# US 2004/0082142 A1 · Fabrication method for a semiconductor structure having a partly filled trench

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2004/0082142 A1
- Document ID: US20040082142A1
- Status: Published application
- Kind: A1
- Application number: 10/660,091
- Filed: 2003-09-10
- Published: 2004-04-29
- Earliest claimed: 2002-09-13
- Assignees: Infineon Technologies AG
- Inventors: Jana Hansel; Matthias Rudolph
- Web page: https://patentgrep.com/patent/US20040082142A1

## CPC

- H10W 10/014: {using trench refilling with dielectric materials, e.g. shallow trench isolations}
- H10P 50/268: {of silicon-containing layers}
- H10P 95/04: {Planarisation of conductive or resistive materials}
- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

The present invention provides a fabrication method for a semiconductor structure having a partly filled trench, having the following steps: provision of a semiconductor structure (1, 5) having a trench (2); filling of the trench (2) with a filling (10) in such a way that the filling (10) projects above a surface (OF) of the semiconductor structure (1, 5) by a first height (h1), the filling (10) covering the trench (2) and the periphery (20) of the trench (2); planarization of the filling (10) in a first etching step in such a way that the filling (10) is essentially planar with the surface (OF) of the semiconductor structure (1, 5); and sinking of the filling (10) in the trench (2) in a second etching step by a predetermined depth (T) proceeding from the surface of the semiconductor structure (1, 5); essentially the same plasma power and the same etchant composition being used for the first and second etching steps.

## Claims

### Claim 1

Fabrication method for a semiconductor structure having a partly filled trench, having the following steps:
provision of a semiconductor structure (1, 5) having a trench (2);
filling of the trench (2) with a filling (10) in such a way that the filling (10) projects above a surface (OF) of the semiconductor structure (1, 5) by a first height (h1), the filling (10) covering the trench (2) and the periphery (20) of the trench (2);
planarization of the filling (10) in a first etching step in such a way that the filling (10) is essentially planar with the surface (OF) of the semiconductor structure (1, 5); and
sinking of the filling (10) in the trench (2) in a second etching step by a predetermined depth (T) proceeding from the surface of the semiconductor structure (1, 5);
essentially the same plasma power and the same etchant composition being used for the first and second etching steps.

### Claim 2 (depends on 1)

Method according to claim 1,
characterized
in that a planarization of the filling (10) is carried out in a zeroth etching step before the first etching step in such a way that the filling (10) projects above the surface (OF) of the semiconductor structure (1, 5) by a second height (h2), the filling (10) covering the trench (2) and the periphery (20) of the trench (2), the zeroth etching step having a higher etching rate than the first etching step.

### Claim 3 (depends on 2)

Method according to claim 2,
characterized
in that essentially the same etchant composition as for the first and second etching steps but an increased plasma power are used for the zeroth etching step.

### Claim 4 (depends on 1, 2, 3)

Method according to claim 1, 2 or 3,
characterized
in that at least the first etching step is carried out with a first time duration which is determined by an end point identification.

### Claim 5 (depends on 2, 3, 4)

Method according to claim 2, 3 or 4,
characterized
in that the zeroth etching step and the second etching step are carried out with a predetermined zeroth and second time duration.

### Claim 6 (depends on 1, 2, 3, 4)

Method according to one of the preceding claims 1 to 4,
characterized
in that the second etching step is carried out with a second time duration which is determined by an end point identification.

### Claim 7

Method according to one of the preceding claims,
characterized
in that the etchant composition contains SF6, Ar and Cl2.

### Claim 8

Method according to one of the preceding claims,
characterized
in that the semiconductor structure (1, 5) comprises a semiconductor substrate (1) and a mask (5) situated thereon, the mask (5) being used for the etching of the trench (2).

### Claim 9 (depends on 4, 5, 6, 7, 8)

Method according to one of the preceding claims 4 to 8,
characterized
in that the end point identification is carried out by interferometry.