# US 2004/0082676 A1 · Method for mixing blowing agents with polyurethane reagents for the production of polyurethane foam boards

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0082676 A1
- Document ID: US20040082676A1
- Status: Published application
- Kind: A1
- Application number: 10/468,487
- Filed: 2003-08-19
- Published: 2004-04-29
- Earliest claimed: 2003-08-19
- Inventors: Bruce F. Douglas; John B. Letts
- Web page: https://patentgrep.com/patent/US20040082676A1

## CPC

- C08G 18/4208: {containing aromatic groups}
- B29C 44/3442: {Mixing, kneading or conveying the foamable material (mixing plastics B29B7/00; mixing in general B01F)}
- C08G 2110/0025: rigid
- C08G 2110/005: < 50kg/m3
- C08G 2115/02: to isocyanurate groups
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)

## Abstract

A method for manufacturing polyurethane and polyisocyanurate foams comprising the steps of charging at least one blowing agent and a polyol component to an in-line continuous mixer, wherein the at least one blowing agent and the polyol component are continuously charged in separate streams advanced at predetermined flow rates chosen to bring about a desired ratio of blowing agent to polyol component within the in-line continuous mixer.

## Claims

### Claim 1

A method for manufacturing polyurethane and polyisocyanurate foams comprising the steps of:
charging at least one blowing agent and a polyol component to an in-line continuous mixer at a pressure of less than about 3,400 kPa, wherein the at least one blowing agent and the polyol component are continuously charged in separate streams advanced at predetermined flow rates chosen to bring about a desired ratio of blowing agent to polyol component within the in-line continuous mixer;
mixing the at least one blowing agent and the polyol component in the in-line continuous mixer to dissolve or emulsify the blowing agent in the polyol component and thereby provide a B-side stream of polyurethane reagents;
contacting the B-side stream of polyurethane reagents with an isocyanate component at a dispensing head to provide a foam formulation; and
dispensing the foam formulation from the dispensing head, wherein the residence time of the B-side stream of polyurethane reagents, from its exit from the in-line continuous mixer to its exit from the dispensing head as part of the foam formulation, is less than about 5 minutes.

### Claim 2

A method for manufacturing polyurethane and polyisocyanurate foams comprising the steps of:
charging at least one blowing agent and a polyol component to an in-line continuous mixer, wherein the at least one blowing agent and the polyol component are continuously charged in separate streams advanced at predetermined flow rates chosen to bring about a desired ratio of blowing agent to polyol component within the in-line continuous mixer.

### Claim 3

A method for manufacturing polyurethane and polyisocyanurate foams comprising the steps of:
charging at least one blowing agent and a polyol component to an in-line continuous mixer, at a pressure of less than about 3,400 kPa, to form a B-side stream of polyurethane reagents;
contacting the B-side stream of polyurethane reagents with an isocyanate component at a dispensing head to provide a foam formulation; and
dispensing the foam formulation from the dispensing head, wherein the residence time of the B-side stream of polyurethane reagents, from its exit from the in-line continuous mixer to its exit from the dispensing head as part of the foam formulation, is less than about 5 minutes.

### Claim 4 (depends on 2)

The method of claim 2, further comprising the steps of mixing the at least one blowing agent and the polyol component in the in-line continuous mixer to dissolve or emulsify the blowing agent in the polyol component and thereby provide a B-side stream of polyurethane reagents;
contacting the B-side stream of polyurethane reagents with an isocyanate component at a dispensing head to provide a foam formulation; and
dispensing the foam formulation from the dispensing head.

### Claim 5 (depends on 1, 2)

The method of claim 1, 2 , or 3, wherein the in-line continuous mixer is selected form the group consisting of dynamic mixer and static mixers.

### Claim 6 (depends on 5)

The method of claim 5, wherein the in-line continuous mixer is a dynamic mixer selected from the group consisting of pin-impeller mixers, turbine mixers, double helix mixers, and radial axial mixers.

### Claim 7 (depends on 1, 2, 3, 5)

The method of claim 1, 2, 3, 5, or 6, where in volume of the in-line continuous mixer is from about 1 to about 40 liters.

### Claim 8 (depends on 1, 3)

The method of claim 1, 3, or 4, wherein the residence time of the B-side stream, from its exit from the in-line continuous mixer to its exit from the dispensing head as part of the foam formulation, is less than about one minute.

### Claim 9 (depends on 8)

The method of claim 8, wherein the residence time of the B-side stream, from its exit from the in-line continuous mixer to its exit from the dispensing head as part of the foam formulation, is less than about thirty seconds.

### Claim 10 (depends on 1, 2)

The method of claim 1, 2, or 3, wherein, in said step of charging the at least one blowing agent and the polyol component to the in-line continuous mixer occurs at a pressure of less than about 500 kPa.