# US 2004/0082169 A1 · Deposition of barrier metal in damascene interconnects using metal carbonyl

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0082169 A1
- Document ID: US20040082169A1
- Status: Published application
- Kind: A1
- Application number: 10/282,388
- Filed: 2002-10-29
- Published: 2004-04-29
- Earliest claimed: 2002-10-29
- Assignees: Chartered Semiconductor Manufacturing Ltd.
- Inventors: Simon Chooi; Mei Sheng Zhou; Subhash Gupta
- Web page: https://patentgrep.com/patent/US20040082169A1

## CPC

- H10W 20/033: {in openings in dielectrics}
- H10P 14/43: Chemical deposition, e.g. chemical vapour deposition [CVD]
- H10W 20/043: {for electroplating}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

This invention relates to a method of fabrication used for semiconductor integrated circuit devices, and more specifically to the formation of single or dual damascene interconnects using a barrier metal layer of WNx or TaNx, deposited by plasma enhanced chemical vapor deposition (PECVD) using metal carbonyl precursors. By using a chemical vapor deposition (CVD) process with these alternate carbonyl precursors, many of the problems are solved, i.e., conformal coverage, gas phase particle generation, and incorporation of halogens or carbon into the film.

## Claims

### Claim 1

A method of forming conducting metal lines and interconnects in trenches and vias in the fabrication of integrated circuit devices using barrier metal layer of WNx or TaNx deposited using metal carbonyl precursors, comprising:
providing a substrate having a thin insulator layer deposited upon it;
depositing a layer of first thick insulator material upon the insulator layer;
blanket depositing a layer of second thick insulator material above the layer of the first thick insulator material;
providing patterning and etching of both the second and first thick insulator material to form trench/via opening or cavity;
depositing a blanket layer of barrier metal over the substrate;
depositing by plating conducting thick copper over the barrier;
then chemical mechanical polishing, planarizing the surface, removing excess material, forming interconnect inlaid metal wiring, in a damascene process with WNx or TaNx barriers.

### Claim 2 (depends on 1)

The method of claim 1, wherein said layer of first thick insulator material is selected from the group consisting of: (a) undoped silicon oxide, (b) doped silicon oxide doped with fluorine, phosphorus, or carbon, (c) organic polymer, (d) porous or non-porous entity of the above, which are deposited by methods selecting from the group consisting of: PECVD or HDP-CVD with TEOS as one of the precursors, or spin coating, in the thickness range from 2,000 to 12,000 Angstroms, followed by an oven bake and furnace cure.

### Claim 3 (depends on 1)

The method of claim 1, wherein said layer of second thick insulator material is selected from the group consisting of: (a) undoped silicon oxide, (b) doped silicon oxide doped with fluorine, phosphorus, or carbon, (c) organic polymer, (d) porous or non-porous entity of the above, which are deposited by methods selecting from the group consisting of: PECVD or HDP-CVD with TEOS as one of the precursors, or spin coating, in the thickness range from 2,000 to 12,000 Angstroms, followed by an oven bake and furnace cure.

### Claim 4 (depends on 1)

The method of claim 1, wherein said barrier metal is composed of WNx or TaNx, deposited by plasma enhanced chemical vapor deposition (PECVD) with metal carbonyl precursors.

### Claim 5 (depends on 1)

The method of claim 1, wherein said barrier metal composed of WNx or TaNx, is deposited by plasma enhanced chemical vapor deposition (PECVD) with metal carbonyl precursors, barrier metal with thickness from approximately 50 to 2,000 Angstroms.

### Claim 6 (depends on 1)

The method of claim 1, for said tungsten nitride and said tantalum nitride are barrier metals deposited by plasma enhanced chemical vapor deposition (PECVD) with metal carbonyl precursors, the deposition (PECVD) conditions used are the following: source temperature between approximately 50 to 250° C., wafer or substrate temperature between approximately 200 to 450° C., chamber pressure between approximately 0.1 to 0.5 Torr, flow rate of carbonyl between approximately 1 to 30 sccm, flow rate of reactive gas or gases between approximately 50 to 1000 sccm (excluding the carrier gases), with ratios of flow rate of carbonyl to reactive gases between 1 to 1,000 and between 1,000 to 1, barrier metal thickness is between approximately 50 to 2,000 Angstroms.

