# US 2004/0175961 A1 · Two-step post nitridation annealing for lower EOT plasma nitrided gate dielectrics

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0175961 A1
- Document ID: US20040175961A1
- Status: Published application
- Kind: A1
- Application number: 10/794,707
- Filed: 2004-03-04
- Published: 2004-09-09
- Earliest claimed: 2003-03-07
- Inventors: Christopher Olsen
- Web page: https://patentgrep.com/patent/US20040175961A1

## CPC

- H10P 14/6526: {introduced into an oxide material, e.g. changing SiO to SiON}
- H10D 64/0134: {with a treatment, e.g. annealing, after the formation of the insulator and before the formation of the conductor}
- H10D 64/693: {the insulator comprising nitrogen, e.g. nitrides, oxynitrides or nitrogen-doped materials}
- H10P 14/6529: {by exposure to a gas or vapour}
- H10P 14/6532: {by exposure to a plasma}
- H10D 64/01344: {in a nitrogen-containing ambient, e.g. N2O oxidation}
- H10P 14/6927: {the material being a silicon oxynitride, e.g. SiON or SiON:H}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A method of forming a dielectric film that includes nitrogen. The method includes incorporating nitrogen into a dielectric film using a plasma nitridation process to form a silicon oxynitride film. The silicon oxynitride film is annealed first in an inert or reducing ambient at a temperature ranging between about 700° C. and 1100° C. The silicon oxynitride film is annealed for the second time in an oxidizing ambient at a temperature ranging between about 900° C. and 1100° C.

## Claims

### Claim 1

A method of forming a dielectric film comprising:
incorporating nitrogen into a dielectric film using a plasma nitridation process to form a silicon oxynitride film;
annealing the silicon oxynitride film in an inert or reducing ambient at a temperature ranging between about 700° C. and 1100° C.; and
annealing the silicon oxynitride in an oxidizing ambient at a temperature ranging between about 900° C. and 1100° C.

### Claim 2 (depends on 1)

The method of forming a dielectric film of claim 1 wherein the nitrogen incorporated into the dielectric film forms a nitrogen concentration peak that occurs at the top surface of the dielectric film.

### Claim 3 (depends on 1)

The method of forming a dielectric film of claim 1 wherein the nitrogen incorporated into the dielectric film has a nitrogen concentration equal to or greater than 5%.

### Claim 4 (depends on 1)

The method of forming a dielectric film of claim 1 wherein the dielectric film is equal to or less than about 14 angstrom.

### Claim 5 (depends on 1)

The method of forming a dielectric film of claim 1 wherein the annealing of the silicon oxynitride film in an inert or reducing ambient includes annealing the silicon oxynitride film in an inert gas or a mixture of inert gas.

### Claim 6 (depends on 1)

The method of claim 1 wherein the annealing of the silicon oxynitride film in an oxidizing ambient includes annealing the silicon oxynitride film with oxygen (02) or oxygen comprising gas.

### Claim 7 (depends on 1)

The method of forming a dielectric film of claim 1 wherein the dielectric film is silicon dioxide (SiO2).

### Claim 8 (depends on 1)

The method of forming a dielectric film of claim 1 wherein the plasma nitridation process includes decoupled plasma nitridation.

### Claim 9

A method of forming a gate stack comprising:
forming a silicon dioxide film on a substrate;
incorporating nitrogen into the silicon dioxide film using a plasma nitridation process to form a silicon oxynitride film, the plasma nitridation occurs at pressure less than about 10 mTorr in a presence of nitrogen gas;
annealing the silicon oxynitride film in an inert or reduced ambient at a temperature ranging between about 700° C. and 1100° C.;
annealing the silicon oxynitride film in an oxidizing ambient at a temperature between about 700° C. and 1100° C.; and
forming a cap layer on the silicon oxynitride.

### Claim 10 (depends on 9)

The method of forming a gate stack of claim 9 wherein the annealing of the silicon oxynitride film in an inert or reducing ambient includes annealing the silicon oxynitride film in an inert gas or a mixture of inert gas.

### Claim 11 (depends on 9)

The method of forming a gate stack of claim 9 wherein the annealing of the silicon oxynitride film in an oxidizing ambient includes annealing the silicon oxynitride film with oxygen (O2) or oxygen comprising gas.

### Claim 12 (depends on 9)

The method of forming a gate stack of claim 9 wherein the nitrogen incorporated into the dielectric film has a nitrogen concentration equal to or greater than 5%.

