# US 2004/0082173 A1 · Micro pattern forming method and semiconductor device manufacturing method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0082173 A1
- Document ID: US20040082173A1
- Status: Published application
- Kind: A1
- Application number: 10/685,790
- Filed: 2003-10-16
- Published: 2004-04-29
- Earliest claimed: 2002-10-18
- Assignees: Fujitsu Limited
- Inventors: Hirofumi Watatani
- Web page: https://patentgrep.com/patent/US20040082173A1

## CPC

- H10W 20/085: {involving intermediate temporary filling with material}
- H10P 50/73: {using masks for insulating materials}
- H10P 76/2043: {using an anti-reflective coating}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A first antireflection film is formed on the surface of an underlying substrate, the first antireflection film suppressing reflection in an absorption mode. A second antireflection film is formed on the first antireflection film, the second antireflection film suppressing reflection in a countervailing interference mode. A cap film is formed on the second antireflection film. A photosensitive resist film is formed on the cap film. A latent image is formed in the photosensitive resist film by exposing the photosensitive resist film to light having a first wavelength. The exposed resist film is developed. Even if the resist film is ashed and resist is again coated, the initial reflectivity lowering effects can be retained.

## Claims

### Claim 1

A method of forming a micro pattern comprising steps of:
forming a first antireflection film on a surface of an underlying substrate, the first antireflection film suppressing reflection in an absorption mode;
forming a second antireflection film on the first antireflection film, the second antireflection film suppressing reflection in a countervailing interference mode;
forming a cap film on the second antireflection film;
forming a photosensitive resist film on the cap film;
forming a latent image in the photosensitive resist film by exposing the photosensitive resist film to light having a first wavelength; and
developing the exposed photosensitive resist film.

### Claim 2 (depends on 1)

A method of forming a micro pattern according to claim 1, wherein an attenuation coefficient of the cap film at the first wavelength is smaller than an attenuation coefficient of the second antireflection film at the first wavelength.

### Claim 3 (depends on 1)

A method of forming a micro pattern according to claim 1, wherein an attenuation coefficient of the cap film at the first wavelength is 0.

### Claim 4 (depends on 1)

A method of forming a micro pattern according to claim 1, wherein an attenuation coefficient of the first antireflection film is 1 or higher at the first wavelength.

### Claim 5 (depends on 1)

A method of forming a micro pattern according to claim 1, wherein an attenuation coefficient of the second antireflection film is 0.9 or lower at the first wavelength.

### Claim 6

A method of manufacturing a semiconductor device comprising steps of:
forming an interlayer insulating film on a surface of a substrate having an insulating surface, formed with semiconductor elements, and having a conductive member exposed in a partial area of the insulating surface;
forming a first antireflection film having a first attenuation coefficient on the interlayer insulating film;
forming a second antireflection film having a second attenuation coefficient smaller than the first attenuation coefficient on the first antireflection film;
forming a cap film on the second antireflection film;
forming a first photosensitive resist film on the cap film;
exposing the first photosensitive resist film to light of a first wavelength, developing the exposed first photosensitive film to form an opening through the first photosensitive resist film; and
etching the interlayer insulating film by using the first photosensitive resist film as a mask.

### Claim 7 (depends on 6)

A method of manufacturing a semiconductor device according to claim 6, wherein an attenuation coefficient of the cap film at the first wavelength is smaller than the second attenuation coefficient of the second antireflection film at the first wavelength.

### Claim 8 (depends on 6)

A method of manufacturing a semiconductor device according to claim 6, wherein an attenuation coefficient of the cap film at the first wavelength is 0.

### Claim 9 (depends on 6)

A method of manufacturing a semiconductor device according to claim 6, wherein the first attenuation coefficient of the first antireflection film is 1 or higher at the first wavelength.

### Claim 10 (depends on 6)

A method of manufacturing a semiconductor device according to claim 6, wherein the second attenuation coefficient of the second antireflection film is 0.9 or lower at the first wavelength.

### Claim 11

A method of manufacturing a semiconductor device comprising steps of:
forming an interlayer insulating film on a surface of a substrate having an insulating surface, formed with semiconductor elements, and having a conductive member exposed in a partial area of the insulating surface;
forming a first antireflection film on the interlayer insulating film, the first antireflection film suppressing reflection in an absorption mode;
forming a second antireflection film on the first antireflection film, the second antireflection film suppressing reflection in a countervailing interference mode;
forming a cap film on the second antireflection film;
forming a first photosensitive resist film on the cap film;
exposing the first photosensitive resist film to light of a first wavelength, developing the exposed film to form an opening through the first photosensitive resist film, the opening corresponding to a via hole for connecting a wiring pattern to be formed on the interlayer insulating film to the conductive member;
etching the interlayer insulating film to form the via hole by using the first photosensitive resist film as a mask;
removing the first photosensitive resist film;
forming a second photosensitive resist film on the cap film;
exposing the second photosensitive resist film to light of the first wavelength, developing the exposed film to form an opening through the second photosensitive resist film, the opening corresponding to the wiring pattern to be formed on the interlayer insulating film;
etching the interlayer insulating film to form a wiring groove by using the second photosensitive resist film as a mask, the wiring groove reaching a midst of the interlayer insulating film in a thickness direction thereof;
removing the second photosensitive resist film;
deepening the via hole until the conductive member is exposed if the conductive member is not exposed on a bottom of the via hole; and
burying an inside of the via hole and the wiring groove with a conductive wiring material.

### Claim 12 (depends on 11)

A method of manufacturing a semiconductor device according to claim 11, wherein an attenuation coefficient of the cap film at the first wavelength is smaller than an attenuation coefficient of the second antireflection film at the first wavelength.

### Claim 13 (depends on 11)

A method of manufacturing a semiconductor device according to claim 11, wherein an attenuation coefficient of the cap film at the first wavelength is 0.

### Claim 14 (depends on 11)

A method of manufacturing a semiconductor device according to claim 11, wherein an attenuation coefficient of the first antireflection film is 1 or higher at the first wavelength.

### Claim 15 (depends on 11)

A method of manufacturing a semiconductor device according to claim 11, wherein an attenuation coefficient of the second antireflection film is 0.9 or lower at the first wavelength.