# US 2004/0082170 A1 · Method for forming fine pattern of semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0082170 A1
- Document ID: US20040082170A1
- Status: Published application
- Kind: A1
- Application number: 10/462,448
- Filed: 2003-06-16
- Published: 2004-04-29
- Earliest claimed: 2002-10-26
- Assignees: Samsung Electronics Co., Ltd.
- Inventors: Sang-Jun Choi; Young-Mi Lee; Woo-Sung Han
- Web page: https://patentgrep.com/patent/US20040082170A1

## CPC

- G03F 7/40: Treatment after imagewise removal, e.g. baking
- H10P 76/2042: {using lasers}
- H10P 76/2043: {using an anti-reflective coating}
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Provided is a method for forming a fine pattern of a semiconductor device by controlling the amount of flow of a resist pattern, including forming a resist pattern having a predetermined pattern distance on a material layer to be etched, forming a flow control barrier layer on the resist pattern to control the amount of flow during a subsequent resist flow process and to make the profile of the flowed pattern be vertical, optionally forming the flow control barrier layer by coating a material including a water-soluble high-molecular material and a crosslinking agent on the resist pattern, mixing and baking the coated material layer, and processing the resultant structure using deionized water, carrying out the flow resist process to form a hyperfine pattern and etching the lower material layer, and thereby forming fine patterns having the shape of contact holes or lines and spaces to have a critical dimension of about 100 nm or less, even with use of a KrF resist.

## Claims

### Claim 1

A method for forming a fine pattern of a semiconductor device, the method comprising:
forming a photoresist layer on a target layer to be etched;
exposing and developing the photoresist layer to form a first resist pattern;
forming a flow control barrier layer on the first resist pattern so as to control flow of the first resist pattern during a subsequent resist flow process to form a second resist pattern;
performing the resist flow process to form a third resist pattern having a pattern distance shorter than that of the second resist pattern; and
etching the target layer by using the third resist pattern as an etch mask.

### Claim 2 (depends on 1)

The method as claimed in claim 1, wherein the first, second, and third resist patterns are contact hole patterns, and the diameter of a contact hole of the third resist pattern is smaller than that of a contact hole of the second resist pattern.

### Claim 3 (depends on 2)

The method as claimed in claim 2, wherein the first resist pattern is formed such that the diameter of a contact hole ranges from 140 nm to 240 nm.

### Claim 4 (depends on 1)

The method as claimed in claim 1, wherein the flow control barrier layer is formed to have a thickness of 10 nm to 100 nm.

### Claim 5 (depends on 1)

The method as claimed in claim 1, wherein the photoresist layer is formed of one of KrF resist and ArF resist.

### Claim 6

A method for forming a fine pattern of a semiconductor device, the method comprising:
forming a photoresist layer on a target layer to be etched;
exposing and developing the photoresist layer to form a first resist pattern;
forming a high-molecular material layer being soluble in a specific solvent on the target layer and the first resist pattern;
forming a flow control barrier layer at an interface between the first resist pattern and the material layer, the flow control barrier layer insoluble in the specific solvent and for controlling the growth of the first resist pattern during a subsequent resist flow process;
removing the remaining high-molecular material layer by using the specific solvent to form a second resist pattern;
performing the resist flow process to form a third resist pattern having a pattern distance shorter than that of the second resist pattern; and
etching the target layer by using the third resist pattern as an etch mask.

### Claim 7 (depends on 6)

The method as claimed in claim 6, wherein the first, second, and third resist patterns are contact hole patterns, and the diameter of a contact hole of the third resist pattern is smaller than that of a contact hole of the second resist pattern.

### Claim 8 (depends on 7)

The method as claimed in claim 7, wherein the first resist pattern is formed such that the diameter of a contact hole ranges from 140 nm to 240 nm.

### Claim 9 (depends on 6)

The method as claimed in claim 6, wherein the material layer is formed of a material including a water-soluble high-molecular material and a water-soluble crosslinking agent, and the flow control barrier layer is formed of a water-insoluble material.

### Claim 10 (depends on 6)

The method as claimed in claim 6, wherein the flow control barrier layer is formed to have a thickness of 10 nm to 100 nm.

### Claim 11 (depends on 6)

The method as claimed in claim 6, wherein the photoresist layer is formed of one of KrF resist and ArF resist.

### Claim 12

A method for forming a fine pattern of a semiconductor device, the method comprising:
forming a photoresist layer on a target layer to be etched;
exposing and developing the photoresist layer to form a first resist pattern;
forming a water-soluble high-molecular material layer on the target layer and the first resist pattern;
mixing and baking the material layer to form a flow control barrier layer that is insoluble in water and formed at an interface between the first resist pattern and the material layer;
removing the remaining water-soluble high-molecular material layer by using water to form a second resist pattern;
performing the resist flow process to form a third resist pattern having a pattern distance shorter than that of the second resist pattern; and
etching the target layer by using the third resist pattern as an etch mask.

### Claim 13 (depends on 12)

The method as claimed in claim 12, wherein the first, second, and third resist patterns, and the diameter of a contact hole of the third resist pattern is smaller than that of a contact hole of the second resist pattern.

### Claim 14 (depends on 13)

The method as claimed in claim 13, wherein the first resist pattern is formed such that the diameter of a contact hole ranges from 140 nm to 240 nm.

### Claim 15 (depends on 12)

The method as claimed in claim 12, wherein the material layer is formed of a material including a water-soluble high-molecular material and a water-soluble crosslinking agent.

### Claim 16 (depends on 12)

The method as claimed in claim 12, wherein the material layer is mixed and baked at a temperature of 90° C. to 150° C.

### Claim 17 (depends on 12)

The method as claimed in claim 12, wherein the flow control barrier layer is formed to have a thickness of 10 nm to 100 nm.

### Claim 18 (depends on 12)

The method as claimed in claim 12, wherein the resist flow process is performed at a temperature higher than the glass transition temperature by about 1° C. to about 50° C.

### Claim 19 (depends on 17)

The method as claimed in claim 17, wherein the resist flow process is performed at a temperature of about 120° C. to about 170° C.

### Claim 20 (depends on 12)

The method as claimed in claim 12, wherein the photoresist layer is formed of one of KrF resist and ArF resist.