# US 2004/0094247 A1 · Aluminum-killed medium-carbon steel sheet for containers and process for its prepration

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0094247 A1
- Document ID: US20040094247A1
- Status: Published application
- Kind: A1
- Application number: 10/699,884
- Filed: 2003-11-04
- Published: 2004-05-20
- Earliest claimed: 1999-07-01
- Assignees: Sollac
- Inventors: Mohamed Bouzekri
- Web page: https://patentgrep.com/patent/US20040094247A1

## CPC

- C21D 8/0468: {between cold rolling steps}
- C21D 9/48: deep-drawing sheets
- C21D 8/0436: {Cold rolling}
- C21D 8/0473: {Final recrystallisation annealing}
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)

## Abstract

A process is provided for preparation of an aluminum-killed medium-carbon steel sheet containing by weight from 0.040 to 0.080% of carbon, from 0.35 to 0.50% of manganese, from 0.040 to 0.070% of aluminum, from 0.004 to 0.006% of nitrogen, the remainder being iron and the inevitable trace impurities, wherein the steel contains carbon in free state, a grain count per mm2 greater than 20000 and, in the aged condition, has a percentage elongation A % satisfying the relationship: (640−Rm)/10≦A%≦(700−Rm)/11 where Rm is the maximum rupture strength.

## Claims

### Claim 1

A process for manufacturing an aluminum-killed medium-carbon steel strip comprising:
supplying a hot-rolled steel strip comprising by weight from 0.040 to 0.080% of carbon, from 0.35 to 0.50% of manganese, from 0.040% to 0.070 of aluminum, from 0.0035 to 0.0060% of nitrogen, and the remainder being iron and trace impurities,
passing the strip through a first cold-rolling, and
annealing the cold-rolled strip;
wherein the annealing step is a continuous annealing using a cycle comprising a temperature rise up to a first temperature higher than an onset temperature of pearlitic transformation Ac1, holding the strip above the first temperature for a duration of longer than 10 seconds, and rapidly cooling the strip to a second temperature of below 350° C. at a cooling rate in excess of 100° C. per second.

### Claim 2 (depends on 1)

The process according to claim 1, wherein the process further comprises performing a secondary cold-rolling after said annealing step.

### Claim 3 (depends on 1)

The process according to claim 1, wherein the strip is maintained during annealing at said first temperature of from 720° C. to 800° C. for a duration ranging from 10 seconds to 2 minutes.

### Claim 4 (depends on 1)

The process according to claim 1, wherein the cooling rate is from 100° C. to 500° C. per second.

### Claim 5 (depends on 1)

The process according to claim 1, wherein the strip is cooled to room temperature and the cooling rate is in excess of 100° C. per second.

### Claim 6 (depends on 1)

The process according to claim 1, wherein the annealing step is a continuous annealing using a cycle comprising:
a temperature rise up to a first temperature higher than an onset temperature of pearlitic transformation Ac1,
holding the strip above said first temperature for a duration of longer than 10 seconds,
rapidly cooling the strip to a second temperature of below 100° C. at a cooling rate in excess of 100° C. per second,
thermally treating the strip at low temperature ranging from 100° C. to 300° C. for a duration in excess of 10 seconds, and
cooling to room temperature.

### Claim 7

An aluminum-killed medium-carbon steel sheet, comprising, by weight, from 0.040 to 0.080% of carbon, from 0.35 to 0.50% of manganese, from 0.040 to 0.070% of aluminum, from 0.0035 to 0.0060% of nitrogen, with the remainder being iron and trace impurities, wherein the steel sheet has an aged condition percentage elongation A % satisfying the relationship:
(640−Rm)/10≦A%≦(700−Rm)/11
where Rm is a maximum rupture strength of the steel, expressed in MPa.

### Claim 8 (depends on 7)

A steel sheet according to claim 7, wherein the steel contains carbon in free state and/or some carbides precipitated at low temperature, and has a grain count per mm2 greater than 20000.

### Claim 9

A container comprising an aluminum-killed medium-carbon steel sheet formed into the container shape, comprising, by weight, from 0.040 to 0.080% of carbon, from 0.35 to 0.50% of manganese, from 0.040 to 0.070% of aluminum, from 0.0035 to 0.0060% of nitrogen, with the remainder being iron and trace impurities, wherein the steel sheet has an aged condition percentage elongation A % satisfying the relationship:
(640−Rm)/10≦A%≦(700−Rm)/11
where Rm is a maximum rupture strength of the steel, expressed in MPa.

### Claim 10 (depends on 9)

The container according to claim 9, wherein the steel steel contains carbon in free state and/or some carbides precipitated at low temperature, and has a grain count per mm2 greater than 20000.