# US 2004/0082200 A1 · Method for forming a silicon nitride layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0082200 A1
- Document ID: US20040082200A1
- Status: Published application
- Kind: A1
- Application number: 10/620,518
- Filed: 2003-07-16
- Published: 2004-04-29
- Earliest claimed: 2002-10-25
- Assignees: Nanya Technology Corporation
- Inventors: Shian-Jyh Lin; Hai-Han Hung; Chung-Yuan Lee
- Web page: https://patentgrep.com/patent/US20040082200A1

## CPC

- H10P 14/6316: {Formation by nitridation, e.g. nitridation of the substrate}
- C23C 14/0652: {Silicon nitride}
- C23C 14/48: Ion implantation
- H10D 1/047: {of conductor-insulator-semiconductor capacitors, e.g. trench capacitors}
- H10P 30/204: {into Group IV semiconductors}
- H10P 30/208: {of electrically inactive species}
- H10P 14/6927: {the material being a silicon oxynitride, e.g. SiON or SiON:H}
- H10P 14/69433: {the material being a silicon nitride not containing oxygen, e.g. SixNy or SixByNz}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A method of forming a silicon nitride layer. The method comprises providing a substrate having a silicon surface thereon, performing an ion implant process on the silicon surface, implanting nitrogen atoms into the silicon surface, and performing a thermal nitridation process and forming a silicon nitride layer on the substrate, wherein the silicon nitride layer comprises the silicon nitride formed on the silicon surface by reaction of the silicon surface with the nitrogen atoms contained therein.

## Claims

### Claim 1

A method of forming a silicon nitride layer, comprising:
providing a substrate having a silicon surface thereon;
performing an ion implant process on the silicon surface, implanting nitrogen atoms into the silicon surface; and
performing a thermal nitridation process, forming a silicon nitride layer on the substrate, wherein the silicon nitride layer comprises the silicon nitride formed on the silicon surface by reaction of the silicon surface with the nitrogen atoms therein.

### Claim 2 (depends on 1)

The method as claimed in claim 1, wherein the silicon nitride layer further comprises the silicon nitride formed by reaction of the silicon surface with a nitrogen-containing gas in the thermal nitridation process.

### Claim 3 (depends on 1)

The method as claimed in claim 1, wherein the substrate is silicon substrate.

### Claim 4 (depends on 1)

The method as claimed in claim 1, wherein the silicon surface is a plane silicon surface of a silicon surface within an opening.

### Claim 5 (depends on 1)

The method as claimed in claim 1, wherein the source gas for the ion implant process is nitrogen gas (N2).

### Claim 6 (depends on 1)

The method as claimed in claim 1, wherein the implant energy for the ion implant process is between 200 eV and 200 KeV.

### Claim 7 (depends on 1)

The method as claimed in claim 1, wherein the implant dosage for the ion implant process is between 1*1014 atoms/cm2 and 5*1017 atoms/cm2.

### Claim 8 (depends on 1)

The method as claimed in claim 1, wherein the thermal nitridation process is a furnace nitridation process or a rapid thermal nitridation (RTN) process.

### Claim 9 (depends on 1)

The method as claimed in claim 1, wherein the process temperature for the thermal nitridation process is between 500° C. and 1200° C.

### Claim 10 (depends on 1)

The method as claimed in claim 1, wherein the process gas for the thermal nitridation process is NH3, N2, N2O or NO.

### Claim 11

A method of forming a silicon nitride layer for a bottle-shaped trench process, comprising:
providing a silicon substrate;
forming a trench in the silicon substrate;
conformally depositing a dielectric layer in the trench;
selectively etching the dielectric layer, exposing an upper region in the trench and sidewalls thereof, leaving a lower region in the trench covered by the remaining dielectric layer;
performing an ion implant process, implanting nitrogen atoms into the silicon substrate adjacent to the sidewalls;
performing a thermal nitridation process, forming a silicon nitride layer on the surface of the sidewalls, wherein the silicon nitride layer includes the silicon nitride formed on the silicon surface by reaction of the silicon surface with the nitrogen atoms therein;
removing the remaining dielectric layer from the lower region of the trench; and
using the silicon nitride layer as an etching mask, etching the silicon substrate in the lower region, forming an expanded region therein, and forming a bottle-shaped trench consisting of the trench portion in the upper region and the expanded region in the lower portion.

### Claim 12 (depends on 11)

The method as claimed in claim 11, wherein the silicon nitride layer further comprises the silicon nitride formed by reaction of the silicon surface with a nitrogen-containing gas in the thermal nitridation process.

### Claim 13 (depends on 11)

The method as claimed in claim 11, wherein the dielectric layer is silicon dioxide.

### Claim 14 (depends on 11)

The method as claimed in claim 11, wherein the method for depositing the dielectric layer is LPCVD or liquid phase deposition (LPD).

### Claim 15 (depends on 1, 11)

The method as claimed in claim 11, wherein the method as claimed in claim 1, wherein the source gas for the ion implant process is nitrogen (N2).

### Claim 16 (depends on 11)

The method as claimed in claim 11, wherein the implant energy for the ion implant process is between 200 eV and 200 KeV.

### Claim 17 (depends on 11)

The method as claimed in claim 11, wherein the implant dosage for the ion implant process is between 1*1014 atoms/cm2 and 5*1017 atoms/cm2.

### Claim 18 (depends on 11)

The method as claimed in claim 11, wherein the thermal nitridation process is a furnace nitridation process or a rapid thermal nitridation (RTN) process.

### Claim 19 (depends on 11)

The method as claimed in claim 11, wherein the process temperature of the thermal nitridation process is between 500° C. and 1200° C.

### Claim 20 (depends on 11)

The method as claimed in claim 11, wherein the etching method for forming the expanded region is wet etching.

### Claim 21 (depends on 11)

The method as claimed in claim 11, wherein the expanded region is wider than the trench in the upper region.

### Claim 22 (depends on 11)

The method as claimed in claim 11, wherein the process gas for the thermal nitridation process is NH3 N2, N2O or NO.