# US 2004/0200240 A1 · Fluorine-doped quartz glass article and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0200240 A1
- Document ID: US20040200240A1
- Status: Published application
- Kind: A1
- Application number: 10/819,176
- Filed: 2004-04-07
- Published: 2004-10-14
- Earliest claimed: 2003-04-08
- Assignees: Shin-Etsu Chemical Co., Ltd.
- Inventors: Jun Abe; Nobuyasu Mantoku
- Web page: https://patentgrep.com/patent/US20040200240A1

## CPC

- C03B 37/01446: {Thermal after-treatment of preforms, e.g. dehydrating, consolidating, sintering (C03B37/01853 takes precedence)}
- C03C 3/06: with more than 90% silica by weight, e.g. quartz {(C03C3/045 takes precedence)}
- C03C 13/046: {Multicomponent glass compositions}
- C03B 2201/075: Hydroxyl ion (OH)
- C03B 2201/12: doped with fluorine (C03B2201/14 takes precedence)
- C03B 2203/22: Radial profile of refractive index, composition or softening point
- C03C 2201/12: containing fluorine (C03C2201/14 takes precedence)
- C03C 2203/22: using colloidal silica sols
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

A method for manufacturing a fluorine-doped quartz glass article by sintering a porous glass preform moving in a heat zone in an atmosphere of a fluorine gas is disclosed, wherein a fluorine gas process is performed by setting a moving speed of the porous glass preform in the heat zone heated at 1000° C. or more in order that L/V is 40 minutes or more, where L is the length (mm) of a heater, and V is the moving speed (mm/min). The temperature of the heat zone may be vitrification temperature. The fluorine gas process may be performed in the heat zone which is at 1000° C. or more not to perform a vitrification process, and then the vitrification process maybe performed by increasing the temperature of the heat zone.

## Claims

### Claim 1

A method for manufacturing a fluorine-doped quartz glass article by sintering a porous glass preform moving in a heat zone in an atmosphere of a fluorine gas, wherein a fluorine gas process is performed by setting a moving speed of said porous glass preform in said heat zone heated at 1000° C. or more in order that L/V is 40 minutes or more, where L is length (mm) of a heater, and V is said moving speed (mm/min).

### Claim 2 (depends on 1)

A method for manufacturing a fluorine-doped quartz glass article as claimed in claim 1, wherein temperature of said heat zone is vitrification temperature.

### Claim 3 (depends on 1)

A method for manufacturing a fluorine-doped quartz glass article as claimed in claim 1, wherein said fluorine gas process is performed in said heat zone which is at 1000° C. or more not to perform a vitrification process, and then said vitrification process is performed by increasing said temperature of said heat zone.

### Claim 4 (depends on 3)

A method for manufacturing a fluorine-doped quartz glass article as claimed in claim 3, wherein said fluorine gas process is performed by setting said moving speed of said porous glass preform in said heat zone heated at 1000° C. or more in order that L/V1+L/V2 is 40 minutes or more, while moving said porous glass preform at a moving speed V1 in said heat zone which is at 1000° C. or more not to perform said vitrification process, and at a moving speed V2 in said heat zone at vitrification temperature.

### Claim 5 (depends on 1)

A method for manufacturing a fluorine-doped quartz glass article as claimed in claim 1, wherein said porous glass preform is solid.

### Claim 6 (depends on 1)

A method for manufacturing a fluorine-doped quartz glass article as claimed in claim 1, wherein said porous glass preform is hollow.

### Claim 7 (depends on 1)

A method for manufacturing a fluorine-doped quartz glass article as claimed in claim 1, wherein said porous glass preform is formed by depositing glass particles on a core rod.

### Claim 8

A method for manufacturing a fluorine-doped quartz glass article, wherein the pressure inside a chamber is positive pressure, when a heating process is performed on a porous glass preform in an atmosphere of a fluorine gas.

### Claim 9 (depends on 8)

A method for manufacturing a fluorine-doped quartz glass article as claimed in claim 8, wherein said heating process is a vitrification process.

### Claim 10 (depends on 9)

A method for manufacturing a fluorine-doped quartz glass article as claimed in claim 9, wherein temperature in said vitrification process is 1350° C. or more.

### Claim 11 (depends on 8)

A method for manufacturing a fluorine-doped quartz glass article as claimed in claim 8, wherein said positive pressure is 10 to 500 Pa.

### Claim 12 (depends on 8)

A method for manufacturing a fluorine-doped quartz glass article as claimed in claim 8, wherein said heating process is performed to prevent external air from entering through a sealed part of said chamber.

### Claim 13 (depends on 8)

A method for manufacturing a fluorine-doped quartz glass article as claimed in claim 8, wherein amount of water contained in said gas supplied into said chamber is 3 ppm or less.

### Claim 14 (depends on 8)

A fluorine-doped quartz glass article manufactured by said method as claimed in claim 8, wherein amount of hydroxyl groups is 50 ppb or less.