# US 2004/0082164 A1 · Chemistry for liner removal in a dual damascene process

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0082164 A1
- Document ID: US20040082164A1
- Status: Published application
- Kind: A1
- Application number: 10/282,386
- Filed: 2002-10-29
- Published: 2004-04-29
- Earliest claimed: 2002-10-29
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Chao-Cheng Chen; Chien-Chung Fu
- Web page: https://patentgrep.com/patent/US20040082164A1

## CPC

- H10W 20/071: {of dielectric parts thereof}
- H10P 95/066: {the removal being a selective chemical etching step, e.g. selective dry etching through a mask}
- H10W 20/084: {for dual-damascene structures}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

An improved and new process for fabricating dual damascene copper, in which trench/via liner removal from porous low-k dielectric, is performed using a new RIE chemistry of CF4/H2, to etch SiN and SiC liners. Prior to the new process, convention liner etching produced the following deleterious results: a) Cu re-deposition by sputtering, b) polymer deposits, and c) surface roughening of the porous low-k IMD dielectric. Process details are: CF4/H2 based with approximate gas flow ratios of greater than 10 to 1, hydrogen to carbon tetra-fluoride. A nominal flow ratio of 300 to 20, hydrogen to carbon tetra-fluoride, or 15 to 1, was developed.

## Claims

### Claim 1

A method for fabricating dual damascene trench and vias openings over copper wiring comprising:
providing a substrate with copper wiring thereon;
depositing an etch stop layer over the copper wiring;
depositing an insulating layer over the etch stop;
etching dual damascene trench/via openings, in the insulating layer exposing regions of the etch stop;
forming etch protected regions on the insulating layer, while exposing trench/via openings and portions of the etch stop layer in the trench/via openings;
etching away the exposed portions of the etch stop layer, thus exposing the underlying copper wiring.

### Claim 2 (depends on 1)

The method of claim 1, wherein said semiconductor substrate includes semiconductor device structures such as gate electrodes and source/drain regions.

### Claim 3 (depends on 1)

The method of claim 1, wherein said semiconductor substrate includes semiconductor device structures such as gate electrodes, source/drain regions and multiple levels of metal interconnections.

### Claim 4 (depends on 1)

The method of claim 1, wherein said insulating layer is a porous, low dielectric constant material or materials with dielectric constants less than 2.5 selected from the group comprised of SiN, SiO, SOG, which is spun-on-glass, PE plasma enhanced TEOS, which is tetraethoxysilane, halogenated SiO, and fluorinated silicate glass, all deposited by a chemical vapor deposition process or a spin-on process, in a thickness range from 2,000 to 15,000 Angstroms.

### Claim 5 (depends on 1)

The method of claim 1, wherein said etch stop layer is selected from the group comprised of SiN and SiC, deposited by chemical vapor deposition, in a thickness range from approximately 200 to 800 Angstroms.

### Claim 6 (depends on 1)

The method of claim 1, whereby trench and via openings are formed by etching the insulating layer by the following reactive ion etch process chemistry selected from the group of gases comprised of CF4, CHF3, CH2F2, C4F8, C5F8, C4F6, combined with ambient gas mixtures selected from the group comprised of Ar, O2, N2, CO and He, stopping the etch removal process on the etch stop layer.

### Claim 7 (depends on 1)

The method of claim 1, wherein the exposed portions of the etch stop layer are etched away exposing the underlying copper wiring by a reactive ion etch process comprised of following etchant chemistry and conditions: gaseous mixtures of CF4 and H2 reactive gases in a plasma with approximate gas flow ratios of greater than 10 to 1, hydrogen to carbon tetra-fluoride, and with a nominal gas flow ratio of 300 to 20, hydrogen gas to carbon tetra-fluoride gas, which reduces to a ratio of 15 to 1, and with power range from 100 to 500 Watts, bias from 50 to 1000 Volts, and temperature from −10 to 200° C.

