# US 2004/0082168 A1 · Method for forming metal silicide layer in active area of semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0082168 A1
- Document ID: US20040082168A1
- Status: Published application
- Kind: A1
- Application number: 10/613,331
- Filed: 2003-07-03
- Published: 2004-04-29
- Earliest claimed: 2002-07-05
- Assignees: Hynix Semiconductor Inc.
- Inventors: In-Haeng Lee; Yoon-Jik Lee
- Web page: https://patentgrep.com/patent/US20040082168A1

## CPC

- H10W 20/033: {in openings in dielectrics}
- H10D 64/0112: {using conductive layers comprising silicides}
- H10D 64/01125: {the silicides being formed by chemical reaction with the semiconductor after the contact hole formation}
- H10P 95/00: Generic processes or apparatus for manufacture or treatments not covered by the other groups of this subclass
- H10W 20/047: {by introducing additional elements therein}
- H10W 20/0523: {by irradiating with ultraviolet or particle radiation}
- H10D 30/0212: {using self-aligned silicidation}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

The present invention provides a method for forming a metal silicide layer in an active area of the semiconductor device. The method for forming the metal silicide layer includes: forming a source/drain junction area on a silicon substrate; forming an attack protection layer on the source/drain junction area, wherein the attack protection layer is electrically conductive and prevents a silicon substrate attack caused by chlorine (Cl) gas; forming a titanium (Ti) layer over the attack protection layer through a low pressure chemical vapor deposition (LPCVD) process using a source gas of TiCl4; and diffusing the Ti layer into the attack protection layer to thereby form a metal silicide layer.

## Claims

### Claim 1

A method of forming a semiconductor device having a metal silicide, comprising the steps of:
forming a source/drain junction area on a silicon substrate;
forming an attack protection layer on the source/drain junction area, wherein the attack protection layer is electrically conductive and prevents a silicon substrate attack caused by chlorine (Cl) gas;
forming a titanium (Ti) layer over the attack protection layer through a low pressure chemical vapor deposition (LPCVD) process using a source gas of TiCl4; and
diffusing the Ti layer into the attack protection layer to thereby form a metal silicide layer.

### Claim 2 (depends on 1)

The method as recited in claim 1, wherein a poly-silicon layer formed by using a chemical vapor deposition (CVD) process is used for forming the attack protection layer.

### Claim 3 (depends on 1)

The method as recited in claim 1, further comprising the step of deoxidizing the surface of the Ti layer using hydrogen (H2) gas to remove a remnant chlorine (Cl) radical in the Ti layer.

### Claim 4 (depends on 1)

The method as recited in claim 1, further comprising the step of illuminating an ultra violet light having a higher energy than a binding energy of a SiCl reaction product on the surface of the Ti layer to remove the remnant chlorine (Cl) radical in the Ti layer.

### Claim 5 (depends on 2)

The method as recited in claim 2, wherein the attack protection layer is formed by the CVD process using a source gas of Si2H6/Cl/H2.

### Claim 6 (depends on 2)

The method as recited in claim 2, wherein a thickness of the attack protection layer ranges from about 50 Å to about 200 Å

### Claim 7 (depends on 5)

The method as recited in claim 5, wherein the CVD process for forming the attack protection layer is carried out at a temperature ranging from about 600° C. to about 700° C. and at a pressure ranging from about 0.1 mtorr to about 1.0 mtorr.

### Claim 8 (depends on 5)

The method as recited in claim 5, further comprising the step of deoxidizing the surface of the attack protection layer by using hydrogen (H2) gas to remove the remnant chlorine (Cl) radical in the attack protection layer after depositing the attack protection layer.

### Claim 9 (depends on 5)

The method as recited in claim 5, further comprising the step of illuminating an ultra violet light having a higher energy than a binding energy of SiCl on the surface of the attack protection layer to remove the remnant chlorine (Cl) radical in the attack protection layer;

### Claim 10 (depends on 1)

The method as recited in claim 1, wherein a titanium nitride (TiN) layer formed by using a chemical vapor deposition (CVD) process is used for forming the attack protection layer.

### Claim 11 (depends on 10)

The method as recited in claim 10, wherein the TiN layer is deposited by using the TiCl4 source gas added with ammonia (NH3) gas in an identical chamber where the Ti layer is subsequently deposited.

### Claim 12 (depends on 10)

The method as recited in claim 10, wherein a thickness of the attack protection layer ranges from about 50 Å to about 200 Å.

### Claim 13 (depends on 1)

The method as recited in claim 1, wherein the Ti layer is deposited by using the LPCVD process at a temperature ranging from about 600° C. to about 700° C. and at a pressure ranging from about 1 torr to about 50 torr.

