# US 2004/0082167 A1 · Methods of forming aluminum structures in microelectronic articles and articles fabricated thereby

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0082167 A1
- Document ID: US20040082167A1
- Status: Published application
- Kind: A1
- Application number: 10/620,995
- Filed: 2003-07-16
- Published: 2004-04-29
- Earliest claimed: 2002-08-26
- Inventors: Jung-Hun Seo; Gil-Heyun Choi; Ju-Young Yun; Byung-Hee Kim; Seung-Gil Yang
- Web page: https://patentgrep.com/patent/US20040082167A1

## CPC

- H10W 20/033: {in openings in dielectrics}
- H10W 20/045: {for deposition from the gaseous phase, e.g. for chemical vapour deposition [CVD]}
- H10W 20/0523: {by irradiating with ultraviolet or particle radiation}
- H10W 20/056: {by filling conductive material into holes, grooves or trenches}
- H10W 20/0425: {comprising multiple stacked seed or nucleation layers}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A recess is formed in a microelectronic substrate, and then a metal-containing layer is formed that conforms to an inner surface of the recess and to a surface of the substrate adjacent the recess. A carbon concentration in a portion of the metal-containing layer on the surface of the substrate adjacent the recess is decreased in comparison to a portion of the metal-containing layer within the recess, e.g., using a plasma treatment that has a greater effect on the surface outside of the recess. Aluminum is then deposited on the metal-containing layer to form an aluminum layer that conforms to the inner surface of the recess and to the surface of the substrate adjacent the recess. Preferably, the carbon concentration in the portion of the metal-containing layer within the recess is sufficiently great to cause aluminum to deposited at a greater rate on the portion of the metal-containing layer within the recess.

## Claims

### Claim 1

A method of forming an aluminum structure in a microelectronic article, the method comprising:
forming a recess in a microelectronic substrate;
forming a metal-containing layer conforming to a surface of the recess and to an adjacent surface of the substrate;
plasma treating the substrate having the metal-containing layer thereon; and
depositing aluminum on the metal-containing layer to form an aluminum layer thereon.

### Claim 2 (depends on 1)

The method of claim 1, wherein depositing aluminum comprises depositing the aluminum at a temperature of about 160° C. or less.

### Claim 3 (depends on 1)

The method of claim 1, wherein forming a recess comprises forming a contact hole in an insulating layer of the substrate that exposes an underlying conductive region of the substrate.

### Claim 4 (depends on 1)

The method of claim 1, wherein the recess has an aspect ratio greater than about 1.

### Claim 5 (depends on 1)

The method of claim 1, wherein forming a metal-containing layer comprises forming the metal-containing layer by metal organic chemical vapor deposition (MOCVD).

### Claim 6 (depends on 5)

The method of claim 5, wherein the metal-containing layer is a barrier metal layer.

### Claim 7 (depends on 6)

The method of claim 6, wherein the metal-containing layer comprises at least one material selected from a group consisting of titanium nitride (TiN), tantalum nitride (TaN), titanium silicon nitride (TiSiN) and tantalum silicon nitride (TaSiN).

### Claim 8 (depends on 1)

The method of claim 1, wherein depositing aluminum comprises depositing aluminum on the metal-containing layer by chemical vapor deposition (CVD) using a methylpyrrolidine alane (MPA) source gas.

### Claim 9 (depends on 1)

The method of claim 1, wherein plasma treating the substrate comprises plasma treating using at least one gas selected from a group consisting of argon (Ar), hydrogen (H2), nitrogen (N2), oxygen (O2), nitrous oxide (N2O) and ammonia (NH3).

### Claim 10 (depends on 1)

The method of claim 1, wherein plasma treating the substrate comprises plasma treating the substrate at a pressure in a range from about 1 Torr to about 6 Torr.

### Claim 11 (depends on 1)

The method of claim 1, wherein plasma treating the substrate comprises plasma treating the substrate at a power level in a range from about 600 W to about 1,000 W.

### Claim 12 (depends on 1)

The method of claim 1, wherein plasma treating the substrate comprises plasma treating the substrate for about 60 seconds.

### Claim 13 (depends on 1)

The method of claim 1:
wherein forming a metal-containing layer is preceded by forming an ohmic layer conforming to an interior surface of the recess and to the adjacent surface of the insulating layer; and
wherein forming a metal-containing layer comprises forming the metal-containing layer on the ohmic layer.

### Claim 14 (depends on 13)

The method of claim 13, wherein the ohmic layer comprises at least one of titanium (Ti) or tantalum (Ta).

### Claim 15 (depends on 1)

The method of claim 1:
wherein forming a metal-containing layer comprises forming a first metal-containing layer;
wherein plasma treating comprises plasma treating the substrate having the first metal-containing layer thereon;
wherein depositing aluminum on the metal-containing layer comprises depositing aluminum on the first metal-containing layer to form a first aluminum layer thereon; and
wherein the method further comprises:
forming a second metal-containing layer conforming to an interior surface of the recess and to an adjacent surface of the insulating layer;
plasma treating the substrate having the second metal-containing layer thereon; and
depositing aluminum on the second metal-containing layer at a temperature of about 160° C. or less to form a second aluminum layer thereon.

