# US 2004/0200295 A1 · MEMS sensor for detecting stress corrosion cracking

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0200295 A1
- Document ID: US20040200295A1
- Status: Published application
- Kind: A1
- Application number: 10/782,011
- Filed: 2004-02-19
- Published: 2004-10-14
- Earliest claimed: 2003-02-28
- Assignees: Southwest Research Institute
- Inventors: Christopher S. Brossia; Heather S. Hanson
- Web page: https://patentgrep.com/patent/US20040200295A1

## CPC

- G01N 27/24: Investigating the presence of flaws
- G01N 17/00: Investigating resistance of materials to the weather, to corrosion, or to light
- G01N 27/20: Investigating the presence of flaws
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)

## Abstract

A sensor for measuring stress corrosion cracking and methods of using the sensor. The sensor is a MEMS device and has a cantilevered beam made from a material of interest. The sensor has on-chip electrical connections for measuring electrical characteristics that indicate cracking of the beam. The sensor may further have on-chip actuators for applying stress to the beam.

## Claims

### Claim 1

A MEMS sensor for measuring stress corrosion cracking of a material of interest, comprising:
a substrate;
an electrically conductive cantilever beam fabricated upon the substrate, the beam having a fixed end attached to the substrate and having a free end, and the beam being made from the material of interest; and
at least one electrical connection to the beam.

### Claim 2 (depends on 1)

The MEMS sensor of claim 1, further comprising at least one actuator fabricated on the substrate, operable to apply stress to the beam.

### Claim 3

A MEMS sensor for measuring stress corrosion cracking of a material of interest, comprising:
a substrate;
an electrically conductive cantilever beam fabricated upon the substrate, the beam having a fixed end attached to the substrate and having a free end, and the beam being made from the material of interest;
at least two conductive pads fabricated on the substrate adjacent the length of the beam; and
conductive leads for electrically connecting the conductive pads to the beam.

### Claim 4 (depends on 3)

The sensor of claim 3, further comprising at least one actuator fabricated on the substrate, operable to apply stress to the beam.

### Claim 5 (depends on 4)

The sensor of claim 4, wherein the actuator moves the beam horizontally over the surface of the substrate.

### Claim 6 (depends on 3)

The sensor of claim 3, wherein the beam is notched to encourage cracking to occur at a predetermined location on the beam.

### Claim 7 (depends on 3)

The sensor of claim 3, further comprising a scale fabricated at the free end of the beam.

### Claim 8 (depends on 3)

The sensor of claim 3, wherein the beam has single arm.

### Claim 9 (depends on 3)

The sensor of claim 3, wherein the beam has a double arm.

### Claim 10 (depends on 9)

The sensor of claim 9, wherein the conductive pads are along the length of a first arm, and further comprising conductive pads along the length of a second arm, and wherein the conductive leads provide an electrical connection to each of said pads.

### Claim 11 (depends on 3)

The sensor of claim 3, wherein the conductive pads are fixed.

### Claim 12 (depends on 3)

The sensor of claim 3, wherein the conductive pads are moveable.

### Claim 13

A method of measuring stress corrosion cracking of a material of interest, comprising the steps of:
placing a MEMS sensor in an environment of interest, the MEMS sensor having a substrate, a cantilevered beam with a free end and a fixed end attached to the substrate, and having electrical connections to the beam to at least two points along the length of the beam;
wherein the beam is made from the material of interest;
applying stress to the beam;
exposing the beam to environmental corrosion; and
measuring the electrical resistance along the length of the beam.

### Claim 14 (depends on 13)

The method of claim 13, further comprising the step of notching the beam to encourage cracking to occur at a predetermined location on the beam.

### Claim 15 (depends on 13)

The method of claim 13, wherein the step of applying stress is performed such that the beam moves horizontally across the substrate.

### Claim 16 (depends on 13)

The method of claim 13, wherein the beam is divided into two arms extending from the fixed end of the beam, and wherein the step of applying stress is performed such that stress is applied to one of the arms.

### Claim 17 (depends on 13)

The method of claim 13, wherein the beam has a single arm, to which stress is applied and whose resistance is measured.

### Claim 18 (depends on 13)

The method of claim 13, wherein the step of applying stress is performed with at least one actuator integrated onto the substrate.

### Claim 19

A MEMS sensor for measuring stress corrosion cracking of a material of interest, comprising:
a substrate;
an electrically conductive cantilever beam fabricated upon the substrate, the beam having a fixed end attached to the substrate and having a free end, and at least a portion of the length of the beam being made from the material of interest; and
a capacitance meter fabricated adjacent the free end of the beam and operable to measure the capacitance between the free end of the beam and the meter.

### Claim 20 (depends on 19)

The sensor of claim 19, wherein the beam is entirely made from the material.

### Claim 21 (depends on 19)

The sensor of claim 19, further comprising at least one actuator fabricated on the substrate, operable to apply stress to the beam.

### Claim 22

A method of measuring stress corrosion cracking of a material, comprising the steps of:
placing a MEMS sensor in an environment of interest, the MEMS sensor having a substrate, a cantilevered beam with a free end and a fixed end attached to the substrate, and having an electrical connection to the beam;
wherein at least a portion of the beam is made from the material;
applying stress to the beam;
exposing the beam to environmental corrosion;
placing a capacitance meter near the free end of the beam; and
measuring the electrical capacitance between the free end of the beam and the capacitance meter.

### Claim 23 (depends on 22)

The method of claim 22, wherein the step of applying stress is performed with at least one actuator integrated onto the substrate.