# US 2004/0082471 A1 · Method of preparation of non-pyrophoric copper-alumina catalysts

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0082471 A1
- Document ID: US20040082471A1
- Status: Published application
- Kind: A1
- Application number: 10/281,635
- Filed: 2002-10-28
- Published: 2004-04-29
- Earliest claimed: 2002-10-28
- Assignees: Engelhard Corporation
- Inventors: Oleg M. Ilinich; Wolfgang F. Ruettinger; Ronald T. Mentz; Robert J. Farrauto
- Web page: https://patentgrep.com/patent/US20040082471A1

## CPC

- H01M 8/0662: Treatment of gaseous reactants or gaseous residues, e.g. cleaning
- B01J 21/04: Alumina
- B01J 23/005: {Spinels}
- B01J 23/72: Copper
- B01J 23/94: of catalysts comprising metals, oxides or hydroxides of the iron group metals or copper
- B01J 37/0018: {Addition of a binding agent or of material, later completely removed among others as result of heat treatment, leaching or washing,(e.g. forming of pores; protective layer, desintegrating by heat)}
- B01J 37/14: with gases containing free oxygen
- B01J 37/18: with gases containing free hydrogen
- C01B 3/16: using catalysts
- H01M 8/0612: from carbon-containing material
- C01B 2203/0283: containing a CO-shift step, i.e. a water gas shift step
- C01B 2203/1076: Copper or zinc-based catalysts
- H01M 8/0668: Removal of carbon monoxide or carbon dioxide
- H01M 8/0675: {Removal of sulfur}
- Y02E 60/50: Fuel cells
- Y02P 20/52: using catalysts, e.g. selective catalysts
- Y02P 20/584: Recycling of catalysts
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Provided is a process for preparing a non-pyrophoric catalyst having about 2 to 20 wt. % of a copper component, wherein at least 50 wt. % of the copper component is in the form of a copper oxide, aluminum oxide-spinel. The catalyst can be prepared by forming a mixture of a copper precursor and an alumina precursor, coextruding the mixture, drying the coextrudate and calcining the dried coextrudate at a temperature of at least 600° C. In other aspects, the invention also relates to processes for the activation of copper-based catalysts and for the regeneration of deactivated copper-based catalysts.

## Claims

### Claim 1

A process for preparing a non-pyrophoric catalyst, comprising:
forming a mixture of a copper precursor and an alumina precursor;
coextruding the mixture;
drying the coextrudate; and
calcining the dried coextrudate at a temperature of at least 600° C. to form the non-pyrophoric catalyst;
wherein the non-pyrophoric catalyst comprises about 2 to 20 wt. % of a copper component, and at least 50 wt. % of the copper component is in the form of a copper oxide, aluminum oxide-spinel.

### Claim 2 (depends on 1)

The process of claim 1, wherein the non-pyrophoric catalyst comprises at least 80 wt. % of alumina.

### Claim 3 (depends on 1)

The process of claim 1, wherein the calcination temperature is at least 650° C.

### Claim 4 (depends on 1)

The process of claim 1, wherein the formation of the mixture comprises mulling a paste of a water-soluble copper salt and hydrated alumina in an aqueous solution.

### Claim 5 (depends on 1)

The process of claim 1, wherein the process further comprises activating the non-pyrophoric catalyst with a reducing gas stream comprising a reductant component and an inert gas at a temperature of about 150 to 300° C.

### Claim 6 (depends on 5)

The process of claim 5, wherein the reductant component comprises hydrogen, carbon monoxide or a combination thereof.

### Claim 7 (depends on 5)

The process of claim 5, wherein the reducing gas stream is substantially dry.

### Claim 8 (depends on 5)

The process of claim 5, wherein the process further comprises passivating the non-pyrophoric catalyst with a gas stream comprising oxygen and an inert gas at a temperature below 50° C.

### Claim 9 (depends on 8)

The process of claim 8, wherein the gas stream comprising oxygen and the inert gas is substantially dry.

### Claim 10

A process for activating a non-pyrophoric catalyst, comprising:
(a) contacting the non-pyrophoric catalyst with a reducing gas stream comprising a reductant component and an inert gas at a temperature of about 150 to 300° C.; and
(b) passivating the reduced non-pyrophoric catalyst with a gas stream comprising oxygen and an inert gas at a temperature below 50° C.;
wherein the non-pyrophoric catalyst comprises about 2 to 20 wt. % of a copper component, and at least 50 wt. % of the copper component is in the form of a copper oxide, aluminum oxide-spinel.

### Claim 11 (depends on 10)

The process of claim 10, wherein the reductant component of (a) comprises hydrogen, carbon monoxide or a combination thereof.

### Claim 12 (depends on 10)

The process of claim 10, wherein the reducing gas stream of (a) is substantially dry.

### Claim 13 (depends on 10)

The process of claim 10, wherein the gas stream of (b) is substantially dry.

### Claim 14

A process for regenerating a deactivated copper-based catalyst, comprising:
(a) contacting the deactivated catalyst with a gas stream comprising oxygen, and wherein hydrogen is substantially absent from the gas stream, at catalyst bed temperatures of about 200 to 800° C.; and
(b) reducing the heated, deactivated copper-based catalyst with a reducing gas stream.

### Claim 15 (depends on 14)

The process of claim 14, wherein the gas stream of (a) comprises about 3 to 21% by volume oxygen.

### Claim 16 (depends on 14)

The process of claim 14, wherein the gas stream of (a) is substantially dry.

### Claim 17 (depends on 14)

The process of claim 14, wherein the step (a) is conducted at catalyst bed temperatures of 300 to 700° C.

### Claim 18 (depends on 14)

The process of claim 14, wherein the reducing gas stream of (b) is substantially dry.

### Claim 19 (depends on 14)

The process of claim 14, wherein the reduction of (b) is conducted at about 150 to 300° C.

### Claim 20

A process for regenerating a deactivated catalyst, the process comprising:
(a) contacting the deactivated catalyst with a gas stream comprising oxygen, and wherein hydrogen is substantially absent from the gas stream, at catalyst bed temperatures of about 200 to 800° C.; and
(b) reducing the heated, deactivated catalyst with a reducing gas stream;
wherein the deactivated catalyst comprises about 2-20 wt. % of a copper component and alumina, wherein at least 50% of the copper component is in the form of a copper oxide, aluminum oxide-spinel.

### Claim 21 (depends on 20)

The process of claim 20, wherein the gas stream of (a) comprises about 3 to 21% by volume oxygen.

### Claim 22 (depends on 20)

The process of claim 20, wherein the gas stream of (a) is substantially dry.

### Claim 23 (depends on 20)

The process of claim 20, wherein step (a) is conducted at catalyst bed temperatures of 300 to 700° C.

### Claim 24 (depends on 20)

The process of claim 20, wherein the reducing gas stream of (b) is substantially dry.

### Claim 25 (depends on 20)

The process of claim 20, wherein the reduction of (b) is conducted at about 150 to 300° C.