Annealed polypropylene pipes and fittings
OwnerEmmanuel Michel Delaite, Virgile Joel Maurice Rouyerinventors
Life of this patent
Estimating the term…
Loading patent…
OwnerEmmanuel Michel Delaite, Virgile Joel Maurice Rouyerinventors
Estimating the term…
A process of manufacture of pipes and of fittings comprising a first stage of utilising a propylene polymer based compound comprising: from 76 to 98 parts by weight of a crystalline homopolymer of propylene or of a crystalline statistical copolymer (A) of propylene which may contain up to 1.5% molar of monomer units derived from ethylene and/or from an alpha-elefin containing from 4 to 6 carbon atoms; from 24 to 2 parts by weight of a statistical copolymer (B) containing from 40 to 70% molar of monomer units derived from ethylene and/or from an alpha-olefin containing from 4 to 6 carbon atoms, so as to obtain a pipe or a fitting, and a second stage of annealing said pipes or fittings by heating for a perior of between one hour and three days at a temperature between 110 and 155° C.
Process for the manufacture of pipes and fittings, comprising a first stage of making a pipe or a fitting from a propylene polymer based composition comprising:
Process according to any preceding claim, wherein the heating in the annealing step lasts for at least 2 hours.
Dependencies are inferred from the claim text.