# US 2004/0082156 A1 · Boron incorporated diffusion barrier material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0082156 A1
- Document ID: US20040082156A1
- Status: Published application
- Kind: A1
- Application number: 10/679,822
- Filed: 2003-10-06
- Published: 2004-04-29
- Earliest claimed: 1999-08-24
- Assignees: Micron Technology, Inc.
- Inventors: Vishnu K. Agarwal; Gurtej S. Sandhu
- Web page: https://patentgrep.com/patent/US20040082156A1

## CPC

- H10D 64/01318: {the conductor comprising a layer of alloy material, compound material or organic material contacting the insulator, e.g. TiN (comprising a layer of alloys of Si, Ge or C H10D64/01314)}
- H10D 64/01312: {the additional layer comprising a metal or metal silicide formed by deposition, i.e. without a silicidation reaction, e.g. sputter deposition}
- H10D 64/664: {the additional layers comprising a barrier layer between the layer of silicon and an upper metal or metal silicide layer}
- H10D 64/667: {the conductor comprising a layer of alloy material, compound material or organic material contacting the insulator, e.g. TiN workfunction layers (having lateral variation H10D64/671)}
- H10D 64/669: {the conductor further comprising additional layers of alloy material, compound material or organic material, e.g. TaN/TiAlN}
- H10W 20/4441: {the principal metal being a refractory metal}
- H10W 20/032: {of conductive barrier, adhesion or liner layers}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A diffusion barrier layer comprising TiNxBy is disclosed for protection of gate oxide layers in integrated transistors. The diffusion barrier layer can be fabricated by first forming a TiN layer and then incorporating boron into the TiN layer. The diffusion barrier layer can also be fabricated by forming a TiNxBy layer using a TDMAT process including boron. The diffusion barrier layer can also be fabricated by forming a TiNxBy layer using a CVD process. The diffusion barrier layer is of particular utility in conjunction with tungsten or tungsten silicide conductive layers formed by CVD.

## Claims

### Claim 1

A method of forming an integrated circuit structure comprising:
forming a gate oxide layer over a semiconductor substrate;
forming a titanium boronitride barrier layer above at least a portion of the gate oxide layer;
forming a polysilicon layer above at least a portion of the titanium boronitride barrier layer; and
forming a conductive layer above at least a portion of the polysilicon layer, wherein the act of forming the conductive layer incorporates fluorine atoms or ions into the conductive layer, and wherein the titanium boronitride barrier layer inhibits diffusion of the fluorine atoms or ions from the conductive layer into the gate oxide layer.

### Claim 2 (depends on 1)

The method of claim 1 wherein the act of forming a titanium boronitride layer comprises:
forming a TiN layer; and
incorporating boron into the TiN layer.

### Claim 3 (depends on 2)

The method of claim 2 wherein the TiN layer is formed by reactively sputtering a titanium target in a nitrogen-containing ambient.

### Claim 4 (depends on 3)

The method of claim 3 wherein the act of sputtering occurs at a radio frequency energy of between about 1 kW and about 2 kW.

### Claim 5 (depends on 3)

The method of claim 3 wherein the nitrogen-containing ambient comprises an inert gas and nitrogen ions from a nitrogen source gas.

### Claim 6 (depends on 5)

The method of claim 5 wherein the nitrogen source gas is selected from the group consisting of nitrogen and ammonia.

### Claim 7 (depends on 5)

The method of claim 5 wherein the concentration of the nitrogen source gas is about 5% to about 30%.

### Claim 8 (depends on 5)

The method of claim 5 wherein the nitrogen source gas is introduced into a sputtering chamber at a rate of between about 1 sccm and about 15 sccm.

### Claim 9 (depends on 2)

The method of claim 2 wherein the TiN layer is formed using a TDMAT process.

### Claim 10 (depends on 9)

The method of claim 9 wherein the act of forming using the TDMAT process occurs at a temperature of between about 300° C. and about 500° C.

### Claim 11 (depends on 9)

The method of claim 9 wherein the act of forming using the TDMAT process occurs at a pressure of between about 0.01 Torr and about 2.0 Torr.

### Claim 12 (depends on 2)

The method of claim 2 wherein the act of incorporating boron into the TiN layer comprises introducing a boron-containing gas into a chemical vapor deposition (CVD) chamber.

### Claim 13 (depends on 12)

The method of claim 12 wherein the boron-containing gas comprises diborane.

### Claim 14 (depends on 12)

The method of claim 12 wherein the boron-containing gas comprises silane at a concentration in the range of about 1% to about 50%.

### Claim 15 (depends on 12)

The method of claim 12 wherein the boron-containing gas is introduced into the CVD chamber at a rate of between about 5 sccm and about 500 sccm.

### Claim 16 (depends on 12)

The method of claim 12 wherein act of incorporating boron into the TiN layer occurs at a pressure of between about 0.5 Torr and about 100 Torr.

### Claim 17 (depends on 12)

The method of claim 12 wherein act of incorporating boron into the TiN layer occurs at a temperature of between about 300° C. and about 700° C.

### Claim 18 (depends on 1)

The method of claim 1 further comprising annealing the integrated circuit structure.