### Claim 13

A method of forming a gate stack comprising:
placing a substrate into a first processing chamber of a cluster tool, the cluster tool having a plurality of processing chambers;
forming a silicon dioxide film on the substrate in the first processing chamber;
without breaking vacuum, transferring the substrate from the first processing chamber into a second processing chamber capable of performing a plasma nitridation process;
introducing a nitrogen reaction gas into the second processing chamber, to perform the plasma nitridation process while maintaining pressure of the second processing chamber at about or less than about 10 Torr to form a silicon oxynitride film;
without breaking vacuum, transferring the substrate from the second processing chamber to a third processing chamber capable of performing a rapid thermal reaction process to perform a first post plasma nitridation annealing on the silicon oxynitride in an inert or reducing ambient and to perform a second post plasma nitridation annealing on the silicon oxynitride in an oxidizing ambient; and
without breaking vacuum, transferring the substrate from the third processing chamber to a fourth processing chamber capable of performing a deposition process to form a gate electrode on the silicon oxynitride.

### Claim 14 (depends on 13)

The method of claim 13 wherein the gate electrode is one of a polysilicon film or an amorphous silicon film.

### Claim 15 (depends on 13)

The method of claim 13 further comprising:
continuing the plasma nitridation process for a sufficient amount of time for nitrogen to be incorporated into the silicon dioxide film to a nitrogen concentration of about or more than 5%.

### Claim 16 (depends on 13)

The method of claim 13 wherein the first post plasma nitridation annealing occurs at a temperature between about 700° C. and about 1100° C.

### Claim 17 (depends on 13)

The method of claim 13 wherein the second post plasma nitridation annealing occurs at a temperature between about 900° C. and 1100° C.

### Claim 18 (depends on 13)

The method of forming a gate stack of claim 13 wherein the nitrogen incorporated into the dielectric film forms a nitrogen concentration peak that occurs at the top surface of the dielectric film.

### Claim 19 (depends on 13)

The method of forming a dielectric film of claim 13 wherein the annealing of the silicon oxynitride film in an inert or reducing ambient includes annealing the silicon oxynitride film in an inert gas or a mixture of inert gas.

### Claim 20 (depends on 13)

The method of claim 13 wherein the annealing of the silicon oxynitride film in an oxidizing ambient includes annealing the silicon oxynitride film with oxygen (02) or oxygen comprising gas.

### Claim 21 (depends on 13)

The method of forming a dielectric film of claim 13 wherein the plasma nitridation process includes decoupled plasma nitridation.

### Claim 22

A method of treating a dielectric film comprising:
exposing the dielectric film to plasma nitridation to incorporate nitrogen into the dielectric film.
subjecting the dielectric film to a first post plasma nitridation annealing wherein a reducing or inert ambient is used, the first post plasma nitridation annealing densifier nitrogen in the dielectric film; and
subjecting the dielectric film to a second post plasma nitration annealing wherein an oxidizing ambient is used.

### Claim 23 (depends on 19)

The method of treating a dielectric film of claim 19 wherein the plasma nitridation is decoupled plasma nitridation.

### Claim 24 (depends on 19)

The method of treating a dielectric film of claim 19 wherein the dielectric film is silicon dioxide (SiO2).

### Claim 25 (depends on 19)

The method of treating a dielectric film of claim 19 wherein after the nitrogen is incorporated, a silicon oxinytride is formed.

### Claim 26 (depends on 19)

The method of treating a dielectric film of claim 19 wherein the first post plasma nitridation annealing occurs at a temperature ranging between about 700° C. and 1100° C.

### Claim 27 (depends on 19)

The method of treating a dielectric film of claim 19 wherein the second post plasma nitridation annealing occurs at a temperature ranging between about 900° C. and 1100° C.

### Claim 28 (depends on 19)

The method of treating a dielectric film of claim 19 wherein the reducing or inert ambient includes using an inert gas to create the reducing or inert ambient.

### Claim 29 (depends on 19)

The method of treating a dielectric film of claim 19 wherein the oxidizing ambient includes using oxygen comprising gas or gas mixture to create the oxidizing ambient.

### Claim 30 (depends on 19)

The method of treating a dielectric film of claim 19 wherein the nitrogen incorporated into the dielectric film has a nitrogen concentration equal to or greater than 5%.