# US 2004/0115347 A1 · Crack resistant sol-gel wafer coatings for integrated optics

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0115347 A1
- Document ID: US20040115347A1
- Status: Published application
- Kind: A1
- Application number: 10/320,313
- Filed: 2002-12-15
- Published: 2004-06-17
- Earliest claimed: 2002-12-15
- Assignees: Optinetrics, Inc.
- Inventors: Fernando A. Sigoli; Lothar U. Kempen; Edgar A. Mendoza
- Web page: https://patentgrep.com/patent/US20040115347A1

## CPC

- C03C 1/008: {for the production of films or coatings}
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

A method of preparing a multi-layer, crack resistant sol-gel glass derived coating on a substrate by removing the outer periphery of each layer before curing the layer and depositing any succeeding layer.

## Claims

### Claim 1

A method of making a crack resistant sol-gel derived glass, comprising the steps of:
a. spin-coating a substrate selected from the group consisting of glass and silicon to deposit a first layer of sol-gel;
b. removing the outer periphery of said first layer of spin-coated sol-gel from said substrate;
c. spin-coating at least one additional layer of sol-gel on top of said first layer; and
d. removing more of the outer periphery of each said additional layer than has been removed from each previously deposited layer.

### Claim 2 (depends on 1)

A method according to claim 1 wherein said substrate having said outer periphery of said first layer removed is cured prior to spin-coating said at least one additional layer.

### Claim 3 (depends on 2)

A method according to claim 2 wherein the spin-coated sol-gel substrate is cured by baking.

### Claim 4 (depends on 1)

A method according to claim 1 wherein said outer periphery of said sol-gel is removed by spraying a solvent at said outer periphery.

### Claim 5 (depends on 1)

A method according to claim 1 wherein said first layer of sol-gel is formed of a viscous mixture of methyl trimethoxysilane and tetraethyl orthosilicate in the presence of diluted hydrochloric acid.

### Claim 6

A method of preparing a multi-layer, crack resistant sol-gel glass derived coating on a substrate by the steps of
spin coating a first sol-gel layer on said substrate;
removing an outer peripheral portion of said spin-coated layer;
curing said spin coated layer; and
removing from each subsequently deposited spin-coated layer an additional outer peripheral portion of before curing said subsequently deposited layer.