### Claim 8

A method for fabricating dual damascene trench and vias openings over copper wiring comprising:
providing a substrate with a first insulating layer overlying the substrate;
providing a second insulating layer over the first insulating layer;
forming a patterned copper interconnection wiring over the first insulating layer and the patterned copper interconnection wiring is embedded in the second insulating layer;
depositing an etch stop layer, or a trench/via liner, over the second insulating layer and over the copper interconnection wiring;
depositing a third insulating layer over the etch stop layer, or trench/via liner;
forming dual damascene openings, trench and via openings, within the third insulating layer exposing regions of the etch stop layer;
forming an etch blocking pattern with photoresist over regions of the third insulating layer and exposing trench and via openings, and regions of the etch stop layer;
removing the exposed regions of the etch stop layer by a specific reactive ion etching process, thus exposing the underlying copper interconnection wiring.

### Claim 9 (depends on 8)

The method of claim 8, wherein said semiconductor substrate includes semiconductor device structures such as gate electrodes and source/drain regions.

### Claim 10 (depends on 8)

The method of claim 8, wherein said semiconductor substrate includes semiconductor device structures such as gate electrodes, source/drain regions and multiple levels of metal interconnections.

### Claim 11 (depends on 8)

The method of claim 8, wherein said insulating layers are porous, low dielectric constant material or materials with dielectric constants less than 2.5 selected from the group comprised of SiN, SiO, SOG, which is spun-on-glass, PE plasma enhanced TEOS, which is tetraethoxysilane, halogenated SiO, and fluorinated silicate glass, all deposited by a chemical vapor deposition process or a spin-on process, in a thickness range from 2,000 to 15,000 Angstroms.

### Claim 12 (depends on 8)

The method of claim 8, wherein said etch stop layer, or trench/via liner is selected from the group comprised of SiN and SiC, deposited by chemical vapor deposition, in a thickness range from approximately 200 to 800 Angstroms.

### Claim 13 (depends on 8)

The method of claim 8, whereby trench and vias opening are formed by etching trench and via openings in the insulating layer or layers by the following reactive ion etch process chemistry selected from the group of gases comprised of CF4, CHF3, CH2F2, C4F8, C5F8, C4F6, combined with ambient gas mixtures selected from the group comprised of Ar, O2, N21 CO and He, stopping the etch removal process on the etch stop layer.

### Claim 14 (depends on 8)

The method of claim 8, wherein the exposed portions of the etch stop layer are etched away exposing the underlying copper wiring by a reactive ion etch process comprised of following etchant chemistry and conditions: gaseous mixtures of CF4 and H2 reactive gases in a plasma with approximate gas flow ratios of greater than 10 to 1, hydrogen to carbon tetra-fluoride, and with a nominal gas flow ratio of 300 to 20, hydrogen gas to carbon tetra-fluoride gas, which reduces to a ratio of 15 to 1, and with power range from 100 to 500 Watts, bias from 50 to 1000 Volts, and temperature from −10 to 200° C.

### Claim 15

A method for fabricating dual damascene trench and vias openings over copper wiring comprising the following steps:
(a) providing a substrate with a first insulating layer overlying the substrate;
(b) providing a second insulating layer over the first insulating layer;
(c) forming a patterned copper interconnection wiring over the first insulating layer and the patterned copper interconnection wiring is embedded in the second insulating layer;
(d) depositing an etch stop layer, or a trench/via liner, over the second insulating layer and over the copper interconnection wiring;
(e) depositing a third insulating layer over the etch stop layer, or trench/via liner;
(f) forming dual damascene openings, trench and via openings, within the third insulating layer exposing regions of the etch stop layer;
(g) forming an etch blocking pattern with photoresist over regions of the third insulating layer and exposing trench and via openings, and regions of the etch stop layer;
(h) removing the exposed regions of the etch stop layer by a specific reactive ion etching process, and exposing the underlying copper interconnection wiring;
(i) depositing in the trench and via openings and on the third insulating layer a barrier layer, followed by a copper seed layer on the barrier layer;
(j) filling the trench and via openings with electrochemically plated copper on the copper seed layer forming an excess of copper on the surface of the third insulating layer;
(k) planarizing the surface by removing the excess copper, and simultaneously, removing the copper seed layer and barrier layer from the surface of the third insulating layer, thus forming inlaid conducting copper interconnect wiring and contact vias in a dual damascene process.

