# US 2004/0082176 A1 · Method of reworking structures incorporating low-k dielectric materials

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0082176 A1
- Document ID: US20040082176A1
- Status: Published application
- Kind: A1
- Application number: 10/280,513
- Filed: 2002-10-24
- Published: 2004-04-29
- Earliest claimed: 2002-10-24
- Assignees: Intenational Business Machines Corporation
- Inventors: Terence Lawrence Kane; Chung-Ping Eng; Brett H. Engel; Barry Jack Ginsberg; Dermott A. Macpherson; John Charles Petrus
- Web page: https://patentgrep.com/patent/US20040082176A1

## CPC

- H10P 72/0604: {Process monitoring, e.g. flow or thickness monitoring}
- G01N 21/68: using high frequency electric fields
- H01J 37/32009: {Arrangements for generation of plasma specially adapted for examination or treatment of objects, e.g. plasma sources (plasma generation in general H05H1/24)}
- H10P 50/262: {by physical means only}
- H10P 50/283: {by chemical means}
- H10P 50/286: {of organic materials}
- H10P 50/287: {by chemical means}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)

## Abstract

Low-k dielectric films such as SiLK are desirably used in semiconductor structures, for example in back-end multilevel metal interconnect structures, as insulators. Low-k dielectric films, however, are prone to damage in the course of typical rework processes such as chemical-mechanical polishing, plasma/reactive ion etching, or wet chemistry processing/etching. The present invention uses an ion milling process with a variable-position endpoint detector to unlayer multiple layers including low-k dielectric films. The ion milling process can be controlled for each material type so as to maintain a planar surface with minimal or no damage to the exposed materials. A different methodology describes unlayering individual die involving in each case mechanical polish of removal of the metal layer and metal interconnection combined with RIE or Plasma deprocessing steps.

## Claims

### Claim 1

A method of etching a semiconductor structure including a first layer of material overlaying a second layer of low-k dielectric film, comprising the steps of:
ion beam-milling said first layer of material; and
detecting, with an optical detector positioned in the ion beam adjacent said first layer of material, an endpoint of said first layer;
whereby to expose said second layer of low-k dielectric film.

### Claim 2 (depends on 1)

A method in accordance with claim 1 wherein said first layer is selected from the group comprising oxide, nitride, and metal.

### Claim 3 (depends on 1)

A method in accordance with claim 1 wherein said detecting step comprises transmitting detected light through an optical cable to a photospectrometer.

### Claim 4 (depends on 1)

A method in accordance with claim 1 and further including the steps of:
supporting said semiconductor structure on a liquid-cooled, movable platen; and
varying the temperature and position of said platen to facilitate said ion beam-milling step.

### Claim 5 (depends on 1)

A method in accordance with claim 1 wherein said step of detecting an endpoint includes detecting the presence of said second layer of low-k dielectric film.

### Claim 6 (depends on 1)

A method in accordance with claim 1, wherein said semiconductor structure includes a third layer of material underlying said second layer of low-k dielectric film; and further including the steps of
ion beam-milling said second layer of low-k dielectric film with Argon beams; and
detecting, with an optical detector position in the ion beam adjacent said second layer of material, an endpoint of said first layer.

### Claim 15

A system for delayering a semiconductor structure including a first layer of material overlaying a second layer of low-k dielectric film, comprising:
a processing chamber;
an ion beam milling source in said processing chamber for generating a beam of ions to mill said semiconductor structure;
a platen in said processing chamber for supporting said semiconductor structure in said beam of ions;
a crystal endpoint detector in said processing chamber;
a photospectrometer outside of said processing chamber;
means for connecting said sapphire crystal endpoint detector to said photospectrometer; and
means for positioning said sapphire crystal endpoint detector proximate said platen to monitor milling of said semiconductor structure.

### Claim 16 (depends on 15)

A system in accordance with claim 15 wherein said crystal endpoint detector comprises a sapphire crystal.

### Claim 17 (depends on 15)

A system in accordance with claim 15 and further including means for introducing a gas into said processing chamber.

### Claim 18 (depends on 15)

A system in accordance with claim 15 wherein said ion beam milling source comprises an Argon ion beam milling source.

### Claim 19 (depends on 18)

A system in accordance with claim 18 and further comprising a charge-neutralizing filament positioned to enclose the Argon ion beam when said Argon ion beam milling source is in operation.

### Claim 20 (depends on 15)

A system in accordance with claim 15 wherein and further including means for cooling said semiconductor structure.

### Claim 21

A method of delayering a semiconductor structure including a first layer of material overlaying a second layer of low-k dielectric film and having multiple layers of interconnect metal therein, comprising the steps of:
removing the first layer of material to expose the second layer of low-k dielectric film;
removing at least a portion of the low-k dielectric film;
depositing a layer of backfill material into the space created by removing at least a portion of the low-k dielectric film; and
polishing to remove the layer of backfill material and at least one layer of the multiple layers of interconnect metal.

### Claim 22 (depends on 21)

A method in accordance with claim 21 wherein the step of removing the first layer of material is performed using one of the group of reactive ion etching and chemical-mechanical polishing.

### Claim 23 (depends on 21)

A method in accordance with claim 21 wherein said step of removing at least a portion of the low-k dielectric film comprises etching said low-k dielectric film with an oxygen ash.

### Claim 24 (depends on 21)

A method in accordance with claim 21 wherein said backfill material comprises one of the group of oxide and tetraothrosilicate.

### Claim 25

A method of delayering a semiconductor structure including a first layer of material overlaying a second layer of low-k dielectric film and having multiple layers of interconnect metal therein, comprising the steps of:
etching the first layer of material to expose the second layer of low-k dielectric film;
exposing the semiconductor structure to a metal etch to remove at least a portion of one level of said multiple layers of interconnect metal;
etching to remove exposed low-k dielectric film; and
polishing exposed metal vias.

### Claim 26 (depends on 25)

A method in accordance with claim 25 wherein the step of etching the first layer of material is performed using a reactive ion etch.

### Claim 27 (depends on 25)