# US 2004/0082158 A1 · Method of forming a self-aligned, selectively etched, double recess high electron mobility transistor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0082158 A1
- Document ID: US20040082158A1
- Status: Published application
- Kind: A1
- Application number: 10/279,358
- Filed: 2002-10-24
- Published: 2004-04-29
- Earliest claimed: 2002-10-24
- Assignees: Raytheon Company
- Inventors: Colin S. Whelan; Elsa K. Tong
- Web page: https://patentgrep.com/patent/US20040082158A1

## CPC

- H10D 30/015: {of FETs having heterojunction interface channels or heterojunction gate electrodes, e.g. HEMT}
- H10D 30/4738: {having multiple donor layers}
- H10D 64/0125: {characterised by the sectional shape, e.g. T or inverted T}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A method is provided for forming a self-aligned, selectively etched, double recess high electron mobility transistor. The method includes providing a semiconductor structure having a III-V substrate; a first relatively wide band gap layer, a channel layer, a second relatively wide band gap Schottky layer, an etch stop layer; a III-V third wide band gap layer on etch stop layer; and an ohmic contact layer on the third relatively wide band gap layer. A mask is provided having a gate contact aperture to expose a gate region of the ohmic contact layer. A first wet chemical etch is brought into contact with portions of the ohmic contact layer exposed by the gate contact aperture. The first wet chemical selectively removes exposed portions of the ohmic contact layer and underlying portions of the third relatively wide band gap layer. The etch stop layer inhibits the first wet chemical etch from removing portions of such etch stop layer. Next, a second wet chemical etch is brought into contact with structure etched by the first wet chemical etch. The second wet chemical etch selectively removes exposed portions of the ohmic contact layer while leaving substantially un-etched exposed portions of the third relatively wide band gap layer, the Schottky contact layer and the etch stop layer. The etch stop layer is removed. A metal layer is deposited over the mask and through gate aperture therein onto, and in Schottky contact with, the Schottky contact layer.

## Claims

### Claim 1

A method for forming a double recess high electron mobility transistor, comprising:
providing a semiconductor structure having a III-V substrate; a wide band gap layer; a small band gap channel layer; a wideband gap Schottky layer; an etch stop layer; a wide band gap layer; and a contact layer.
providing a mask, such mask having a gate contact aperture to expose a gate region of the contact layer;
bringing a first wet chemical etch into contact with portions of the contact layer exposed by the gate contact aperture, such etch selectively removing exposed portions of the contact layer and underlying portions of the top wide band gap layer, such etch stop layer inhibiting such etch from removing portions of such etch stop layer;
bringing a second wet chemical etch into contact with structure etched by the first wet etch, such second etch selectively removing exposed portions of the contact layer while leaving substantially un-etched exposed portions of the wide band gap and the etch stop layer; and
removing the etch stop layer;
depositing a metal layer over the mask and through gate aperture therein onto, and in Schottky contact with the Schottky contact layer.

### Claim 2 (depends on 1)

The method recited in claim 1 wherein the etch stop layer comprises an AlAs.

### Claim 3 (depends on 2)

The method recited in claim 2 wherein the channel layer comprises InGaAs.

### Claim 4 (depends on 3)

The method recited in claim 3 wherein the third relatively wide band gap layer comprises AlGaAs, InAlAs or InAlGaAs.

### Claim 5 (depends on 2)

The method recited in claim 2 wherein the Schottky contact layer comprises InAlAs, InAlGaAs or AlGaAs.

### Claim 6 (depends on 5)

The method recited in claim 5 wherein the ohmic contact layer is InGaAs or GaAs.

### Claim 7 (depends on 5)

The method recited in claim 5 wherein the first wet chemical etch is substantially 2.5 pH acid:H2O2 or 4.2 pH succinic acid: H2O2.

### Claim 8 (depends on 5)

The method recited in claim 5 wherein the second wet chemical etch is substantially 5.3 pH Succinic acid: H2O2 or 6.4 pH citric acid: H2O2

### Claim 9

A method for forming a double recess high electron mobility transistor, comprising:
providing a semiconductor structure having a III-V substrate; a first relatively wide band gap layer; a relatively small band gap channel layer, a second relatively wide band gap layer, an etch stop layer over the substrate; a III-V Schottky layer on etch stop layer; a third relatively wide band gap layer on the etch stop layer; and an ohmic contact layer on the third relatively wide band gap layer;
providing a mask on over the ohmic contact layer, such mask having a lower portion with a gate contact aperture exposing a gate region of the channel layer; an upper portion vertically spaced from the lower portion and having a gate electrode metalization aperture; edges of the gate electrode metalization aperture terminating in overhangs which expose the gate contact aperture; surface portions of the lower portion of the mask being disposed adjacent to the gate contact aperture;
bringing a first wet chemical etch into contact with portions of the ohmic contact layer exposed by the gate contact aperture, such etch selectively removing exposed portions of the ohmic contact layer and underlying portions of the third relatively wide band gap layer, such etch stop layer inhibiting such etch from removing portions of such etch stop layer;
bringing a second wet chemical etch into contact with structure etched by the first wet etch, such second etch selectively removing exposed portions of the ohmic contact layer while leaving substantially un-etched exposed portions of the third wide band gap layer and the etch stop layer;
removing the etch stop layer;
depositing a metal layer over the mask, such metal being deposited on the upper portion thereof, through the gate electrode metalization aperture, through the gate contact aperture, and through gate aperture onto, and in Schottky contact with, the Schottky contact layer; and
lifting portions mask to remove portions of the metal disposed onto the upper surface of the mask while leaving portions of the deposited metal to provide a gate electrode for the transistor.

### Claim 12 (depends on 11)

The method recited in claim 11 wherein the etch stop layer comprises AlAs.

### Claim 13 (depends on 12)

The method recited in claim 12 wherein the channel layer comprises InGaAs.

### Claim 14 (depends on 13)

The method recited in claim 13 wherein the wide band gap layer comprises AlGaAs, InAlGaAs, InAlAs.

### Claim 15 (depends on 12)

The method recited in claim 12 wherein the channel layer Schottky contact layer comprises InAlGaAs, InAlAs or AlGaAs.

### Claim 16 (depends on 15)

The method recited in claim 15 wherein the ohmic contact layer comprises InGaAs or GaAs.

### Claim 17 (depends on 16)

The method recited in claim 16 wherein the first wet chemical etch is substantially 2.5 pH citric acid: H2O2.

### Claim 18 (depends on 16)

The method recited in claim 16 wherein the second wet chemical etch is substantially 5.3 pH Succinic acid: H2O2.

### Claim 19 (depends on 15)

The method recited in claim 15 wherein the first wet chemical etch is substantially 4.2 pH succinic acid: H2O2.

### Claim 20 (depends on 19)

The method recited in claim 19 wherein the second wet chemical etch is substantially 6.4 pH citric acid: H2O2.