claim 2 (depends on 1)

The method of claim 1, wherein the film has a nominal thickness of greater than or equal to about 2 micrometers.

### Claim 3 (depends on 1)

The method of claim 1, wherein laser trimming the annealed material further comprises setting a laser trimming device to a first setting to achieve a first inputted resistance value and laser trimming the heat treated material further comprises setting a laser trimming device to a second setting to achieve a second inputted resistance value.

### Claim 4 (depends on 3)

The method of claim 3, further comprising laser trimming an amount of the annealed material sufficient to meet the first inputted resistance value, and laser trimming an amount of the heat treated material sufficient to meet the second inputted resistance value.

### Claim 5 (depends on 1)

The method of claim 1, wherein the heat treating is maintained until an inflection in a resistance versus time curve is reached.

### Claim 6 (depends on 1)

The method of claim 1, wherein the heat treating is at a temperature of about 1,000° C. to about 1,600° C.

### Claim 7 (depends on 1)

The method of claim 1, further comprising:
determining a value for a resistance overshoot as a function of a thermal coefficient of resistance of the material; and
wherein the annealed material is laser trimmed by an amount determined in relation to the resistance overshoot value.

### Claim 8 (depends on 1)

The method of claim 1, wherein laser trimming the annealed material further comprises cutting a pattern having an elongated configuration into the material.

### Claim 9 (depends on 8)

The method of claim 8, wherein the elongated configuration is chosen from a serpentine pattern and a spiral pattern.

### Claim 10 (depends on 1)

The method of claim 1, further comprising laser trimming greater than 25 mm of the annealed material.

### Claim 11 (depends on 10)

The method of claim 10, comprising laser trimming greater than or equal to about 50 mm of the annealed material.

### Claim 12 (depends on 11)

The method of claim 11, comprising laser trimming about 100 mm to about 250 mm of the annealed material.

### Claim 13 (depends on 1)

The method of claim 1, wherein the material comprises platinum.

### Claim 14 (depends on 1)

The method of claim 1, wherein the material is platinum.

### Claim 15

A method for manufacturing a planar temperature sensor, the method comprising:
disposing a film of material having a material thermal coefficient of resistance of greater than or about 800 parts per million per degree Celsius, on a substrate;
measuring a resistance value of the material;
setting a laser trimming device to ablate material consistent with achieving the inputted resistance value; and
ablating greater than or equal to about 50 mm of the material to form the sensor.

### Claim 16

A method for manufacturing a planar temperature sensor, the method comprising:
disposing a material having a thermal coefficient of resistance of greater than about 800 parts per million per degree Celsius, on a substrate;
measuring a resistance value of the material;
setting a laser trimming device to ablate material consistent with achieving the inputted resistance value; and
ablating greater than or equal to about 50 mm of the material.

### Claim 17

A method for manufacturing a planar temperature sensor, the method comprising:
disposing a material having a thermal coefficient of resistance of greater than about 800 parts per million per degree Celsius, wherein the substrate has a single film thereon;
measuring a resistance value of the material;
setting a laser trimming device to ablate material consistent with achieving the inputted resistance value; and
ablating the material to form the sensor.

### Claim 18

A method of making a planar temperature sensor, the method comprising:
disposing a material on a substrate, wherein the material is selected from the group consisting of platinum, rhodium, palladium, gold, and mixtures and alloys comprising at least one of the foregoing materials;
annealing the material; and
vaporizing a portion of the material to form a sensing element on the substrate;
vaporizing a portion of the substrate; and
depositing the vaporized substrate material on the sensing element to form a protective coating.

### Claim 19 (depends on 18)

The method of claim 18, further comprising disposing an additional protective layer over the sensing element.

### Claim 20 (depends on 18)

The method of claim 18, wherein the substrate comprises about 86 wt. % alumina to about 99.5 wt. % alumina, based on a total weight of the substrate.

### Claim 21 (depends on 18)

The method of claim 18, wherein the substrate comprises greater than or equal to about 95 wt. % alumina, based on a total weight of the substrate.

### Claim 22 (depends on 18)

The method of claim 18, wherein the protective coating has a thickness sufficient to inhibit grain growth, pore coalescence, and pore nucleation in the sensing element.

### Claim 23 (depends on 22)

The method of claim 22, wherein the thickness is about 2 nm to about 2000 nm.

### Claim 24 (depends on 18)

The method of claim 18, wherein the protective coating comprises a material selected from the group consisting of aluminum, silicon, yttrium, zirconium, and mixtures comprising at least one of the foregoing materials.

### Claim 25 (depends on 18)

The method of claim 18, wherein the protective coating is an aluminide or a silicide.

### Claim 26 (depends on 18)

The method of claim 18, further comprising cutting a margin portion of the sensing element and a portion of the substrate, such that vaporized substrate material is re-deposited onto the sensing element to form a protective coating.

### Claim 27

A method of making a planar temperature sensor, the method comprising:
disposing a material on a substrate, wherein the material is selected from the group consisting of platinum, rhodium, palladium, gold, and mixtures and alloys comprising at least one of the foregoing materials;
annealing the material; and
vaporizing a portion of the material to form a sensing element on the substrate;
vaporizing a secondary target material; and
depositing the vaporized secondary target material on the sensing element to form a protective coating.

### Claim 28 (depends on 27)

The method of claim 27, wherein the secondary target comprises about 86 wt. % alumina to about 99.5 wt. % alumina, based on a total weight of the secondary target.

### Claim 29 (depends on 27)

The method of claim 27, wherein the secondary target comprises greater than or equal to about 95 wt. % alumina, based on a total weight of the secondary target.

### Claim 30 (depends on 27)

The method of claim 27, wherein the protective coating is an aluminide or a silicide.

### Claim 31

A planar temperature sensor comprising:
a substrate;
a sensing material disposed on the substrate, wherein the sensing material is selected from the group consisting of platinum, rhodium, palladium and mixtures and alloys comprising at least one of the foregoing sensing materials;
a protective coating disposed on at least a portion of the sensing material, wherein the protective coating comprises an aluminide or silicide of the sensing material.

### Claim 32 (depends on 31)

The planar temperature sensor of claim 31, wherein the protective coating further comprises an additional material selected from the group consisting of yttrium, zirconium, and mixtures comprising at least one of the foregoing materials.

### Claim 33 (depends on 32)

The planar temperature sensor of claim 32, wherein the protective coating has a thickness of about 2 nm to about 20 nm.