### Claim 19

A method of forming a gate in an integrated circuit comprising:
forming a dielectric layer;
forming a polysilicon layer over at least a portion of the dielectric layer;
forming a diffusion barrier layer comprising titanium boronitride over at least a portion of the polysilicon layer; and
forming a conductive layer over at least a portion of the diffusion barrier layer, wherein the conductive layer has at least some fluorine atoms or ions therein, and wherein the diffusion barrier layer inhibits diffusion of the fluorine atoms or ions from the conductive layer into the polysilicon layer.

### Claim 20 (depends on 19)

The method of claim 19 wherein the titanium boronitride is formed using a chemical vapor deposition (CVD) process.

### Claim 21 (depends on 20)

The method of claim 20 wherein the CVD process includes a titanium-containing source gas, a nitrogen-containing source gas, and a boron-containing source gas.

### Claim 22 (depends on 21)

The method of claim 21 wherein the titanium-containing source gas is selected from the group consisting of titanium tetrachloride and titanium tetraiodide.

### Claim 23 (depends on 21)

The method of claim 21 wherein the nitrogen-containing source gas comprises ammonia.

### Claim 24 (depends on 21)

The method of claim 21 wherein the boron-containing source gas comprises diborane.

### Claim 25 (depends on 20)

The method of claim 20 wherein the CVD process occurs at a pressure of between about 0.5 Torr and about 100 Torr.

### Claim 26 (depends on 20)

The method of claim 20 wherein the CVD process occurs at a temperature of between about 500° C. and about 700° C.

### Claim 27 (depends on 19)

The method of claim 19 wherein the act of forming titanium boronitride comprises combining tetrakisdimethyl-aminotitanium with a boron-containing source gas.

### Claim 28 (depends on 27)

The method of claim 27 wherein the act of combining occurs at about 0.5 Torr to 100 about Torr.

### Claim 29

The method of 27 wherein the act of combining occurs at about 300° C. to about 600° C.

### Claim 30 (depends on 27)

The method of claim 27 wherein the boron-containing source gas comprises diborane.

### Claim 31 (depends on 19)

The method of claim 19 further comprising annealing the gate.

### Claim 32 (depends on 19)

The method of claim 19 wherein the diffusion barrier layer inhibits diffusion of the fluorine atoms or ions from the conductive layer into the dielectric layer.

### Claim 33

A method of forming a gate electrode comprising:
forming a dielectric layer on a semiconductor substrate;
forming a diffusion barrier layer comprising titanium boronitride over at least a portion of the dielectric layer;
forming a polysilicon layer over at least a portion of the diffusion barrier layer;
forming a conductive layer over at least a portion of the polysilicon layer, wherein the act of forming the conductive layer incorporates fluorine atoms or ions into the conductive layer; and
annealing the conductive layer, wherein the diffusion barrier layer inhibits fluorine diffusion from the conductive layer into the dielectric layer.

### Claim 34 (depends on 33)

The method of claim 33 wherein the titanium boronitride has a thickness of about 50 angstroms to about 500 angstroms.

### Claim 35 (depends on 33)

The method of claim 33 wherein the act of forming the conductive layer forms tungsten.

### Claim 36 (depends on 33)

The method of claim 33 wherein the act of forming the conductive layer forms tungsten silicide.

### Claim 37 (depends on 33)

The method of claim 33 wherein the act of forming the conductive layer comprises combining tungsten hexafluoride and silicon tetrahydride.

### Claim 38 (depends on 37)

The method of claim 37 wherein the act of combining comprises a chemical vapor deposition (CVD) process.

### Claim 39 (depends on 33)

The method of claim 33 wherein the act of forming the conductive layer comprises combining a metal source and a silicon source gas in a chemical vapor deposition (CVD) process.

### Claim 40 (depends on 39)

The method of claim 39 wherein the metal source is selected from the group consisting of titanium tetrachloride and tungsten hexafluoride.

### Claim 41 (depends on 39)

The method of claim 39 wherein the silicon source gas is selected from the group consisting of silane, disaline, trisaline, and di-chlorosilane.

### Claim 42 (depends on 33)

The method of claim 33 wherein the conductive layer has a thickness of about 200 angstroms to about 4,000 angstroms.

### Claim 43 (depends on 33)

The method of claim 33 wherein the dielectric layer has a thickness of about 30 angstroms to about 200 angstroms.

### Claim 44 (depends on 33)

The method of claim 33 wherein the act of forming the dielectric layer comprises growing a gate oxide layer through a mask.

### Claim 45 (depends on 33)

The method of claim 33 wherein the act of forming the dielectric layer comprises forming a gate oxide layer through trench isolation.

### Claim 46 (depends on 33)

The method of claim 33 wherein the polysilicon layer has a thickness of about 300 angstroms to about 1,500 angstroms.

### Claim 47 (depends on 33)

The method of claim 33 wherein the act of forming the polysilicon layer comprises a chemical vapor deposition (CVD) process.

### Claim 48 (depends on 33)

The method of claim 33 wherein the act of annealing occurs at a temperature of between about 600° C. and about 900° C.

### Claim 49 (depends on 33)

The method of claim 33 wherein the act of annealing occurs for about 25 minutes.