# US 2004/0082159 A1 · Fabrication method for solder bump pattern of rear section wafer package

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0082159 A1
- Document ID: US20040082159A1
- Status: Published application
- Kind: A1
- Application number: 10/383,757
- Filed: 2003-03-10
- Published: 2004-04-29
- Earliest claimed: 2002-10-23
- Inventors: Wen-Lo Shieh; Fu-Yu Huang; Ning Huang; Hui-Pin Chen; Shu-Wan Lu; Zhe-Sung Wu; Chih-Yu Tsai; Mei-Hua Chen; Chia-Ling Lu; Yu-Ju Wang; Yu-Chun Huang; Tzu-Lin Liu; Wen-Tsung Weng; Ya-Hsin Tseng
- Web page: https://patentgrep.com/patent/US20040082159A1

## CPC

- H10W 72/20: Bump connectors, e.g. solder bumps or copper pillars; Dummy bumps; Thermal bumps
- H10W 72/012: {of bump connectors, dummy bumps or thermal bumps}
- H10W 72/01215: {forming coatings}
- H10W 72/251: {Materials}
- H10W 72/90: Bond pads, in general
- H10W 72/9415: {relative to the surface, e.g. recessed, protruding}
- H10W 72/952: {comprising metals or metalloids, e.g. PbSn, Ag or Cu}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A fabrication method for solder bump pattern of rear section wafer package is disclosed and the method includes the steps of: (a) pattern-etching the wafer at a passivation layer for the positioning of the solder bump; (b) depositing the entire under bump metal layer, (c) performing an opening on a solder pad using a photoresistor of an appropriate thickness; (d) placing the wafer at a vacuuming system and a heating system, where at this instance, the solder is in a liquid state having a fluidity but without formation of bubbles; and (e) forming a solder bump pattern at the opening position of the photoresistor of under bump metal of the wafer.

## Claims

### Claim 1

A fabrication method for solder bump pattern of rear section wafer package, comprising the steps of:
(a) pattern-etching the wafer at a passivation layer for the positioning of the solder bump;
(b) depositing the entire under bump metal layer;
(c) performing an opening on a solder pad using a photoresistor of an appropriate thickness;
(d) placing the wafer at a vacuuming system and a heating system, where at this instance, the solder is in a liquid state having a fluidity but without formation of bubbles; and
(e) forming a solder bump pattern at the opening position of the photoresistor of under bump metal of the wafer.

### Claim 2 (depends on 1)

The fabrication method of claim 1, wherein the formation of the solder bump on the wafer comprises the steps of:
(a) placing the wafer at a sloping position into a solder bath within a vacuuming system and the surface position of the solder is provided with a squeegee to contact the surface of the wafer, and the wafer being withdrawn and the solder being squeezed into the photo-resistor opening and the excessive solder being scraped off;
(b) removing the wafer from the vacuuming system and the heating system, and after the wafer being cooled, removing the photo-resistor to retain the solder ingot at under bump metal and further etching the under bump metal between the solder ingots so that the solder ingots are isolated into separate one;
(c) performing a wafer re-flow to a melting furnace step to melt the solder ingot into a solder bump having a spherical shape.

### Claim 3 (depends on 1)

The fabrication method of claim 1, wherein the formation of solder bump on the wafer via silk-screening printing method comprises the steps of:
(a) horizontally placing the wafer in a vacuuming system and heating system and melted solder at one lateral edge of the wafer being squeezed from one end to the other end of the wafer such that the solder fills the photo-resistor opening position of an under bump metal layer;
(b) removing the wafer from the vacuuming system and the heating system, and after the wafer being cooled, removing the photo-resistor to retain the solder ingot at under bump metal and further etching the under bump metal between the solder ingots so that the solder ingots are isolated into separate one;
(c) performing a wafer re-flow to a melting furnace step to melt the solder ingot into a spherical solder bump.