### Claim 16 (depends on 15)

The method of claim 15, wherein said semiconductor substrate includes semiconductor device structures such as gate electrodes and source/drain regions.

### Claim 17 (depends on 15)

The method of claim 15, wherein said semiconductor substrate includes semiconductor device structures such as gate electrodes, source/drain regions and multiple levels of metal interconnections.

### Claim 18 (depends on 15)

The method of claim 15, wherein said insulating layers are porous, low dielectric constant material or materials with dielectric constants less than 2.5 selected from the group comprised of SiN, SiO, SOG, which is spun-on-glass, PE plasma enhanced TEOS, which is tetraethoxysilane, halogenated SiO, and fluorinated silicate glass, all deposited by a chemical vapor deposition process or a spin-on process, in a thickness range from 2,000 to 15,000 Angstroms.

### Claim 19 (depends on 15)

The method of claim 15, wherein said etch stop layer, or trench/via liner is selected from the group comprised of SiN and SiC, deposited by chemical vapor deposition, in a thickness range from approximately 200 to 800 Angstroms.

### Claim 20 (depends on 15)

The method of claim 15, whereby trench and vias opening are formed by etching trench and via openings in the insulating layer or layers by the following reactive ion etch process chemistry selected from the group of gases comprised of CF4, CHF3, CH2F2, C4F8, C5F8, C4F6, combined with ambient gas mixtures selected from the group comprised of Ar, O2, N2, CO and He, stopping the etch removal process on the etch stop layer.

### Claim 21 (depends on 15)

The method of claim 15, wherein the exposed portions of the etch stop layer are etched away exposing the underlying copper wiring by a reactive ion etch process comprised of following etchant chemistry and conditions: gaseous mixtures of CF4 and H2 reactive gases in a plasma with approximate gas flow ratios of greater than 10 to 1, hydrogen to carbon tetra-fluoride, and with a nominal gas flow ratio of 300 to 20, hydrogen gas to carbon tetra-fluoride gas, which reduces to a ratio of 15 to 1, and with power range from 100 to 500 Watts, bias from 50 to 1000 Volts, and temperature from −10 to 200° C.

### Claim 22 (depends on 15)

The method of claim 15, wherein said barrier layer is selected from the group comprised of TaN and W, deposited by physical vapor deposition, sputter deposited to an approximate thickness from 20 to 700 Angstroms.

### Claim 23 (depends on 15)

The method of claim 15, wherein said copper seed layer is comprised of copper, deposited by physical vapor deposition, sputter deposited to an approximate thickness from 50 to 2000 Angstroms.

### Claim 24 (depends on 15)

The method of claim 15, wherein multilevel interconnect wiring and contact vias are formed by repeating steps (d) through (k).

### Claim 25 (depends on 15)

The method of claim 15, whereby the electrochemically plated copper on the copper seed layer is comprised of copper deposited by a plating process, using sulfuric acid bath, which fills the trench and via openings with electrochemically plated copper on the copper seed layer, and forms an excess of copper on the surface of the third insulating layer, with a plated copper thickness approximately 2000 to 5000 Angstroms.

### Claim 26 (depends on 15)

The method of claim 15, whereby the surface is planarized by removing the excess copper, and simultaneously, removing the copper seed layer and barrier layer from the surface of the third insulating layer, by chemical mechanical polishing, to form inlaid conducting copper interconnect wiring and contact vias in a dual damascene process.