### Claim 14 (depends on 13)

The method as recited in claim 13, wherein the LPCVD process is performed by using the TiCl4 source gas added with ammonia (NH3) gas and hydrogen (H2) gas including argon (Ar) gas and a flow amount ratio of the NH3 gas to the Ar gas is about 1 to about 5.

### Claim 15

A method for forming a barrier metal layer for a semiconductor device fabrication, comprising the steps of:
a) forming a contact hole exposing an active area through a selective etch of an insulation layer formed on a silicon substrate providing the active area;
b) forming an attack protection layer for preventing the silicon substrate attack caused by a succeeding titanium layer deposition process on the active area exposed by the contact hole, wherein the attack protection layer is electrically conductive;
c) forming a titanium (Ti) layer along a profile of the attack protection layer formed on the active area by using a low pressure chemical vapor deposition (LPCVD) process using a source gas of TiCl4;
d) diffusing the Ti layer into the attack protection layer to thereby forming a metal silicide layer; and
e) forming a titanium nitride (TiN) layer on the Ti layer.

### Claim 16 (depends on 15)

The method as recited in claim 15, wherein a poly-silicon layer formed by a chemical vapor deposition (CVD) process is used as the attack protection layer.

### Claim 17 (depends on 16)

The method as recited in claim 16, wherein the CVD process is carried out by using a source gas of Si2H6/Cl/H2.

### Claim 18 (depends on 17)

The method as recited in claim 17, wherein the CVD process for forming the attack protection layer is performed at a temperature ranging from about 600° C. to about 700° C. and at a pressure ranging from about 0.1 mtorr to about 1 mtorr.

### Claim 19 (depends on 15)

The method as recited in claim 15, wherein a titanium nitride (TiN) layer formed by a chemical vapor deposition (CVD) process is used as the attack protection layer.

### Claim 20 (depends on 19)

The method as recited in claim 19, wherein the attack protection layer is deposited by using the TiCl4 source gas added with ammonia (NH3) gas in an identical chamber where the Ti layer will be deposited.

### Claim 21 (depends on 19)

The method as recited in claim 19, wherein a thickness of the attack protection layer ranges from about 10 Å to about 100 Å

### Claim 22 (depends on 15)

The method as recited in claim 15, wherein the Ti layer is deposited by using the LPCVD process at a temperature ranging from about 600° C. to about 700° C. and at a pressure ranging from about 1 torr to about 50 torr.

### Claim 23 (depends on 22)

The method as recited in claim 22, wherein the LPCVD process is performed by using the TiCl4 source gas added with ammonia (NH3) gas and hydrogen (H2) gas including argon (Ar) gas and a flow amount ratio of the NH3 gas to the Ar gas is about 1 to about 5;

### Claim 24 (depends on 15)

The method as recited in claim 15, wherein the TiN layer is deposited on the Ti layer by using a low pressure chemical vapor deposition (LPCVD) process at a temperature ranging from about 600° C. to about 700° C. and at a pressure ranging from about 1 torr to about 50 torr.

### Claim 25 (depends on 24)

The method as recited in claim 24, wherein the LPCVD process is performed by using the TiCl4 source gas added with ammonia (NH3) gas and hydrogen (H2) gas including argon (Ar) gas and a flow amount ratio of the NH3 gas to the Ar gas is about 8 to about 15.

### Claim 26 (depends on 25)

The method as recited in claim 25, wherein the TiN layer is deposited in an identical chamber where the Ti layer is deposited.

### Claim 27 (depends on 15)

The method as recited in claim 15, wherein the titanium silicide layer is produced by carrying out a heat treatment process at a temperature ranging from about 700° C. to about 900° C.

### Claim 28 (depends on 15)

The method as recited in claim 15, wherein further comprising the step of deoxidizing the surface of the Ti layer using hydrogen (H2) gas to remove a remnant chlorine radical after depositing the Ti layer and the TiN layer.

### Claim 29 (depends on 17)

The method as recited in claim 17, further comprising the step of deoxidizing the surface of the attack protection layer using a hydrogen (H2) gas to remove remnant chlorine radical after depositing the attack protection layer, i.e., the poly-silicon layer.

### Claim 30 (depends on 15)

The method as recited in claim 15, further comprising the step of illuminating an ultra violet light having a bigger energy than a binding energy of SiCl on the surface of the Ti layer to remove remnant chlorine (Cl) radical in the Ti layer.

### Claim 31 (depends on 17)

The method as recited in claim 17, further comprising the step of illuminating an ultra violet light having a bigger energy than a binding energy of SiCl to remove remnant chlorine (Cl) radical in the attack protection layer.