### Claim 7 (depends on 1)

The method of claim 1, a copper seed layer of copper is needed for copper plating wherein thick copper is deposited by electroplating upon a copper seed layer, which is deposited by CVD in a thickness range from 50 to 1,000 Angstroms, upon a barrier layer.

### Claim 8 (depends on 1)

The method of claim 1, for said conducting thick copper is copper, deposited in a thickness range from 1 to 10 microns.

### Claim 9 (depends on 1)

The method of claim 1, wherein a single damascene process is a subset of said dual damascene, with a single damascene process forming a via or a trench.

### Claim 10

A method of using the dual damascene technique to form a conductive contact to a multi-level metal line and interconnection wiring pattern, in the fabrication semiconductor devices comprising:
providing said conducting line on an inter-level dielectric, which is on a semiconductor substrate;
depositing an insulator layer upon the conducting line;
depositing a layer of first thick insulator material upon the insulator layer;
blanket depositing a layer of second thick insulator material above the layer of the first thick insulator material;
providing patterning and etching of the second and first thick insulator material, insulating layer to form trench/via opening or cavity, etching down to the conducting line;
depositing a blanket layer of barrier metal over the substrate using barrier metal layer of WNx or TaNx, deposited by plasma enhanced chemical vapor deposition (PECVD) with metal carbonyl precursors;
depositing by plating conducting thick copper over the barrier metal layer;
chemical-mechanical polishing, planarizing the surface, removing excess thick copper and excess barrier metal, forming inlaid interconnect and contact via to conducting line, in a dual damascene process, with WNx or TaNx barrier metal lining the trench/via.

### Claim 11 (depends on 10)

The method of claim 10, wherein said layer of first thick insulator material is selected from the group consisting of: (a) undoped silicon oxide, (b) doped silicon oxide doped with fluorine, phosphorus, or carbon, (c) organic polymer, (d) porous or non-porous entity of the above, which are deposited by methods selecting from the group consisting of: PECVD or HDP-CVD with TEOS as one of the precursors, or spin coating, in the thickness range from 2,000 to 12,000 Angstroms, followed by an oven bake and furnace cure.

### Claim 12 (depends on 10)

The method of claim 10, wherein said layer of second thick insulator material is selected from the group consisting of: (a) undoped silicon oxide, (b) doped silicon oxide doped with fluorine, phosphorus, or carbon, (c) organic polymer, (d) porous or non-porous entity of the above, which are deposited by methods selecting from the group consisting of: PECVD or HDP-CVD with TEOS as one of the precursors, or spin coating, in the thickness range from 2,000 to 12,000 Angstroms, followed by an oven bake and furnace cure.

### Claim 13 (depends on 10)

The method of claim 10, wherein said barrier metal is composed of WNx or TaNx, deposited by plasma enhanced chemical vapor deposition (PECVD) with metal carbonyl precursors.

### Claim 14 (depends on 10)

The method of claim 10, wherein said barrier metal composed of WNx or TaNx, is deposited by plasma enhanced chemical vapor deposition (PECVD) with metal carbonyl precursors, barrier metal with thickness from approximately 50 to 2,000 Angstroms.

### Claim 15 (depends on 10)

The method of claim 10, for said tungsten nitride and said tantalum nitride are barrier metals deposited by plasma enhanced chemical vapor deposition (PECVD) with metal carbonyl precursors, the deposition (PECVD) conditions used are the following: source temperature between approximately 50 to 250° C., wafer or substrate temperature between approximately 200 to 450° C., chamber pressure between approximately 0.1 to 0.5 Torr, flow rate of carbonyl between approximately 1 to 30 sccm, flow rate of reactive gas or gases between approximately 50 to 1000 sccm (excluding the carrier gases), with ratios of flow rate of carbonyl to reactive gases between 1 to 1,000 and between 1,000 to 1, barrier metal thickness is between approximately 50 to 2,000 Angstroms.

### Claim 16 (depends on 10)

The method of claim 10, a copper seed layer of copper is needed for copper plating wherein thick copper is deposited by electroplating upon a copper seed layer, which is deposited by CVD in a thickness range from 50 to 1,000 Angstroms, upon a barrier layer.

### Claim 17 (depends on 10)

The method of claim 10, for said conducting thick copper is copper, deposited in a thickness range from 1 to 10 microns.

### Claim 18 (depends on 10)

The method of claim 10, wherein a single damascene process is a subset of said dual damascene, with a single damascene process forming a via or a trench.

