# US 2004/0082467 A1 · Silicon-containing alumina support, a process for preparing the support and a catalyst containing the support

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0082467 A1
- Document ID: US20040082467A1
- Status: Published application
- Kind: A1
- Application number: 10/682,221
- Filed: 2003-10-09
- Published: 2004-04-29
- Earliest claimed: 2002-10-10
- Assignees: China Petroleum & Chemical Corporation; Fushun Research Institute of Petroleum and Petrochemicals, Sinopec
- Inventors: Dengling Wei; Shaozhong Peng
- Web page: https://patentgrep.com/patent/US20040082467A1

## CPC

- C10G 45/08: in combination with chromium, molybdenum, or tungsten metals, or compounds thereof
- B01J 21/12: Silica and alumina
- B01J 23/85: Chromium, molybdenum or tungsten
- B01J 27/182: with silicon
- B01J 27/188: with chromium, molybdenum, tungsten or polonium
- B01J 35/19: {Catalysts containing parts with different compositions}
- B01J 37/0009: {Use of binding agents; Moulding; Pressing; Powdering; Granulating; Addition of materials ameliorating the mechanical properties of the product catalyst}
- B01J 23/883: and nickel
- B01J 35/615: {100-500 m2/g}
- B01J 35/633: {less than 0.5 ml/g}
- B01J 35/635: {0.5-1.0 ml/g}
- B01J 35/66: Pore distribution
- C10G: CRACKING HYDROCARBON OILS; PRODUCTION OF LIQUID HYDROCARBON MIXTURES, e.g. BY DESTRUCTIVE HYDROGENATION, OLIGOMERISATION, POLYMERISATION (cracking to hydrogen or synthesis gas C01B; cracking or pyrolysis of hydrocarbon gases to individual hydrocarbons or mixtures thereof of definite or specified constitution C07C; cracking to cokes C10B); RECOVERY OF HYDROCARBON OILS FROM OIL-SHALE, OIL-SAND, OR GASES; REFINING MIXTURES MAINLY CONSISTING OF HYDROCARBONS; REFORMING OF NAPHTHA; MINERAL WAXES
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS

## Abstract

A silicon-containing alumina support, a process for preparing the support, and a catalyst containing the support are provided. The alumina support includes an additive silicon enriched on its surface, with the difference between the atomic ratio of silicon to aluminum on the surface of alumina support and that of the alumina support is at least 0.10. The process for preparing the silicon-containing alumina support comprises adding a nanometer silicon compound. The inventive alumina support can be used in manufacturing a catalyst for hydrotreating hydrocarbons with good physico-chemical properties and performance.

## Claims

### Claim 1

A silicon-containing alumina support comprising 0.5 to 10.0 weight percent of silica, wherein the difference between the atomic ratio of silicon to aluminum on the surface of alumina support and the average atomic ratio of silicon to aluminum of the alumina support is at least 0.10.

### Claim 2 (depends on 1)

The alumina support of claim 1 wherein the difference between the atomic ratio of silicon to aluminum on the surface of the alumina support and the average atomic ratio of silicon to aluminum of the alumina support is 0.10 to 0.25.

### Claim 3 (depends on 1)

The alumina support of claim 1 wherein the difference between the atomic ratio of silicon to aluminum on the surface of alumina support and the average atomic ratio of silicon to aluminum of the alumina support is 0.12 to 0.20.

### Claim 4 (depends on 1)

The alumina support of claim 1 wherein the alumina support comprises 1.0 to 7.0 weight percent of silica.

### Claim 5 (depends on 1)

The alumina support of claim 1 wherein the atomic ratio of silicon to aluminum on the surface of the alumina support is at least 0.15.

### Claim 6 (depends on 5)

The alumina support of claim 5 wherein the atomic ratio of silicon to aluminum on the surface of the alumina support is 0.15 to 0.30.

### Claim 7 (depends on 1)

The alumina support of claim 1 wherein the alumina support has a specific surface area of 270-320 m2/g, and a pore volume of 0.55 to 0.68 ml/g, with the volume of the pores of a size between 3 to 15 nm constituting at least 90% of the total volume of the pores of the alumina support.

### Claim 8 (depends on 7)

The alumina support of claim 7 wherein the volume of the pores of a size between 3 to 15 nm constitutes 90 to 96% of the total volume of the pores of the alumina support.

### Claim 9

A process for preparing a silicon-containing alumina support comprising:
mixing and/or kneading aluminum hydroxide or alumina, while adding a nanometer silicon compound; adding a peptizing acid and mixing all the materials to form a plastic mass; moulding the mass, drying it and calcining it, so as to provide a silicon-containing alumina support, the nanometer silicon compound being added in such an amount that the alumina support contains 0.5 to 40.0 weight percent of silica.

### Claim 10 (depends on 9)

The process of claim 9 wherein the nanometer silicon compound is nanometer silica with a particle diameter of 6-100 nm.