### Claim 16 (depends on 1)

The method of claim 1, wherein depositing aluminum comprises depositing aluminum by CVD until the recess is filled.

### Claim 17 (depends on 1)

The method of claim 1, wherein depositing aluminum comprises:
depositing aluminum by CVD to form a seed aluminum layer in the recess; and
sputter depositing aluminum on the seed aluminum layer in the recess; and
wherein the method further comprises reflowing the deposited aluminum in the recess.

### Claim 18 (depends on 1)

The method of claim 1, wherein plasma treating the substrate comprises plasma treating the substrate under conditions sufficient to cause aluminum to deposit at a greater rate on a portion of the metal-containing layer within the recess than on a portion of the metal-containing layer adjacent the recess.

### Claim 19 (depends on 1)

The method of claim 1, wherein the recess comprises one of a hole, a trench, a groove or a step.

### Claim 20

A method of forming an aluminum structure in a microelectronic article, the method comprising:
forming a recess in a microelectronic substrate;
forming a metal-containing layer that conforms to an inner surface of the recess and to a surface of the substrate adjacent the recess;
decreasing a carbon concentration in a portion of the metal-containing layer on the surface of the substrate adjacent the recess in comparison to a portion of the metal-containing layer within the recess; and
depositing aluminum on the metal-containing layer to form an aluminum layer that conforms to the inner surface of the recess and to the surface of the substrate adjacent the recess.

### Claim 21 (depends on 20)

The method of claim 20, wherein decreasing a carbon concentration comprises plasma-treating the substrate having the metal-containing layer thereon.

### Claim 22 (depends on 21)

The method of claim 21, wherein plasma treating the substrate comprises plasma treating the substrate with at least one gas selected from a group consisting of argon (Ar), hydrogen (H2), nitrogen (N2), oxygen (O2), nitrous oxide (N2O) and ammonia (NH3) at a pressure in a range from about 1 Torr to about 6 Torr and a power level in a range from about 600 W to about 1,000 W.

### Claim 23 (depends on 21)

The method of claim 21, wherein plasma treating the substrate comprises plasma treating the substrate with at least one gas selected from a group consisting of argon (Ar), hydrogen (H2), nitrogen (N2), oxygen (O2), nitrous oxide (N2O) and ammonia (NH3) at a pressure in a range from about 1 Torr to about 6 Torr and a power level in a range from about 600 W to about 1,000 W for a duration of about 60 seconds.

### Claim 24 (depends on 20)

The method of claim 20, wherein decreasing a carbon concentration in a portion of the metal-containing layer on the surface of the substrate adjacent the recess in comparison to a portion of the metal-containing layer within the recess comprises creating a difference in carbon concentration between the portion of the metal-containing layer on the surface of the substrate adjacent the recess and the portion of the metal-containing layer within the recess sufficient to cause aluminum to deposited at a greater rate on the portion of the metal-containing layer within the recess than on the portion of the metal-containing layer on the surface of the substrate adjacent the recess.

### Claim 25 (depends on 20)

The method of claim 20, wherein forming a metal-containing layer comprises depositing a layer comprising at least one of Ta and Ti using a metal organic source gas.

### Claim 26 (depends on 20)

The method of claim 20, wherein depositing aluminum comprises depositing aluminum on the metal-containing layer using a CVD process with an MPA source gas.

### Claim 27 (depends on 26)

The method of claim 26, wherein depositing aluminum comprises depositing aluminum on the metal-containing layer using an MPA source gas at a temperature of about 160° C. or less.

### Claim 28 (depends on 20)

The method of claim 20, wherein the recess comprises one of a hole, a trench, a groove or a step.

### Claim 29

A microelectronic article of manufacture, comprising:
a substrate having a recess herein; and
a metal-containing layer on the substrate that conforms to an inner surface of the recess and to a surface of the substrate adjacent the recess, wherein the metal-containing layer has a substantially higher concentration of carbon in a portion of the metal-containing layer in the recess than in a portion of the metal-containing layer on the surface of the substrate adjacent the recess.

### Claim 30 (depends on 29)

The microelectronic article of manufacture of claim 29, wherein the metal-containing layer comprises at least one of Ta and Ti.

### Claim 31 (depends on 29)

The microelectronic article of manufacture according to claim 29, wherein the concentration of carbon in the portion of the metal-containing layer in the recess is sufficiently higher that the carbon concentration in the portion of the metal-containing layer on the surface of the substrate adjacent the recess to cause aluminum to deposit more rapidly on the portion of the metal-containing layer in the recess that on the portion of the metal-containing layer on the surface of the substrate adjacent the recess in an CVD process using an MPA source gas.