### Claim 19

A method of using the dual damascene technique to form a conductive contact to a semiconductor doped diffusion and interconnection wiring pattern, in the fabrication of an MOSFET comprising:
providing an active device element, doped diffusion region in a semiconductor substrate;
depositing a layer of first thick insulator material upon the insulator layer;
blanket depositing a layer of second thick insulator material above the layer of the first thick insulator material;
providing patterning and etching of the second and first thick insulator material, insulating layer to form trench/via opening or cavity, etching down to the doped diffusion region;
depositing a blanket layer of barrier metal over the substrate using barrier metal layer of WNx or TaNx, deposited by plasma enhanced chemical vapor deposition (PECVD) with metal carbonyl precursors;
depositing by plating conducting thick copper upon the barrier layer;
chemical-mechanical polishing, planarizing the surface, removing excess thick copper and excess barrier metal, forming inlaid interconnect and contact via to the doped diffusion region, in a dual damascene process, with WNx or TaNx barrier metal lining the trench/via.

### Claim 20 (depends on 19)

The method of claim 19, wherein said layer of first thick insulator material is selected from the group consisting of: (a) undoped silicon oxide, (b) doped silicon oxide doped with fluorine, phosphorus, or carbon, (c) organic polymer, (d) porous or non-porous entity of the above, which are deposited by methods selecting from the group consisting of: PECVD or HDP-CVD with TEOS as one of the precursors, or spin coating, in the thickness range from 2,000 to 12,000 Angstroms, followed by an oven bake and furnace cure.

### Claim 21 (depends on 19)

The method of claim 19, wherein said layer of second thick insulator material is selected from the group consisting of: (a) undoped silicon oxide, (b) doped silicon oxide doped with fluorine, phosphorus, or carbon, (c) organic polymer, (d) porous or non-porous entity of the above, which are deposited by methods selecting from the group consisting of: PECVD or HDP-CVD with TEOS as one of the precursors, or spin coating, in the thickness range from 2,000 to 12,000 Angstroms, followed by an oven bake and furnace cure.

### Claim 22 (depends on 19)

The method of claim 19, wherein said barrier metal is composed of WNx or TaNx, deposited by plasma enhanced chemical vapor deposition (PECVD) with metal carbonyl precursors.

### Claim 23 (depends on 19)

The method of claim 19, wherein said barrier metal composed of WNx or TaNx, is deposited by plasma enhanced chemical vapor deposition (PECVD) with metal carbonyl precursors, barrier metal with thickness from approximately 50 to 2,000 Angstroms.

### Claim 24 (depends on 19)

The method of claim 19, for said tungsten nitride and said tantalum nitride are barrier metals deposited by plasma enhanced chemical vapor deposition (PECVD) with metal carbonyl precursors, the deposition (PECVD) conditions used are the following: source temperature between approximately 50 to 250° C., wafer or substrate temperature between approximately 200 to 450° C., chamber pressure between approximately 0.1 to 0.5 Torr, flow rate of carbonyl between approximately 1 to 30 sccm, flow rate of reactive gas or gases between approximately 50 to 1000 sccm (excluding the carrier gases), with ratios of flow rate of carbonyl to reactive gases between 1 to 1,000 and between 1,000 to 1, barrier metal thickness is between approximately 50 to 2,000 Angstroms.

### Claim 25 (depends on 19)

The method of claim 19, a copper seed layer of copper is needed for copper plating wherein thick copper is deposited by electroplating upon a copper seed layer, which is deposited by CVD in a thickness range from 50 to 1,000 Angstroms, upon a barrier layer.

### Claim 26 (depends on 19)

The method of claim 19, for said conducting thick copper is copper, deposited in a thickness range from 1 to 10 microns.

### Claim 27 (depends on 19)

The method of claim 19, wherein a single damascene process is a subset of said dual damascene, with a single damascene process forming a via or a trench.
2 TABLE I DEP. OF WNx DEP. OF TaNx W(CO)6 + NH3 Ta(CO)4Cp + NH3 W(CO)6 + N2/H2 Ta(CO)4Cp + N2/H2 W(CO)6 + N2H2 Ta(CO)4Cp + N2H2 W(CO)6 + NO Ta(CO)4Cp + NO Note: N2H2 is hydrazine and Cp is cyclo-pentadiene.