### Claim 11 (depends on 9)

The process of claim 9 wherein the alumina support comprises 0.5 to 10% by weight of silica.

### Claim 12 (depends on 9)

The process of claim 9 wherein the aluminum hydroxide is a phosphorus-containing aluminum hydroxide containing 0.3 to 3.0% by weight of phosphorus pentoxide; the phosphorus-containing aluminum hydroxide is prepared by slurrying aluminum hydroxide precipitate; adding thereto a phosphorus compound; maintaining the slurry at a temperature between 30 to 90° C.; filtering, drying the slurry and calcining the dried slurry to obtain the phosphorus-containing aluminum hydroxide.

### Claim 13 (depends on 9)

The process of claim 9 wherein the nanometer silicon compound is added by one of the following methods:
(a) mixing the nanometer silicon compound with the starting material containing aluminum;
(b) wetting the nanometer silicon compound with deionized water and then adding the wetted compound to the starting material containing aluminum;
(c) mixing the nanometer silicon compound with a peptizing acid solution to give a mixture, and adding the mixture to the starting material containing aluminum;
(d) mixing the whole or a portion of the small-pore aluminum hydroxide, a peptizing acid solution and the nanometer silicon compound to give a peptizing agent, and mixing the peptizing agent with large-pore aluminum hydroxide; and
(e) adding the nanometer silicon compound portionwise in at least two steps of steps (a), (b), (c), and (d).

### Claim 14 (depends on 13)

The process of claim 13 wherein the large-pore aluminum hydroxide has a pore volume of 0.7 to 1.1 ml/g, an average pore size of 6.0 to 11.0 nm, and a specific surface area of 300 to 380 m2/g; the small-pore aluminum hydroxide has a pore volume of 0.2 to 0.6 ml/g, an average pore size of 2.0 to 10.0 nm, and a specific surface area of 200 to 300 m2/g; the mixing ratio by weight of the large-pore aluminum hydroxide to the small-pore aluminum hydroxide is 1:1 to 1:5; the ratio between the total weight of the large-pore aluminum hydroxide and the small-pore aluminum hydroxide used for mixing on the one hand and that of the large-pore aluminum hydroxide and the small-pore aluminum hydroxide used for preparing peptizing agent on the other hand is 5:1 to 25:1.

### Claim 15 (depends on 9)

The process of claim 9 wherein the drying step is carried out at 90-150° C. for 8 to 16 hours, and the calcining step is carried out at 450 to 650° C. for 1-6 hours.

### Claim 16 (depends on 9)

The process of claim 9 wherein one or more additives selected from the group consisting of titanium, born, zirconium and phosphorus are introduced into the alumina support by mixing alumina or pseudo-boehmite and a nanometer additive source selected from the group consisting of nanometer titanium-containing compound, nanometer boron-containing compound, nanometer zirconium-containing compound, and nanometer phosphorus-containing compound.

### Claim 17 (depends on 1)

Use of the alumina support of claim 1 in the manufacture of a catalyst.

### Claim 18 (depends on 17)

The use of claim 17 wherein the catalyst is used for for hydrotreating hydrocarbons.

### Claim 19 (depends on 1)

A catalyst for hydrotreating hydrocarbons comprising the silicon-containing alumina support of claim 1, and a metal from Group VIB and a metal from Group VIII of the Periodic Table of Elements as active components.

### Claim 20 (depends on 19)

The catalyst of claim 19 wherein the catalyst comprises 0.3 to 7.0 weight percent of silica, and the catalyst has an atomic ratio of silicon to aluminum on the surface of at least 0.15, a pore volume of 0.30 to 0.40 ml/g, with the volume of the pores of a size between 3 to 15 nm constituting at least 90% of the total volume of the pores of the catalyst.

### Claim 21 (depends on 20)

The catalyst of claim 20 wherein the catalyst has an atomic ratio of silicon to aluminum on the surface of 0.15-0.25.

### Claim 22 (depends on 20)

The catalyst of claim 20 wherein the difference between the atomic ratio of silicon to aluminum on the surface of the catalyst and the average atomic ratio of silicon to aluminum of the catalyst is 0.10 to 0.20.

### Claim 23 (depends on 19)

The catalyst of claim 19 wherein the catalyst further comprises phosphorus.

### Claim 24 (depends on 19)

The catalyst of claim 19 wherein the metal from Group VIB is 18.0 to 28.0 weight percent of the oxide of tungsten and/or molybdenum; the metal from Group VIII is 2.0 to 6.0 weight percent of the oxide of nickel and/or cobalt; and the catalyst comprises 0.5 to 8.0 weight percent of phosphorus pentoxide.

### Claim 25 (depends on 19)

The catalyst of claim 19 wherein the catalyst has a specific surface area of 150 to 200 m2/g, a pore volume of 0.32 to 0.38 ml/g, with the volume of the pores of a size between 3 to 15 nm constituting at least 92 to 96% of the total volume of pores of the catalyst.