# US 2004/0082177 A1 · Method of forming isolation films in semiconductor devices

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0082177 A1
- Document ID: US20040082177A1
- Status: Published application
- Kind: A1
- Application number: 10/622,532
- Filed: 2003-07-18
- Published: 2004-04-29
- Earliest claimed: 2002-10-28
- Assignees: Hynix Semiconductor Inc.
- Inventors: Won Kwon Lee
- Web page: https://patentgrep.com/patent/US20040082177A1

## CPC

- H10P 50/692: {characterised by their composition, e.g. multilayer masks or materials}
- H10P 50/242: {of Group IV materials}
- H10P 50/695: {characterised by the process involved to create the mask, e.g. lift-off masks or sidewalls or to modify the mask}
- H10P 95/062: {involving a dielectric removal step}
- H10W 10/0145: {of trenches having shapes other than rectangular or V-shape (H10W10/0143 takes precedence)}
- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

Disclosed is a method of forming the isolation film in the semiconductor device which can prevent concentration of an electric field by forming a dual slant angle at the top corner of the trench in the course of forming the trench. After a photoresist pattern containing silicon components or an amorphous silicon film is formed on a pad oxide film instead of a pad nitride film, the surface of the photoresist pattern or the amorphous silicon film is oxidized so that the oxidized portion is fused with the isolation film. Accordingly, it is possible to prevent generation of a moat in the course of removing the photoresist pattern and the pad oxide film after the trench is buried with an insulating material. Therefore, the disclosed method can improve reliability of the process and an electrical characteristic of the resulting device.

## Claims

### Claim 1

A method of forming an isolation film in a semiconductor device, comprising:
forming a stack structure of a pad oxide film and a photoresist which an isolation region is defined pattern on a semiconductor substrate, the isolation region having one or more corners and a central portion, the photresist pattern containing silicon;
implementing an over etch so that polymer is formed at the corners of the isolation region to form an etch slant face at one or more corners of the isolation region while etching the semiconductor substrate at the central portion of the isolation region;
forming a trench at the central portion of the isolation region;
oxidizing a surface of the photoresist pattern to form a surface oxide film;
forming an insulating material layer on the entire structure to bury the trench; and
implementing a polishing process until the photoresist pattern has a given thickness and then removing the photoresist pattern and the pad oxide film.

### Claim 2 (depends on 1)

The method as claimed in claim 1, wherein the amount of silicon contained in the photoresist pattern is in the range of from about 7 to about 50%.

### Claim 3 (depends on 1)

The method as claimed in claim 1, wherein the over etch process uses a CHF3 gas, a CF4 gas or a mixture thereof as an etch gas to etch the central portion of the isolation region in depth an amount ranging from about 50 to about 400 Å.

### Claim 4 (depends on 3)

The method as claimed in claim 3, wherein a supply flow of CHF3 is from about 50 to about 70 sccm, the supply flow of CF4 is from about 30 to about 50 sccm and an Ar gas flow of from about 1000 to about 2000 sccm is supplied as a carrier gas.

### Claim 5 (depends on 1)

The method as claimed in claim 1, wherein the over etch process is implemented for a time period from about 5 to about 30 seconds with a pressure of from about 500 to about 2500 mTorr and a power of from about 600 to about 2000 W is applied.

### Claim 6 (depends on 1)

The method as claimed in claim 1, wherein a width of the etch slant face is from about 0.02 μm to about 0.07 μm and a tilt angle of the sidewall of the etch slant face is from about 20 to about 50°.

### Claim 7 (depends on 1)

The method as claimed in claim 1, wherein the surface oxide film is formed by means of an O2 plasma processing.

### Claim 8 (depends on 7)

The method as claimed in claim 7, wherein the O2 plasma processing is implemented at a temperature ranging from about 50 to about 200° C. by means of an O2 ashing process or an O2 ion implantation process.

### Claim 9 (depends on 1)

The method as claimed in claim 1, wherein the insulating material layer is formed using a low thermal oxide film at a temperature ranging from about 50 to about 300° C.

### Claim 10

A method of forming an isolation film in a semiconductor device, comprising the steps of:
forming a stack structure of a pad oxide film, an amorphous silicon layer, an anti-reflection film and a photoresist pattern on a semiconductor substrate which an isolation region is defined;
implementing an over etch so that polymer is formed at a corner of the isolation region to form an etch slant face at the corner of the isolation region while etching the semiconductor substrate at the central portion of the isolation region;
removing the photoresist pattern and the anti-reflection film;
oxidizing the surface of the amorphous silicon layer to form a surface oxide film;
forming an insulating material layer on the entire structure to bury a trench; and
implementing a polishing process until the insulating material layer is at a given thickness and then removing the amorphous silicon layer and the pad oxide film.

### Claim 11 (depends on 10)

The method as claimed in claim 10, wherein the over etch process uses a CHF3 gas, a CF4 gas or a mixed gas of them as an etch gas to etch a central portion of the isolation region in depth in an amount ranging from about 50 to about 400 Å.

### Claim 12 (depends on 10)

The method as claimed in claim 10, wherein the width of the etch slant face ranges from about 0.02 μm to about 0.07 μm and a tilt angle of the sidewall of the etch slant face ranges from about from 20 to about 50°.

### Claim 13 (depends on 10)

The method as claimed in claim 10, further comprising the step of before the surface of the amorphous silicon layer is oxidized after the anti-reflection film is removed, oxidizing the sidewall and bottom of the trench to form a surface oxide film at the sidewall and bottom of the trench.

### Claim 14 (depends on 10)

The method as claimed in claim 10, wherein the surface oxide film is formed by means of an O2 plasma processing.

### Claim 15 (depends on 14)

The method as claimed in claim 14, wherein the O2 plasma processing is implemented at a temperature ranging from about 50 to about 200° C. by means of an O2 ashing process or an O2 ion implantation process.

### Claim 16

A method of forming an isolation film in a semiconductor device, comprising the steps of:
stacking a pad oxide film, an amorphous silicon layer, an anti-reflection film and a photoresist pattern on a semiconductor substrate which an isolation region is defines;
implementing over etch so that polymer is formed at a corner of the isolation region to form an etch slant face at the corner of the isolation region while etching the semiconductor substrate at the central portion of the isolation region;
etching a part of the semiconductor substrate using the polymer film as an etch mask to form a trench;
burying the trench with an insulating film and then removing the polymer film and a hard mask film;
implementing an O2 plasma oxidization process to oxidizing the amorphous silicon film on the amorphous silicon film and at the sidewall of the insulating film, thus forming an oxide film;
etching the oxide film on the amorphous silicon film; and
etching the amorphous silicon film and the pad oxide film below the amorphous silicon film.

### Claim 17 (depends on 16)

The method as claimed in claim 16, wherein the O2 plasma oxidization process is implemented to oxidize a top and sidewall of the amorphous silicon film using a plasma ashing method and an O2 ion implantation method having a temperature ranging from about 50 to about 200° C.

### Claim 18 (depends on 16)

The method as claimed in claim 16, wherein the polymer film is formed by etching about 200 Å of the semiconductor substrate using a gas such as CF4 and CHF3.