US 2004/0106469 A1Published application
Thin-layer-covered golf ball with improved velocity
AssigneeAcushnet Company
InventorsShenshen Wu, Edmund A. Hebert, Laurent Bissonnette, David A. Bulpett, Murali Rajagopalan, Peter Voorheis, Mark N. Wrigley
Life of this patent
Estimating the term…
Abstract
A golf ball comprising a center comprising a polybutadiene having a molecular weight of greater than 200,000 and a resilience index of at least about 40; and a cover layer comprising a polyurethane composition formed from a prepolymer having no greater than 7.5 percent by weight unreacted isocyanate groups.
Claims21
A golf ball comprising:
- a center comprising a resilient polymer comprising:
- a rubber material having a molecular weight of greater than about 200,000, wherein the rubber material has a resilience index of at least about 40, and wherein the resilience index of the rubber material is calculated using the formula:
- Resilience Index=100,000*[(Tan δ at 10 cpm)−(Tan δ at 1000 cpm)]/990;
- a crosslinking material present in an amount of about 10 to about 40 parts per hundred of the resilient polymer;
- a free radical source present in an amount of about 0.1 to about 15 parts per hundred of the resilient polymer;
- a cis-to-trans catalyst present in an amount of about 0.1 to about 10 parts per hundred of the resilient polymer;
- and
- a cover comprising a thermoplastic or thermoset polyurethane.
5 more elements
A golf ball comprising:
- a center comprising a resilient polymer, wherein the resilient polymer comprises:
- polybutadiene having a molecular weight of about 300,000 to about 500,000 and a resilience index of about 40, wherein the resilience index is calculated using the formula:
- Resilience Index=100,000*[(Tan δ at 10 cpm)−(Tan δ at 1000 cpm)]/990;
- a crosslinking material present in an amount of about 10 to about 40 parts per hundred of the resilient polymer;
- a free radical source present in an amount of about 0.1 to about 15 parts per hundred of the resilient polymer;
- a cis-to-trans catalyst present in an amount of about 0.1 to about 10 parts per hundred of the resilient polymer;
- and
- a cover formed of a castable reactive liquid material.
5 more elements
A golf ball comprising:
- a center comprising a resilient polymer, wherein the resilient polymer comprises:
- a rubber material having a molecular weight of greater than about 200,000 and a resilience index of about 50, wherein the resilience index is calculated using the equation:
- Resilience Index=100,000*[(Tan δ at 10 cpm)−(Tan δ at 1000 cpm)]/990;
- a crosslinking material present in an amount of about 10 to about 40 parts per hundred of the resilient polymer;
- a free radical source present in an amount of about 0.1 to about 15 parts per hundred of the resilient polymer;
- a cis-to-trans catalyst present in an amount sufficient to produce a resilient polymer comprising about 12 percent or greater trans-isomer;
- and
- a cover formed of a thermoset or thermoplastic polyurethane, wherein the cover has a hardness of about 30 Shore D to about 60 Shore D.