# US 2004/0082274 A1 · Polishing slurry used for copper chemical mechanical polishing (CMP) process

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0082274 A1
- Document ID: US20040082274A1
- Status: Published application
- Kind: A1
- Application number: 10/279,351
- Filed: 2002-10-24
- Published: 2004-04-29
- Earliest claimed: 2002-10-24
- Inventors: Yaojian Leng
- Web page: https://patentgrep.com/patent/US20040082274A1

## CPC

- C09G 1/02: containing abrasives or grinding agents {(abrasives as such C09K3/14; polishing of semi-conductors H10P52/40)}
- H10P 52/403: {of conductive or resistive materials}
- C09G: POLISHING COMPOSITIONS (French polish C09F11/00); SKI WAXES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A polishing slurry for the chemical-mechanical polishing (CMP) process used in the integrated circuit manufacture process is disclosed. The slurry of the present invention may comprise colloid silica (SiO2) as abrasive particles, and a corrosion inhibitor (e.g., benzotriazole (BTA)). The slurry does not require any oxidizing agent. The slurry may be used as a barrier slurry in copper CMP processes; and it has a similar polishing rate for copper, barrier, and dielectric materials on patterned wafers. The slurry of the present invention also reduces CMP defectivity on polished wafers.

## Claims

### Claim 1

A polishing slurry comprising:
a dispersing medium;
a colloidal silicon suspended in the dispersing medium; and
a corrosion inhibitor in the dispersing medium.

### Claim 2 (depends on 1)

The polishing slurry of claim 1 wherein the slurry does not contain an oxidizing agent.

### Claim 3 (depends on 1)

The polishing slurry of claim 1 wherein the ratio of colloidal silica to corrosion inhibitor is adjustable to a desired selectivity.

### Claim 4 (depends on 1)

The polishing slurry of claim 1 wherein slurry is a pre-blended or on-platen point-of-use mix.

### Claim 5 (depends on 1)

The polishing slurry of claim 1 wherein surfactant is added to the slurry.

### Claim 6 (depends on 1)

The polishing slurry of claim 1 wherein the slurry may be aged before polish.

### Claim 7 (depends on 1)

The polishing slurry of claim 1 wherein the corrosion inhibitor comprises benzotriazole.

### Claim 8 (depends on 1)

The polishing slurry of claim 1, comprising about 0.005 to 0.2% by weight of BTA and about 1 to 30% by weight of SiO2.

### Claim 9

A method of polishing a damascene structure using a chemical-mechanical polishing apparatus, comprising the steps of:
providing a damascene structure;
providing a polishing pad;
applying a polishing slurry to the interface between the damascene structure and the polishing pad; and
performing polishing using polishing parameters of the CMP apparatus, wherein at least a portion of the metal layer is removed.

### Claim 10 (depends on 9)

The method of claim 9, wherein the slurry comprises colloidal silicon and corrosion inhibitors.

### Claim 11 (depends on 9)

The method of claim 9 wherein the slurry does not contain an oxidizing agent.

### Claim 12 (depends on 9)

The method of claim 9 wherein the ratio of colloidal silica to corrosion inhibitor in the slurry is adjustable to a desired selectivity.

### Claim 13 (depends on 9)

The method of claim 9 wherein the slurry can be pre-blended or on-platen point-of-use mixed.

### Claim 14 (depends on 9)

The method of claim 9 wherein surfactant is added to the slurry.

### Claim 15 (depends on 9)

The method of claim 9 wherein the slurry may be aged before polish.

### Claim 16 (depends on 9)

The method of claim 9 wherein the corrosion inhibitor comprises benzotriazole.

### Claim 17 (depends on 9)

The method of claim 9, wherein the slurry contains about 0.005 to 0.2% by weight of BTA and about 1 to 30% by weight of SiO2.